Influence of surface condition on the corrosion of ultra-high-purity Mg alloy wire
Source abstract
Abstract
Corrosion of extruded and cold-drawn XHP-ZX00 wire samples was studied using immersion in CO2-bicarbonate buffered Hanks' solution. Six surface conditions were studied: as-extruded, as-drawn, annealed, mechanically cleaned, chemically polished and cleaned with acetic acid. Cold drawing introduced some iron impurity particles onto the wire surface, however the low corrosion rates suggest that the amount of these particles was low. Corrosion was evaluated by mass loss, hydrogen evolution and radius reduction, an adapted corrosion evaluation method. There was good agreement between the corrosion rates evaluated from mass loss and radius reduction. Mechanically cleaning produced the lowest corrosion rate. (C) 2016 Elsevier Ltd. All rights reserved.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Magnesium Alloys: Properties and Applications · Hydrogen Storage and Materials · Aluminum Alloys Composites Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (64)
Show source-provided references
1. The history of biodegradable magnesium implants: a review10.1016/j.actbio.2010.02.028 ↗
2. Review of recent developments in the field of magnesium corrosion10.1002/adem.201400434 ↗
3. Biodegradable metals10.1016/j.mser.2014.01.001 ↗
4. A review on magnesium alloys as biodegradable materials10.1007/s11706-010-0024-1 ↗
5. Novel magnesium alloys developed for biomedical application: a review10.1016/j.jmst.2013.02.005 ↗
6. Biodegradable magnesium alloys: a review of material development and applications10.4028/www.scientific.net/JBBTE.12.25 ↗
7. Biomedical magnesium alloys: a review of material properties, surface modifications and potential as a biodegradable orthopaedic implant10.5923/j.ajbe.20120206.02 ↗
8. Biodegradable surgical implants based on magnesium alloys—a review of current research
9. AMS INSIGHT—absorbable metal stent implantation for treatment of below-the-knee critical limb ischemia: 6-month analysis10.1007/s00270-008-9472-8 ↗
10. Drug-eluting bioabsorbable magnesium stent10.1111/j.1540-8183.2004.04081.x ↗
11. Corrosion mechanism applicable to biodegradable magnesium implants10.1016/j.mseb.2010.12.017 ↗
12. MgZnCa glasses without clinically observable hydrogen evolution for biodegradable implants10.1038/nmat2542 ↗
13. Degradable biomaterials based on magnesium corrosion10.1016/j.cossms.2009.04.001 ↗
14. The in vivo and in vitro corrosion of high-purity magnesium and magnesium alloys WZ21 and AZ9110.1016/j.corsci.2013.06.019 ↗
15. Corrosion of high purity Mg, Mg2Zn0.2Mn ZE41 and AZ91 in Hank’s solution at 37°C10.1016/j.corsci.2011.06.030 ↗
16. Corrosion of high purity Mg, AZ91 ZE41 and Mg2Zn0.2Mn in Hank’s solution at room temperature10.1016/j.corsci.2010.10.008 ↗
17. Evaluation of coatings for Mg alloys for biomedical applications10.1002/adem.201300516 ↗
18. Rates of in vivo (arterial) and in vitro biocorrosion for pure magnesium10.1002/jbm.a.35179 ↗
19. Tensile testing as a novel method for quantitatively evaluating bioabsorbable material degradation10.1002/jbm.b.32775 ↗
20. Magnesium as a biodegradable and bioabsorbable material for medical implants10.1007/s11837-009-0129-0 ↗
21. A survey of bio-corrosion rates of magnesium alloys10.1016/j.corsci.2009.09.033 ↗
22. Magnesium alloys: predicting in vivo corrosion with in vitro immersion testing10.1002/jbm.b.32680 ↗
23. The in vitro and in vivo evaluation of the biocompatibility of Mg alloys10.1088/1748-6041/9/1/015006 ↗
24. In vivo corrosion behavior of Mg-Mn-Zn alloy for bone implant application10.1002/jbm.a.31273 ↗
25. Biocorrosion of magnesium alloys: a new principle in cardiovascular implant technology?10.1136/heart.89.6.651 ↗
26. Buffer-regulated biocorrosion of pure magnesium
27. Mechanical property, biocorrosion and in vitro biocompatibility evaluations of Mg–Li–(Al)–(RE) alloys for future cardiovascular stent application10.1016/j.actbio.2013.01.032 ↗
28. In vitro and in vivo corrosion measurements of magnesium alloys10.1016/j.biomaterials.2005.07.037 ↗
29. Magnesium biomaterials: past, present and future10.1179/1743278212Y.0000000034 ↗
30. Kirkland · 2014
31. The influence of pH on the corrosion rate of high-purity Mg, AZ91 and ZE41 in bicarbonate buffered Hanks' solution10.1016/j.corsci.2015.09.018 ↗
32. Understanding magnesium corrosion—a framework for improved alloy performance10.1002/adem.200310405 ↗
33. Corrosion mechanisms of magnesium alloys10.1002/(SICI)1527-2648(199909)1:1<11::AID-ADEM11>3.0.CO;2-N ↗
34. Calculated phase diagrams and the corrosion of die-cast Mg–Al alloys10.1016/j.corsci.2008.12.015 ↗
35. Assessing the degradation performance of ultrahigh-purity magnesium in vitro and in vivo10.1016/j.corsci.2014.09.008 ↗
36. C. Wegmann, J. Löffler, P. Uggowitzer, M. Becker, H. Feichtinger, Process and apparatus for vacuum distillation of high-purity magnesium, European Patent Application, (2012) PCT/EP 2013/000131-WO2013/107644.
