journal article·2011-03

Simulation of crack growth during hydrostatic testing of pipeline steel in near-neutral pH environment

Yongwang Kang, Weixing Chen, Richard Kania, Gregory Van Boven, Robert Worthingham

Corrosion Science· Volume 53· Issue 3
Publisher page

Abstract

Abstract The objective of this investigation was to understand the role of crack dimension, hydrogen, room-temperature creep and loading procedure on crack growth during hydrostatic testing of pipeline steels in near-neutral pH aqueous soil environments. Crack growth was found during hydrotesting, but was not linearly related to the stress intensity factor at the crack tip. Crack growth is mainly driven through the internal-hydrogen-assisted-cracking mechanism, instead of the hydrogen-environmental-assisted-cracking mechanism. Excessive plastic deformation induced by room-temperature creep prior to hydrotesting reduces crack advance during hydrotesting. Lower loading rate generally induces larger crack growth by hydrostatic loading. More crack growth occurs during loading in high stress regime.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Non-Destructive Testing Techniques · Material Properties and Failure Mechanisms

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (26)

Show source-provided references
1. National Energy Board of Canada, Public inquiry concerning stress corrosion cracking on Canadian oil and gas pipeline, 1996, MH-2-95.
2. Mechanisms of high-pH and near-neutral-pH SCC of underground pipelines10.1115/1.1376716 ↗
3. Review of stress corrosion cracking of pipeline steels in “low” and “high” pH solutions10.1023/A:1021126202539 ↗
4. R.N. Parkins, A review of stress corrosion cracking of high pressure gas pipelines, Corrosion 2000, NACE International, Houston, 2000, Paper No. 00363.
5. Stress corrosion cracking of pipeline steels
6. Canadian Energy Pipeline Association, Stress corrosion cracking – Recommend practices, CEPA, 2007.
7. Effect of hydrostatic testing on ductile tearing of X-65 line pipe steel with stress corrosion cracks10.5006/1.3294382 ↗
8. J.A. Beavers, C.E. Jaske, Near neutral pH SCC in pipelines: effect of pressure fluctuations on crack propagation, Corrosion 98, NACE International, Houston, 1998, Paper No. 257.
9. B.N. Leis, F.W. Brust, Hydrostest strategies for gas transmission pipelines based on ductile-flaw-growth considerations, NG-18 Report No. 194, 1992.10.55274/R0010296 ↗
10. W. Chen, R. Sutherby, Laboratory simulation of hydrostatic test in near-neutral pH soil environments, in: International Pipeline Conference 2006, Calgary, Canada, pp. 25–29.10.1115/IPC2006-10477 ↗
11. Tansgranular crack growth in the pipeline steels exposed to near-neutral pH soil aqueous solutions: the role of hydrogen10.1016/j.actamat.2009.08.047 ↗
12. Characteristics of near-neutral-pH stress corrosion cracks in an X-65 pipeline10.5006/1.3279878 ↗
13. S. Asher, P.M. Singh, Hydrogen production and permeation of X-65 pipeline steel in near-neutral pH environments, Corrosion 2008, NACE International, Houston, 2008, Paper No. 08411.
14. Effect of dissolved hydrogen and elastic and plastic deformation on active dissolution of pipeline steel in anaerobic groundwater of near-neutral pH10.1016/j.actamat.2008.08.035 ↗
15. Environmentally assisted cracking mechanism of pipeline steel in near-neutral pH groundwater10.1016/j.corsci.2010.02.020 ↗
16. Effects of hydrogen on the fracture toughness of a X70 pipeline steel10.1016/j.corsci.2009.07.013 ↗
17. Hydrogen-assisted cracking
18. Anderson · 2005
19. The role of residual stress in neutral pH stress corrosion cracking of pipeline steels – Part II: Crack dormancy10.1016/j.actamat.2006.07.021 ↗
20. A study on the pre-cyclic-load-induced burst of creep deformation of a pipeline steel under subsequent static load10.1016/S0921-5093(01)01548-9 ↗
21. Hydrogen diffusivities and concentrations in 520m carbon steel under cathodic protection in 0.5m NaCl and the effect of added sulphite, dithionite, thiosulphate, and sulphide10.1016/S1452-3981(23)17054-4 ↗
22. W. Chen, T.R. Jack, F. King, M.J. Wilmott, Hydrogen permeation behavior of X-70 piperline steel in a near-neutral pH soil environment, in: International Pipeline Conference 2000, Calgary, Canada, pp. 953–960.10.1115/IPC2000-218 ↗
23. Effect of cathodic potential on hydrogen content in a pipeline steel exposed to NS4 near-neutral pH soil solution10.5006/1.3287857 ↗
24. W. Chen, R.L. Eadie, R.L. Sutherby, Environmental effects on near-neutral pH stress corrosion cracking in pipelines, in: Second International Conference on Environment-induced Cracking of Metals, 2004, The Banff Centre, Banff, Alberta, Canada, pp. 211–220.10.1016/B978-008044635-6.50059-5 ↗
25. W. Chen, R. Sutherby, Environmental effect of crack growth rate of pipelines steel in near-neutral pH soil environments, in: International Pipeline conference 2004, Calgary, Canada, pp. 123–132.10.1115/IPC2004-0449 ↗
26. Crack growth behavior of pipeline steel in near-neutral pH soil environment10.1007/s11661-007-9184-8 ↗