Oxidation pre-treatment to improve the mechanical property and oxidation resistance of Si–Mo–Cr coated C/C composites
Source abstract
Abstract
Abstract A transition layer with an interlocking structure was obtained at the interface between C/C composites and Si–Mo–Cr coating by oxidation pre-treatment and pack cementation process. The effects of pre-oxidation time on the microstructures, mechanical property and oxidation behavior of the coated C/C samples were investigated. After oxidation pre-treatment at 1173 K in air for 6 min, the flexural strength of the coated samples increases by 71.7% and the mass loss rate decreases by 77.4%. The improvements of the mechanical property and oxidation resistance are primarily attributed to the formation of the moderate transition layer between C/C and Si–Mo–Cr coating.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · Intermetallics and Advanced Alloy Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (25)
Show source-provided references
1. Oxidation resistant carbon materials derived from boronated carbon–silicon alloys10.1016/j.carbon.2004.07.004 ↗
2. Oxidation protection of carbon–carbon composites using chemical vapor deposition and glaze technology10.1016/0010-938X(93)90344-G ↗
3. HfC/ZrC ablation protective coating for carbon/carbon composites10.1016/j.corsci.2013.06.042 ↗
4. Laser ablation behaviors of SiC–ZrC coated carbon/carbon composites10.1016/j.surfcoat.2011.03.039 ↗
5. A simple model for the oxidation of carbon-containing composites10.1016/j.corsci.2009.12.002 ↗
6. Microstructure and oxidation resistance of Si–Mo–B coating for C/SiC coated carbon/carbon composites10.1016/j.corsci.2013.03.015 ↗
7. Multilayer coating with self-sealing properties for carbon–carbon composites10.1016/S0008-6223(03)00228-8 ↗
8. Ablation behavior of HfC protective coatings for carbon/carbon composites in an oxyacetylene combustion flame10.1016/j.corsci.2012.08.064 ↗
9. An AlPO4/SiC coating prepared by pulse arc discharge deposition for oxidation protection of carbon/carbon composites10.1016/j.corsci.2013.11.006 ↗
10. A comparative overview of molybdenum disilicide composites10.1016/0921-5093(92)90308-N ↗
11. Microstructure and oxidation of multi-layer MoSi2–CrSi2–Si coatings for SiC coated carbon/carbon composites10.1016/j.corsci.2010.05.020 ↗
12. Multilayer and multi-component oxidation protective coating system for carbon/carbon composites from room temperature to 1873 K10.1016/j.corsci.2013.03.006 ↗
13. Phase equilibria in the system iron oxide–Cr2O3–SiO2 in air10.1111/j.1151-2916.1960.tb13609.x ↗
14. ZrO2–SiO2 gradient multilayer oxidation protective coating for SiC coated carbon/carbon composites10.1016/j.surfcoat.2004.02.014 ↗
15. Thermal fatigue behavior of C/C composites modified by SiC–MoSi2–CrSi2 coating10.1016/j.jallcom.2011.05.068 ↗
16. The effect of pre-oxidation treatment on the plasticity behavior of B2 iron aluminide10.1016/j.vacuum.2012.09.017 ↗
17. Corrosion behavior of pre-oxidized and thermally nitrided stainless steel for polymer electrolyte membrane fuel cell bipolar plates10.1016/j.corsci.2012.01.014 ↗
18. Effect of pre-oxidization on the cyclic coking and carburizing resistance of HP40 alloy: with and without yttrium modification10.1016/j.corsci.2013.06.002 ↗
19. SiC whisker-toughened SiC oxidation protective coating for carbon/carbon composites10.1016/j.carbon.2005.09.026 ↗
20. Microstructure and mechanical properties of ultrafine bamboo-shaped SiC rod-reinforced HfC ceramic coating10.1016/j.surfcoat.2013.08.028 ↗
21. CNT–PyC–SiC/SiC double-layer oxidation-protection coating on C/C composite
22. High-temperature oxidation behavior of carbon materials in air10.1016/0008-6223(93)90148-4 ↗
23. SiC/C multi-layered coating contributing to the antioxidation of C/C composites and the suppression of through-thickness cracks in the layer10.1016/S0008-6223(00)00276-1 ↗
24. Mullite based oxidation protection for SiC-C/C composites in air at temperatures up to 1900K10.1016/S0955-2219(98)00242-8 ↗
25. SiC nanowire-toughened MoSi2–SiC coating to protect carbon/carbon composites against oxidation10.1016/j.corsci.2010.01.031 ↗