journal article·2021-10

Oxidation characteristics of Fe22Cr5Al3Mo-xNb alloys in high temperature steam

Wenhuai Zhang, Yue Qian, Rongrong Sun, Xiaodong Lin, Meiyi Yao, Yunlong Qiu, Jian Yang, Guoguang Cheng, Jianxin Dong

Corrosion Science· Volume 191
Publisher page

Abstract

Abstract The oxidation behaviors of Fe22Cr5Al3Mo-xNb (x=0.5, 1.0, 2.0 wt%) alloys under simulated loss of coolant accident (LOCA) conditions at 1000 and 1200 ℃ were investigated. The results revealed that fine granular oxides and a ridged oxide film were formed on the FeCrAl alloys at 1000 and 1200 ℃, respectively. The oxide film was composed of α-Al2O3, α-Cr2O3 and a trace amount of FeO at 1000 ℃ but only consisted of α-Al2O3 at 1200 ℃ due to volatilization of Fe and Cr oxides. Nb addition decreased the weight gains and improved the oxidation resistance of FeCrAl alloys under simulated LOCA condition.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Nuclear Materials and Properties · High-Temperature Coating Behaviors · Nuclear reactor physics and engineering

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (63)

Show source-provided references
1. Insights from review and analysis of the Fukushima Dai-ichi accident10.1080/18811248.2011.636538 ↗
2. Analyses of core melt and re-melt in the Fukushima Daiichi nuclear reactors10.1080/18811248.2011.636537 ↗
3. Preliminary assessment of accident-tolerant fuels on LWR performance during normal operation and under DB and BDB accident conditions10.1016/j.jnucmat.2013.09.052 ↗
4. Deformation behavior of laser welds in high temperature oxidation resistant Fe–Cr–Al alloys for fuel cladding applications10.1016/j.jnucmat.2014.08.013 ↗
5. Advanced oxidation-resistant iron-based alloys for LWR fuel cladding10.1016/j.jnucmat.2013.06.041 ↗
6. Research progress in the FeCrAl alloys for accident tolerant fuel cladding
7. Influence of composition and heating schedules on compatibility of FeCrAl alloys with high-temperature steam10.1016/j.jnucmat.2018.09.026 ↗
8. Andresen · 2014 · 1
9. Improving accident tolerance of nuclear fuel with coated Mo-alloy cladding10.1016/j.net.2015.12.003 ↗
10. Development status of accident-tolerant fuel for light water reactors in Korea10.1016/j.net.2015.11.011 ↗
11. Current status of materials development of nuclear fuel cladding tubes for light water reactors10.1016/j.nucengdes.2017.02.031 ↗
12. Protective coatings on zirconium-based alloys as accident-tolerant fuel (ATF) claddings10.1515/corrrev-2017-0010 ↗
13. Accident tolerant fuels for LWRs: a perspective10.1016/j.jnucmat.2013.12.005 ↗
14. Oxidation of FeCrAl alloy: influence of temperature and atmosphere on scale growth rate and mechanism10.1016/S0257-8972(00)00989-0 ↗
15. The oxidation of high-purity iron-chromium-aluminum alloys at 800 ℃10.1007/BF00662042 ↗
16. Wrinkling of α-alumina films grown by oxidation—II. Oxide separation and failure10.1016/S1359-6454(98)00134-7 ↗
17. The morphology of oxidation of alumina-forming iron-base alloys containing chromium and aluminum10.1007/BF00603839 ↗
18. High-temperature oxidation behavior of iron-chromium-aluminum alloys10.1023/A:1004682316408 ↗
19. High-temperature-oxidation behavior of iron–aluminide diffusion coatings10.1007/s11085-006-9033-y ↗
20. Oxidation properties of Fe-5Cr-4Al (wt. %) alloys in oxygen at temperatures 1000 ℃-1320 ℃10.1007/BF01058835 ↗
21. Growth of α-alumina oxide film in high temperature oxidation of Fe-20Cr-5Al alloy thin strip10.1016/S1359-6462(98)00283-8 ↗
22. The oxidation behaviour of NiAl-I. Phase transformations in the alumina scale during oxidation of NiAl and NiAl-Cr alloys10.1016/0010-938X(92)90002-K ↗
23. On the transient oxidation of a Ni-15Cr-6Al alloy10.1007/BF00605003 ↗
24. 1995 · 20 · 75
25. Oxidation characteristics of two FeCrAl alloys in air and steam from 800 °C to 1300 °C10.1007/s11837-018-2979-9 ↗
26. The effect of water vapor on the initial stages of oxidation of the FeCrAl alloy Kanthal AF at 900 °C10.1007/s11085-007-9055-0 ↗
27. Water-vapor-effect on the oxidation of Fe-21.5 wt.%Cr-5.6 wt.%A1 at 1000 °C10.1007/BF02134786 ↗
