journal article·2019-03Open access

Influence of hydrogen on the propagation of intergranular corrosion defects in 2024 aluminium alloy

Marie-Laetitia de Bonfils-Lahovary, Claudie Josse, Lydia Laffont, Christine Blanc

Corrosion Science· Volume 148

Abstract

To study the influence of hydrogen on the intergranular corrosion mechanism of a 2024 aluminium alloy, samples were hydrogen precharged by cathodic polarisation and then exposed to a NaCl solution. EBSD analyses and SEM observations showed that hydrogen increased the number of corroded interfaces and led to the embrittlement of low-angle grain boundaries which were not susceptible to corrosion without hydrogen precharging. The increase of the reactivity of the 2024 aluminium alloy in the presence of hydrogen gave a new insight into the intergranular corrosion mechanism: corrosion-induced hydrogen promoted the intergranular corrosion propagation and partially controlled the corrosion defect morphology.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Corrosion Behavior and Inhibition · Hydrogen embrittlement and corrosion behaviors in metals · Non-Destructive Testing Techniques

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (46)

Show source-provided references
1. Commission on Engineering and Technical Systems · 1997
2. Success stories: air force; material substitution and new sealing
3. The intergranular corrosion susceptibility of 2024 Al alloy during re–ageing after solution treating and cold–rolling10.1016/j.corsci.2016.11.013 ↗
4. Intergranular corrosion propagation rate of 2024 alloy investigated via the “one-dimensional artificial pit” technique10.1016/j.corsci.2016.05.033 ↗
5. In situ X-ray tomography of intergranular corrosion of 2024 and 7050 aluminium alloys10.1016/j.corsci.2010.08.026 ↗
6. Localised corrosion initiation and microstructural characterisation of an Al 2024 alloy with a higher Cu to Mg ratio10.1016/j.corsci.2011.10.035 ↗
7. A localized approach to study corrosion inhibition of intermetallic phases of AA 2024-T3 by cerium malate10.1016/j.apsusc.2018.10.243 ↗
8. B.E. Amitha Rani, Corrosion inhibition of 2024-T3 aluminum alloy in 3.5% NaCl by thiosemicarbazone derivatives10.1016/j.corsci.2018.03.021 ↗
9. Transitions between pitting and intergranular corrosion in AA202410.1016/S0013-4686(02)00828-9 ↗
10. Detection of nanoscale η-MgZn2 phase dissolution from an Al-Zn-Mg-Cu alloy by electrochemical mocrotransients10.1002/sia.2868 ↗
11. Localised corrosion of 2024 T351 aluminum alloy in chloride media10.1016/S0010-938X(98)00116-4 ↗
12. Mechanism of intergranular corrosion of Al-Cu alloys10.1016/S0010-938X(70)80003-8 ↗
13. Study of grain boundary character along intergranular stress corrosion crack paths in austenitic alloys10.1016/S1359-6454(01)00064-7 ↗
14. The coincidence site lattice and the ‘sigma enigma’10.1016/S1044-5803(02)00193-6 ↗
15. Corrosion behaviors of random and special grain boundaries in a sensitized 304 stainless steel10.1016/S1006-706X(08)60107-7 ↗
16. Grain boundary character distribution and intergranular corrosion behavior in high purity aluminum10.1016/S1359-6462(00)00682-5 ↗
17. Intergranular corrosion and stress corrosion cracking of sensitised AA518210.4028/www.scientific.net/MSF.519-521.641 ↗
18. Identification of the metallurgical parameters explaining the corrosion susceptibility in a 2050 aluminium alloy10.1016/j.corsci.2015.10.020 ↗
19. Observations of intergranular corrosion in AA2024-T351: the influence of grain stored energy10.1016/j.corsci.2012.04.005 ↗
20. Characterization of intergranular corrosion defects in a 2024 T351aluminium alloy10.1016/j.corsci.2017.02.020 ↗
21. Discontinuities in the porous anodic film formed on AA2099-T8 aluminium alloy10.1016/j.corsci.2011.08.023 ↗
22. Structure of the copper-enriched layer introduced by anodic oxidation of copper-containing aluminium alloy10.1016/j.electacta.2015.01.133 ↗
23. Grain stored energy and the propagation of intergranular corrosion in AA2xxx aluminium alloys10.1002/sia.5218 ↗
24. Investigation of dealloying of S phase (Al2CuMg) in AA 2024-T3 aluminium alloy using high resolution 2D and 3D electron imaging10.1016/j.corsci.2015.11.013 ↗
25. Characterization and control of the intergranular corrosion defects in a 2024 T351 aluminium alloy
26. Investigation of Kelvin probe force microscopy efficiency for the detection of hydrogen ingress by cathodic charging in an aluminium alloy10.1016/j.scriptamat.2012.11.026 ↗
27. A Kelvin probe force microscopy study of hydrogen insertion and desorption into 2024 aluminum alloy10.1016/j.jallcom.2017.06.143 ↗
28. Hydrogen mapping in an aluminium alloy using an alternating current scanning electrochemical microscope (AC-SECM)10.1016/j.elecom.2017.05.007 ↗
29. Spatially resolved mapping of the relative concentration of dissolved hydrogen using the scanning electrochemical microscope10.1016/j.elecom.2014.12.004 ↗
30. The effect of absorbed hydrogen on the dissolution of steel10.1016/j.heliyon.2016.e00209 ↗
31. Traction-separation relationships for hydrogen induced grain boundary embrittlement in nickel via molecular dynamics simulations10.1016/j.msea.2015.10.042 ↗
32. Direct evaluation of grain boundary hydrogen embrittlement: a micro-mechanical approach10.1016/j.msea.2016.03.035 ↗
33. On the implication of hydrogen on inter-granular fracture10.1016/j.mspro.2014.06.327 ↗
34. Grain size and grain boundary effects on diffusion and trapping of hydrogen in pure nickel10.1016/j.actamat.2012.09.004 ↗
35. Meso-scale anisotropic hydrogen segregation near grain-boundaries in polycrystalline nickel characterized by EBSD/SIMS10.1016/j.matlet.2015.12.016 ↗
36. Grain-boundary engineering markedly reduces susceptibility to intergranular hydrogen embrittlement in metallic materials10.1016/j.actamat.2009.05.012 ↗
37. Hydrogen in aluminium10.1016/S0925-8388(96)02968-4 ↗
38. Localized corrosion growth kinetics in AA2024 alloys10.1149/1.1513984 ↗
39. Anisotropy of localized corrosion in AA2024-T310.1149/1.1391121 ↗
40. Les joints de grains: De la théorie à l’ingénierie
41. Transition between low and high angle grain boundaries10.1016/j.actamat.2005.03.005 ↗
42. Nano-scale dissolution phenomena in Al–Cu–Mg alloys10.1016/j.elecom.2007.10.032 ↗
43. Morphology of enriched alloy layers in an anodized Al-Cu alloy10.1016/S0169-4332(02)01040-1 ↗
44. Humphreys · 2004
45. Effect of grain boundary structure on sensitization and corrosion of stainless steel10.1007/BF02668561 ↗
46. A study of the relation between grain boundary type and sensitisation in a partially-sensitised AISI 304 stainless steel using electron back-scattering patterns10.1016/0036-9748(89)90480-8 ↗