Thermal oxidation of Ti-6Al–4V alloy and pure titanium under external bending strain: Experiment and modelling
Source abstract
Abstract
Abstract The thermal oxidation behaviour of Ti-6Al–4V alloy as well as pure titanium under external bending strains was investigated through experimental and modelling approaches. Dislocation accumulation due to creep deformation was responsible for the acceleration of oxidation at initial stage. However, the promoted formation of alumina would retard the subsequent scale growth. Moreover, the bending strain had a multi-fold influence on the formation of oxygen diffusion zone. An analytical model was developed to predict the variation of growth stress within the oxide layer along with time. The prediction results agreed well with experimental data.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Nuclear Materials and Properties · Titanium Alloys Microstructure and Properties · Intermetallics and Advanced Alloy Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (52)
Show source-provided references
1. In situ impedance spectroscopy study of the electrochemical corrosion of Ti and Ti-6Al-4V in simulated body fluid at 25°C and 37°C10.1016/j.corsci.2009.06.035 ↗
2. Phosphoric acid anodization of Ti-6Al-4V-structure and corrosion aspects10.1016/j.corsci.2006.06.021 ↗
3. Corrosion behaviour of selective laser melted Ti-6Al-4V alloy in NaCl solution10.1016/j.corsci.2015.10.041 ↗
4. Improving corrosion resistance of Ti-6Al-4V alloy through plasma-assisted PVD deposited nitride coatings10.1016/j.corsci.2014.07.047 ↗
5. The role of cold work and applied stress on surface oxidation of 304 stainless steel10.1016/j.corsci.2011.11.021 ↗
6. Air oxidation behavior of Ti-6Al-4V alloy between 650 and 850°C10.1016/0010-938X(94)90069-8 ↗
7. Various aspects of the air oxidation behaviour of a Ti6Al4V alloy at temperatures in the range 600–700C10.1007/BF00445984 ↗
8. Thermal oxidation of Ti6Al4V alloy: microstructural and electrochemical characterization10.1016/j.matchemphys.2009.09.007 ↗
9. Oxidation of Ti-6Al-4V alloy10.1016/j.jallcom.2008.04.024 ↗
10. Glass-ceramic coating on titanium alloys for high temperature oxidation protection: oxidation kinetics and microstructure10.1016/j.corsci.2013.04.041 ↗
11. Surface modification of a Ti-6Al-4V alloy by thermal oxidation10.1016/j.surfcoat.2004.05.018 ↗
12. The oxidation behaviour of gamma-titanium aluminide alloys under thermal cycling conditions10.1016/0010-938X(92)90192-6 ↗
13. Oxygen boost diffusion for the deep-case hardening of titanium alloys10.1016/S0921-5093(99)00697-8 ↗
14. Thermal oxidation behaviour of bulk titanium with nanocrystalline surface layer10.1016/j.corsci.2012.03.005 ↗
15. Photoelectrochemical imaging of metal-scale decohesion on titanium thermally oxidised in oxygen10.1016/j.corsci.2007.11.010 ↗
16. Determination of the growth stress and strain in α-Al2O3 scales during the oxidation of Fe-22Cr-4.8Al-0.3Y alloy10.1016/S1359-6454(97)00306-6 ↗
17. Tensile stress and creep in thermally grown oxide10.1038/nmat1626 ↗
18. Stresses in NiO, Cr2O3 and Al2O3 oxide scales10.1016/0921-5093(94)09747-X ↗
19. Growth stresses in α-Cr2O3 thermal oxide films determined by in situ high temperature Raman spectroscopy10.1063/1.2805638 ↗
20. Stress effect in high temperature oxidation10.1179/imr.1995.40.1.1 ↗
21. Role of interface structure and interfacial defects in oxide scale growth10.1007/BF01046723 ↗
22. The lateral growth strain accompanying the formation of a thermally grown oxide10.1016/S1359-6454(02)00532-3 ↗
23. Coupled mechanical-oxidation modelling during silicon thermal oxidation process10.1063/1.4930255 ↗
24. Analytical modeling of stress and strain of symmetrically oxidized metal10.1063/1.4740048 ↗
25. Residual stresses within oxide layers due to lateral growth strain and creep strain: analytical modelling10.1063/1.3626052 ↗
26. On the elastic and creep stress analysis modeling in the oxide scale/metal substrate system due to oxidation growth strain10.1016/j.corsci.2012.09.035 ↗
27. General approach on chemistry and stress coupling effects during oxidation10.1063/1.4826530 ↗
28. Influence of external mechanical loadings (creep, fatigue) on oxygen diffusion during nickel oxidation10.1007/BF01046824 ↗
29. Effect of cracking in diffusion aluminide coating on their cyclic oxidation performance on Ti-based IMI-834 alloy10.1016/j.corsci.2009.03.027 ↗
30. Dry oxidation of silicon: a new model of growth including relaxation of stresses by viscous flow10.1063/1.331986 ↗
31. Finite element modelling of the oxidation kinetics of Zircaloy-4 with a controlled metal-oxide interface and the influence of growth stress10.1016/j.corsci.2015.07.024 ↗
32. Analytical modeling on stress assisted oxidation and its effect on creep response of metals10.1007/s11085-014-9493-4 ↗
33. Silicon oxidation studies: a revised model for thermal oxidation10.1063/1.332722 ↗
34. Comparative study of oxidation kinetics for pure nickel oxidized under tensile and compressive stress10.1016/j.corsci.2009.09.005 ↗
35. Pellissier · 1971
36. Standard practice for preparation and use of bent-beam stress-corrosion testspecimens, ASTM G39-99. http://www.astm.org/Standards/G39.htm
37. Stress analysis of polycrystalline thin films and surface regions by X-ray diffraction10.1107/S0021889804029516 ↗
38. Determination of the residual stress state in a natural titanium oxide layer10.1016/1359-6454(95)00213-8 ↗
39. On the determination of diffusion coefficients of oxygen in one-phase Ti (α-Ti) and two-phase Ti-4Nb (α- and β-Ti) by micro-hardness measurements10.1023/A:1010333410938 ↗
40. High temperature steady-state creep of polycrystalline rutile, pure and doped with tantalum10.1007/BF00542065 ↗
41. Initial stages of plasma electrolytic oxidation of titanium10.1016/S0010-938X(03)00101-X ↗
42. Thermal expansion of various ceramic materials to 1500°C10.1111/j.1151-2916.1956.tb15619.x ↗
43. In situ observations of lattice expansion and transformation rates of α and β phases in Ti-6Al-4V10.1016/j.msea.2004.08.084 ↗
44. Effect of oxygen and hydrogen on mechanical properties of commercial purity titanium10.1179/imr.1996.41.1.1 ↗
45. Oxidation of commercial purity titanium10.1007/BF00659186 ↗
46. Enhanced wear resistance of titanium surfaces by a new thermal oxidation treatment10.1016/S0043-1648(99)00359-2 ↗
47. Surface characterization of mechanical property evaluation of thermally oxidized Ti-6Al-4V10.1016/j.matchar.2008.12.014 ↗
48. Formation of alumina on Ti-Al alloys10.1016/0036-9748(87)90291-2 ↗
49. Deformation modes of the α-phase of Ti-6Al-4V as a function of oxygen concentration and aging temperature10.1007/BF02642403 ↗
50. Creep mechanisms and physical modeling for Ti-6Al-4V10.1016/j.msea.2003.11.016 ↗
51. Creep behavior of Ti-6Al-4V and a comparison with titanium matrix composites10.1016/j.msea.2006.05.089 ↗
52. Dislocations and point defects10.1039/df9572300122 ↗