28. In steam short-time oxidation kinetics of FeCrAl alloys10.1007/s11665-018-3665-3 ↗
29. Formation and stability of oxide layer in FeCrAl fuel cladding material under high-temperature steam10.1016/j.jallcom.2016.05.145 ↗
30. Effect and role of alloyed Nb on the air oxidation behaviour of Ni-Cr-Fe alloys at 1000 °C10.1016/j.corsci.2017.08.003 ↗
31. Oxidation behavior of ferritic stainless steel containing Nb, Nb–Si and Nb–Ti for SOFC interconnect10.1016/j.ijhydene.2012.12.073 ↗
32. Effects of minor alloy additions and oxidation temperature on protective alumina scale formation in creep-resistant austenitic stainless steels10.1016/j.scriptamat.2007.08.032 ↗
33. Design of Laves phase strengthened ferritic heat resisting steels inthe Fe – Cr – Nb(– Ni) system10.1016/S0921-5093(01)01586-6 ↗
34. Effect of Nb on microstructure and corrosion resistance of Fe22Cr5Al3Mo alloy
35. Microstructural control of FeCrAl alloys using Mo and Nb additions10.1016/j.matchar.2017.08.008 ↗
36. Effects of Laves phase particles on recovery and recrystallization behaviors of Nb-containing FeCrAl alloys10.1016/j.actamat.2017.11.027 ↗
37. Cold-rolling & annealing process for nuclear grade wrought FeCrAl cladding alloy to enhance the strength and ductility10.1016/j.jmatprotec.2019.116434 ↗
38. Study on high temperature creep behavior of the accident-resistant cladding Fe–13Cr–4Al-1.85Mo-0.85Nb alloy10.1016/j.msea.2020.140688 ↗
39. Dynamic strain aging behavior of accident tolerance fuel cladding FeCrAl-based alloy for advanced nuclear energy10.1007/s10853-021-05820-6 ↗
40. Effects of Nb-doping on the mechanical properties and high-temperature steam oxidation of annealing FeCrAl fuel cladding alloys10.1016/j.msea.2020.140500 ↗
41. Microstructure, mechanical properties and strengthening mechanisms of friction stir welded Kanthal APMTTM steel10.1016/j.jnucmat.2018.07.001 ↗
42. The oxidation of alloys10.1088/0034-4885/39/5/001 ↗
43. The mechanism of the high‐temperature oxidation of iron‐chromium alloys in water vapor10.1149/1.2425963 ↗
44. Effect of titanium addition on alumina growth mechanism on yttria-containing FeCrAl-base alloy10.1007/s11085-018-9861-6 ↗
45. Sintering and reactive sintering by Spark Plasma Sintering (SPS)
46. Sulfidation–oxidation behavior of FeCrAl and TiCrAl and the third-element effect10.1007/s11085-010-9194-6 ↗
47. The effect of oxide volatilization on the oxidation kinetics of Cr and Fe-Cr alloys10.1149/1.2424115 ↗
48. The nature of the third-element effect in the oxidation of Fe–xCr–3at.% Al alloys in 1atm O2 at 1000°C10.1016/j.corsci.2007.06.019 ↗
49. Oxidation of FeCrAl alloys at 500-900°C in dry O210.1002/maco.200503882 ↗
50. The isothermal oxidation behaviour of Fe-Cr-Al and Fe-Cr-Al-Y alloys at 1200 °C
51. New insights into the mechanism of yttrium changing high-temperature oxide growth of Fe-13Cr–6Al–2Mo–0.5Nb alloy for fuel cladding10.1016/j.corsci.2020.108728 ↗
52. On the measurement of strain in coatings formed on a wrinkled elastic substrate10.1023/A:1018848607100 ↗
53. On the mechanical behavior of brittle coatings and layers10.1007/BF00656841 ↗
54. Effects of morphology on the decohesion of compressed thin films10.1016/S0921-5093(97)00848-4 ↗
55. Effect of Nb on the high temperature oxidation of Ti–(0–50 at.%)Al10.1016/S1359-6462(02)00042-8 ↗
56. Oxidation behavior of TiAl protected by Al and Nb combined ion implantation at high temperature10.1016/S0168-583X(01)00934-X ↗
57. Thermodynamic activities in the alloys of the Ti-Al-Nb system
58. The relationship between specific heat capacity and oxidation resistance of TiAl alloys
59. The effect of niobium-ion implantation on the oxidation behavior of γ-TiAl alloys in static and flowing air10.1023/A:1010381326868 ↗
60. Effect of Nb on the bonging characteristics of TiAl intermetallic compounds: a first-principle study
61. First principles studies of TiAl-based alloys10.1016/S1471-5317(02)00038-X ↗
62. Effect of Nb on oxidation behavior of high Nb containing TiAl alloys10.1016/j.intermet.2010.08.029 ↗
63. Mechanical properties and oxidation characteristics of TiNiAl(Nb) intermetallics10.1016/j.intermet.2006.10.005 ↗