Comparison of the oxidation behavior of a zirconium nitride coating in water vapor and air at high temperature
Source abstract
Abstract
The oxidation behavior of zirconium nitride coating in high-temperature water vapor and air environments was studied. The parabolic rate constant of ZrN oxidizing in the water vapor environment at 600 °C was approximately 100 times faster than that in air, due to the larger pores and greater number of cracks that were formed across ZrO2 oxide layer formed during the water vapor oxidation process than during the air oxidation process. A bilayer-structure ZrO2 with tetragonal ZrO2 near the ZrN/ZrO2 interface and monoclinic ZrO2 approaching the outer ZrO2 surface were formed in both cases. The lateral cracks across the ZrO2 scale were caused by volume expansion from the tetragonal ZrO2 phase to the monoclinic ZrO2 phase transition.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Semiconductor materials and devices · Metal and Thin Film Mechanics · Advanced ceramic materials synthesis
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (27)
Show source-provided references
1. A study of the oxidation of FeCrAl alloy in pressurized water and high-temperature steam environment10.1016/j.corsci.2015.02.027 ↗
2. Oxidation of zircaloy by steam10.1016/0022-3115(91)90428-A ↗
3. Protection of zirconium by alumina- and chromia-forming iron alloys under high-temperature steam exposure10.1016/j.jnucmat.2013.03.006 ↗
4. Superior corrosion resistance properties of TiN-based coatings on zircaloy tubes in supercritical water10.1016/j.jnucmat.2014.04.010 ↗
5. Thin films of hard cubic Zr3N4 stabilized by stress10.1038/nmat1338 ↗
6. Decorative hard coatings with improved corrosion resistance10.1016/S0257-8972(98)00791-9 ↗
7. Study of mechanical properties of PVD ZrN films, deposited under positive and negative substrate bias conditions10.1016/j.scriptamat.2004.06.005 ↗
8. Mechanism and kinetics of oxidation of ZrN ceramics10.1111/jace.13575 ↗
9. In situ and ex situ studies of microstructure evolution during high-temperature oxidation of ZrN hard coating10.1016/j.scriptamat.2014.10.024 ↗
10. Oxidation of TiN, ZrN, TiZrN, CrN, TiCrN and TiN/CrN multilayer hard coatings reactively sputtered at low temperature10.1016/0040-6090(96)08663-4 ↗
11. The high-temperature oxidation kinetics of Zr-alloy claddings in air and steam
12. Oxidation behavior of silicon carbide at 1200°C in both air and water–vapor-rich environments10.1016/j.corsci.2014.07.052 ↗
13. The influence of silver content on the tribological and antimicrobial properties of ZrN/Ag nanocomposite coatings10.1166/jnn.2011.3790 ↗
14. Comparison of tribological and anti-microbial properties of CrN/Ag, ZrN/Ag, TiN/Ag, and TiN/Cu nanocomposite coatings10.1016/j.surfcoat.2010.07.029 ↗
15. The microstructure and microtexture of zirconium oxide films studied by transmission electron backscatter diffraction and automated crystal orientation mapping with transmission electron microscopy10.1016/j.actamat.2014.07.062 ↗
16. Determination_of_residual stresses_by_X-ray_diffraction
17. Effect of platinum addition on oxidation behavior of γ/γ′ nickel aluminide10.1016/j.actamat.2014.12.023 ↗
18. Residual stresses and tetragonal phase fraction characterisation of corrosion tested zircaloy-4 using energy dispersive synchrotron X-ray diffraction10.1016/j.jnucmat.2012.07.025 ↗
19. A comparative study of the oxidation behavior of Cr2N and CrN coatings10.1016/j.tsf.2013.01.031 ↗
20. Influence of niobium addition on microstructure, mechanical properties and oxidation resistance of ZrN coatings10.1016/j.tsf.2014.05.019 ↗
21. Crystallization and creep behavior of Si–B–C–N ceramics10.1016/j.actamat.2005.06.011 ↗
22. Modeling of oxidation-induced growth stresses10.1016/j.scriptamat.2004.03.001 ↗
23. In situ measurement of stresses and phase compositions of the zirconia scale during oxidation of zirconium by Raman spectroscopy10.1007/s11085-013-9433-8 ↗
24. Silicon carbide oxidation in steam up to 2 MPa
25. Mechanisms of room temperature metastable tetragonal phase stabilisation in zirconia10.1179/174328005X14267 ↗
26. The influence of Y ion implantation on the oxidation behavior of ZrN coating10.1016/j.vacuum.2004.06.004 ↗
27. Flexible hard Al-Si-N films for high temperature operation10.1016/j.surfcoat.2016.05.054 ↗