The role of acetic acid or H+ in initiating crevice corrosion of N80 carbon steel in CO2-saturated NaCl solution
Source abstract
Abstract
Abstract The role of acetic acid (HAc) or H+ in initiating the crevice corrosion of N80 carbon steel in CO2-saturated NaCl solution was studied by weight loss and electrochemical measurements. It is demonstrated that crevice corrosion could be initiated by the concentration difference either HAc or H+ between outside and inside the crevice. The corrosion rate inside the crevice becomes higher than that outside the crevice and the total corrosion rate inside and outside the crevice decreases after connection. Crevice corrosion is more severe in the solution with HAc than that in the solution with H2SO4 at the same pH value.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Corrosion Behavior and Inhibition · Hydrogen embrittlement and corrosion behaviors in metals · Concrete Corrosion and Durability
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (46)
Show source-provided references
1. Effect of pressure on corrosion behaviour of X60, X65, X70, and X80 carbon steels in water-unsaturated supercritical CO2 environments10.1016/j.ijggc.2016.06.002 ↗
2. Effect of small amount of H2S on the corrosion behaviour of carbon steel in the dynamic supercritical CO2 environments10.1016/j.corsci.2015.11.009 ↗
3. Recommend design of filler metal to minimize carbon steel weld metal preferential corrosion in CO2-saturated oilfield produced water10.1016/j.apsusc.2016.07.151 ↗
4. Synergistic effect of stress and crevice on the corrosion of N80 carbon steel in the CO2-saturated NaCl solution containing acetic acid10.1016/j.corsci.2017.05.005 ↗
5. Single-boss crevice former for studying crevice corrosion of UNS S32003 in chloride-containing solution at high temperature10.1016/j.jallcom.2014.09.060 ↗
6. The self-sustaining propagation of crevice corrosion on the hybrid BC1 Ni–Cr–Mo alloy in hot saline solutions10.1016/j.corsci.2016.01.003 ↗
7. Electrochemical investigations on crevice corrosion of a martensitic stainless steel in a thin-layer cell10.1016/j.jelechem.2014.07.008 ↗
8. Electrochemical evaluation of under-deposit corrosion and its inhibition using the wire beam electrode method10.1016/j.corsci.2010.12.015 ↗
9. Oxyanions as inhibitors of chloride-induced crevice corrosion of Alloy 2210.1016/j.corsci.2012.10.037 ↗
10. The crevice corrosion behaviour of stainless steel in sodium chloride solution10.1016/j.corsci.2011.08.012 ↗
11. Crevice corrosion behaviour of superaustenitic stainless steels: dynamic electrochemical impedance spectroscopy and atomic force microscopy studies10.1016/j.corsci.2008.11.008 ↗
12. Augmentation of crevice corrosion resistance of medical grade 316L VM stainless steel by plasma carburising10.1016/j.corsci.2012.02.023 ↗
13. Test methods for electrochemical migration: a review10.1007/s10854-016-5713-9 ↗
14. Effects of crevice geometry on corrosion behaviour of 304 stainless steel during crevice corrosion in high temperature pure water10.1016/j.corsci.2016.04.049 ↗
15. Simultaneous visualization of pH and Cl− distributions inside the crevice of stainless steel10.1016/j.corsci.2016.01.028 ↗
16. A mathematical model of crevice corrosion for buried pipeline with disbonded coatings under cathodic protection10.1016/j.jlp.2016.03.024 ↗
17. The corrosion behaviour of carbon steel in CO2-saturated NaCl crevice solution containing acetic acid10.1002/maco.201006027 ↗
18. Crevice corrosion of stainless steels: I. A mathematical model10.1179/000705978798358671 ↗
19. Crevice corrosion of stainless steels: II. Experimental studies10.1179/000705978798276258 ↗
20. The role of copper on the crevice corrosion behaviour of nickel-chromium-molybdenum alloys in aggressive solutions10.5006/1876 ↗
21. Crevice corrosion of copper for radioactive waste packaging material in simulated groundwater10.1179/1743278215Y.0000000026 ↗
22. Behaviour of crevice corrosion in iron10.1016/j.corsci.2004.08.001 ↗
23. The significance of the local electrode potential within pits, crevices and cracks10.1016/0010-938X(89)90039-5 ↗
24. In situ investigation of crevice corrosion on UNS S32101 duplex stainless steel in sodium chloride solution10.1016/j.corsci.2013.06.039 ↗
25. Electrochemical evaluation of crevice corrosion of 430 ferritic stainless steel using the microcapillary tube technique10.1016/j.desal.2005.05.016 ↗
26. The effect of crevice opening dimension on the stability of crevice corrosion for nickel in sulfuric acid10.1149/1.1838632 ↗
27. The significance of the local electrode potential within pits, crevices and cracks10.1016/0010-938X(89)90039-5 ↗
28. The effect of acetic acid on the pit propagation in CO2 corrosion of carbon steel10.1016/j.elecom.2007.11.028 ↗
29. Pit growth and stifling on carbon steel in CO2-containing media in the presence of HAc10.1016/j.electacta.2009.07.061 ↗
30. Numerical simulation of a single corrosion pit in CO2 and acetic acid environments10.1016/j.corsci.2010.01.010 ↗
31. Crevice corrosion of N80 carbon steel in CO2-saturated environment containing acetic acid10.1016/j.corsci.2016.08.002 ↗
32. Corrosion of X65 steel in CO2-saturated oilfield formation water in the absence and presence of acetic acid10.1016/j.corsci.2009.04.004 ↗
33. A study of the inhibition of iron corrosion in HCl solutions by some amino acids10.1016/j.corsci.2010.01.019 ↗
34. EIS study of the surface film on the surface of carbon steel from supercritical carbon dioxide corrosion10.1016/j.apsusc.2003.12.025 ↗
35. Evolution of dissolution processes at the interface of carbon steel corroding in a CO2 environment studied by EIS10.1016/j.corsci.2009.10.007 ↗
36. An XPS characterization of FeCO3 films from CO2 corrosion10.1016/S0010-938X(98)00180-2 ↗
37. New 1H-pyrrole-2,5-dione derivatives as efficient organic inhibitors of carbon steel corrosion in hydrochloric acid medium: electrochemical, XPS and DFT studies10.1016/j.corsci.2014.10.052 ↗
38. The electrode kinetics of the deposition and dissolution of iron10.1016/0013-4686(61)80026-1 ↗
39. Initial stages of the anodic oxidation of iron in chloride solutions10.5006/1.3585204 ↗
40. The effects of anions on the behaviour of scratched iron electrodes in aqueous solutions10.1016/0010-938X(80)90145-6 ↗
41. The dissolution mechanism of iron in chloride solutions10.1149/1.2108381 ↗
42. Effects of chloride content on CO2 corrosion of carbon steel in simulated oil and gas well environments10.1016/j.corsci.2014.03.025 ↗
43. Electrodissolution kinetics of iron in chloride solutions III. Acidic solutions10.1149/1.2404023 ↗
44. Localized corrosion of carbon steel in a CO2-saturated oilfield formation water10.1016/j.electacta.2010.10.059 ↗
45. Area relationships in galvanic corrosion10.5006/0010-9312-27.10.436 ↗
46. On the fundamentals of electrochemical corrosion of X65 steel in CO2-containing formation water in the presence of acetic acid in petroleum production10.1016/j.corsci.2008.10.013 ↗