37. Corrosion of ultra-high-purity Mg in 3.5% NaCl solution saturated with Mg(OH)210.1016/j.corsci.2013.05.018 ↗
38. High-strength low-alloy (HSLA) Mg–Zn–Ca alloys with excellent biodegradation performance10.1007/s11837-014-0875-5 ↗
39. Performance-driven design of biocompatible Mg alloys10.1007/s11837-011-0089-z ↗
40. New magnesium alloys for potential application of implantation biomaterial10.4028/www.scientific.net/AMR.79-82.1443 ↗
41. In vitro degradation and mechanical integrity of Mg–Zn–Ca alloy coated with Ca-deficient hydroxyapatite by the pulse electrodeposition process10.1016/j.actbio.2009.12.009 ↗
42. Microstructure, mechanical properties and bio-corrosion properties of Mg–Zn–Mn–Ca alloy for biomedical application10.1016/j.msea.2008.06.019 ↗
43. Influence of Ca and Zn on the microstructure and corrosion of biodegradable Mg–Ca–Zn alloys10.1016/j.corsci.2015.01.027 ↗
44. Tensile properties of glassy MgZnCa wires and reliability analysis using Weibull statistics10.1016/j.actamat.2009.03.028 ↗
45. Corrosion of, and cellular responses to Mg–Zn–Ca bulk metallic glasses10.1016/j.biomaterials.2009.11.015 ↗
46. Bulk metallic glasses10.1016/j.mser.2004.03.001 ↗
47. G.-L. Song (ed.), Corrosion Prevention of Mg Alloys, Woodhouse, 2013.10.1533/9780857098962 ↗
48. Surface modification of magnesium alloy AZ31 by hydrofluoric acid treatment and its effect on the corrosion behaviour10.1016/j.tsf.2010.04.114 ↗
49. D. Sachdeva, A.M. Kumar, G. Song, Surface treatment of magnesium alloy castings for corrosion protection, US Patent, (2013) 8,608,869.
50. The surface, microstructure and corrosion of magnesium alloy AZ31 sheet10.1016/j.electacta.2010.02.068 ↗
51. Cold-drawn ZM21 and WE43 wires exhibit exceptional strength and ductility
52. Expanding magnesium’s reach through cold drawing
53. Effects of organic acid pickling on the corrosion resistance of magnesium alloy AZ31 sheet10.1016/j.corsci.2010.03.002 ↗
54. Influence of inorganic acid pickling on the corrosion resistance of magnesium alloy AZ31 sheet10.1016/j.corsci.2009.06.045 ↗
55. Assessing the corrosion of biodegradable magnesium implants: a critical review of current methodologies and their limitations10.1016/j.actbio.2011.11.014 ↗
56. Arterial blood gas analysis10.7748/ns2004.02.18.21.45.c3544 ↗
57. An innovative specimen configuration for the study of Mg corrosion10.1016/j.corsci.2010.09.016 ↗
58. Advances in Mg corrosion and research suggestions10.1016/j.jma.2013.09.003 ↗
59. Influence of the β-phase morphology on the corrosion of the Mg alloy AZ9110.1016/j.corsci.2008.04.010 ↗
60. Effect of pH on the in vitro corrosion rate of magnesium degradable implant material10.1016/j.msec.2010.04.003 ↗
61. Bio-corrosion of a magnesium alloy with different processing histories10.1016/j.matlet.2007.12.052 ↗
62. Influence of the chloride ion concentration on the corrosion of high-purity Mg, ZE41 and AZ91 in buffered Hank’s solution
63. Engineering the Mg–Mg2Ni eutectic transformation to produce improved hydrogen storage alloys10.1016/j.ijhydene.2009.07.036 ↗
64. On the immersion testing of degradable implant materials in simulated body fluid: active pH regulation using CO210.1002/adem.201200218 ↗