Abstract

Abstract High purity SiC nanostructures were grown in situ on the surfaces of C/SiC composites by the chemical vapor reaction route to improve the anti-oxidation capability of C/SiC composites. It was found that the SiC nanostructures formed a dense cluster with a thickness of about 20 μm. The nanostructures mainly included nanoparticles and nanorods. The oxidation tests found that the SiC nanostructures could significantly improve the anti-oxidation capability of C/SiC composites, particularly, at the temperature beyond 900 °C. The improvement of the anti-oxidation capability of the C/SiC composites was attributed to the formation of a silica layer.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Aluminum Alloys Composites Properties · Advanced materials and composites

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (34)

Show source-provided references
1. Carbon fiber reinforced CMC for high-performance structures10.1111/j.1744-7402.2004.tb00169.x ↗
2. Design, preparation and properties of non-oxide CMCs for application in engines and nuclear reactors: an overview10.1016/S0266-3538(03)00230-6 ↗
3. CMC body flaps for the X-38 experimental space vehicle10.1002/9780470294741.ch38 ↗
4. Microstructure and oxidation behavior of C/C-ZrB2-SiC composites coated with SiC coating at high temperature10.1016/j.corsci.2015.08.015 ↗
5. Oxidation behavior of C/SiC-Ti3SiC2 at 800–1300°C in air10.1016/j.jeurceramsoc.2016.03.029 ↗
6. Oxidation behaviour of two-dimensional C/SiC modified with self-healing Si-B-C coating in static air10.1016/j.corsci.2012.08.003 ↗
7. Corrosion of barium aluminosilicates by water-vapor: an investigation from first principles10.1016/j.corsci.2009.05.040 ↗
8. Hot corrosion behavior of barium aluminosilicate-coated C/SiC composites at 900°C10.1111/j.1551-2916.2009.03339.x ↗
9. Microstructure, oxidation protection and failure mechanism of Yb2SiO5/LaMgAl11O19 coating deposited on C/SiC composites by atmospheric plasma spraying10.1016/j.corsci.2012.05.020 ↗
10. Failure mechanism associated with the thermally grown silica scale in environmental barrier coated C/SiC composites10.1111/jace.14273 ↗
11. Effects of temperature, oxidation and fiber preforms on fatigue life of carbon fiber-reinforced ceramic-matrix composites
12. Oxidation behavior of C/C composites with the fibre/matrix interface modified by carbon nanotubes grown in situ at low temperature10.1016/j.corsci.2011.09.024 ↗
13. Improving mechanical strength and thermal shock resistance of SiC/zinc aluminum silicate joint by electrophoretic deposited multi-walled carbon nanotubes10.1016/j.matdes.2016.01.061 ↗
14. CNT-PyC-SiC/SiC double-layer oxidation-protection coating on C/C composite10.1016/j.carbon.2008.07.014 ↗
15. HfC nanowire-toughened TaSi2-TaC-SiC-Si multiphase coating for C/C composites against oxidation10.1016/j.corsci.2014.10.048 ↗
16. Thermal shock resistance and isothermal oxidation behavior of C/SiC-SiCnano functionally gradient coating on graphite produced via reactive melt infiltration (RMI)10.1016/j.matchemphys.2016.07.004 ↗
17. Effect of SiC nanowires on the mechanical and oxidation protective ability of SiC coating for C/C composites10.1111/j.1551-2916.2012.05412.x ↗
18. Nanowire-toughened transition layer to improve the oxidation resistance of SiC-MoSi2-ZrB2 coating for C/C composites10.1016/j.corsci.2016.05.013 ↗
19. In-situ PIP-SiC NWs-toughened SiC-CrSi2-Cr3C2-MoSi2-Mo2C coating for oxidation protection of carbon/carbon composites10.1016/j.jallcom.2016.03.126 ↗
20. Electrophoretic deposition of SiC nanowires onto carbon/carbon composites to improve the interface bonding of Ti-Ni-Si joint10.1016/j.matdes.2015.04.042 ↗
21. Recent progress in synthesis, properties and potential applications of SiC nanomaterials10.1016/j.pmatsci.2015.01.003 ↗
22. One-dimensional nanostructures: synthesis, characterization, and applications10.1002/adma.200390087 ↗
23. In situ growth of SiC nanowires on RS-SiC substrate(s)10.1016/j.jcrysgro.2003.12.073 ↗
24. Laser synthesis of carbon-rich SiC nanoribbons10.1063/1.1570928 ↗
25. Superhydrophobic carbon nanotube/silicon carbide nanowire nanocomposites10.1016/j.matdes.2015.08.025 ↗
26. Carbon fiber reinforced ceramics based on reactive melt infiltration processes10.4191/kcers.2012.49.4.287 ↗
27. Interlaminar shear strength of C-SiC based composites reinforced with heat treated carbon fibers
28. Morphology and stacking faults of β-silicon carbide whisker synthesized by carbothermal reduction10.1111/j.1151-2916.2000.tb01593.x ↗
29. Syntheses and growth mechanisms of 3C-SiC nanostructures from carbon and silicon powders10.1166/jnn.2009.1323 ↗
30. Surface modification of carbon nanofibers with SiC by heating different SiO vapor sources in argon atmosphere10.2109/jcersj2.122.822 ↗
31. Kinetics and mechanisms of oxidation of 2D woven C/SiC composites: i experimental approach10.1111/j.1151-2916.1994.tb07096.x ↗
32. Oxidation kinetics and its impact on the strength of carbon short fiber reinforced C/SiC ceramics10.1002/adem.201200130 ↗
33. Kinetics and mechanisms of oxidation of 2D woven C/SiC composites: II theoretical approach10.1111/j.1151-2916.1994.tb07096.x ↗
34. Oxidation mechanisms and kinetics of SiC-matrix composites and their constituents10.1023/B:JMSC.0000048745.18938.d5 ↗