Impurity and temperature enhanced growth behaviour of anodic aluminium oxide from AA5052 Al-Mg alloy using hybrid pulse anodization at room temperature

C.K. Chung, C.H. Tsai, C.R. Hsu, E.H. Kuo, Y. Chen, I.C. Chung

Corrosion Science· Volume 125
Publisher page

Abstract

Abstract Conventional anodic aluminium oxide (AAO) was formed using direct-current anodization from high-purity (99.99%–99.999%) Al foils at low 0–5 °C with a growth rate about 2–3 μm/h. Here, we investigate the greatly enhanced growth behaviour of AAO from AA5052 Al-Mg alloy (96.6%Al-2.6%Mg) at high 25 °C using hybrid-pulse anodization. The Mg-impurity and high-temperature enhanced growth rate of AAO at 25 °C is over three-fold to 9.7 μm/h; it also reduces the average pore size to 32.2 nm from 42.8 nm due to high-activity Mg hydrolysis releasing high Mg(OH) 2 -formation heat and H 2 gas. The unique property of AAO from AA5052 is discussed.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Anodic Oxide Films and Nanostructures · Aluminum Alloys Composites Properties · Aluminum Alloy Microstructure Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (36)

Show source-provided references
1. Structural and optical properties of InGaN&z.urule;GaN multiple quantum wells grown on nano-air-bridged GaN template10.1063/1.2372686 ↗
2. Optical characteristics of two-dimensional photonic crystals in anodic aluminum oxide films10.1143/JJAP.43.3643 ↗
3. Nanoair-bridged lateral overgrowth of GaN on ordered nanoporous GaN template10.1063/1.2147716 ↗
4. Fabrication of porous anodic aluminium oxide layers on paper for humidity sensors10.1016/j.snb.2015.05.053 ↗
5. Sensitivity evolution and enhancement mechanism of porous anodic aluminum oxide humidity sensor using magnetic field10.1016/j.snb.2014.03.057 ↗
6. Nanostructuring of nickel hydroxide via a template solution approach for efficient electrochemical devices10.1002/smll.201303889 ↗
7. Template-assisted synthesis of Ni–Co bimetallic nanowires for urea electrocatalytic oxidation10.1007/s10800-015-0846-8 ↗
8. Template-grown high-density nanocapacitor arrays10.1063/1.1290598 ↗
9. Effect of sealing on the morphology of anodized aluminum oxide10.1016/j.corsci.2015.03.021 ↗
10. Corrosion properties of anodized aluminum: effects of equal channel angular pressing prior to anodization10.1016/j.corsci.2014.08.020 ↗
11. Super-hydrophobic surface treatment as corrosion protection for aluminum in seawater10.1016/j.corsci.2009.04.027 ↗
12. Corrosion behavior of superhydrophobic aluminum alloy in concentrated potassium halide solutions: when the specific anion effect is manifested10.1016/j.corsci.2016.08.019 ↗
13. Functionalized arrays of Raman-enhancing nanoparticles for capture and culture-free analysis of bacteria in human blood10.1038/ncomms1546 ↗
14. Surface plasmon resonance and interference coenhanced SERS substrate of AAO/Al-based Ag nanostructure arrays10.1021/jp5026152 ↗
15. Gap-tunable Ag-nanorod arrays on alumina nanotip arrays as effective SERS substrates10.1039/c3tc30669k ↗
16. Fabrication of high quality anodic aluminum oxide (AAO) on low purity aluminum—a comparative study with the AAO produced on high purity aluminum10.1016/j.electacta.2013.04.160 ↗
17. Porous anodic film formation on Al-Ti alloys in sulphuric acid10.1016/j.corsci.2011.12.035 ↗
18. The role and effect of residual stress on pore generation during anodization of aluminium thin films10.1016/j.corsci.2013.04.047 ↗
19. The effect of temperature and concentration on the self-organized pore formation in anodic alumina10.1088/0022-3727/38/14/015 ↗
20. Anodic films containing zirconia nanoparticles for corrosion protection of AA1050 aluminum alloy10.1007/s10008-013-2274-1 ↗
21. Influence of oxidation heat on hard anodic film of aluminum alloy10.1016/S1003-6326(11)61521-5 ↗
22. The electrical and mechanical properties of porous anodic 6061-T6 aluminum alloy oxide film10.1155/2015/343541 ↗
23. Effect of electrolyte concentration on the growth of porous anodic aluminium oxide (AAO) on Al-Mn alloys10.4028/www.scientific.net/AMR.626.610 ↗
24. Effect of anodizing voltage on the morphology and growth kinetics of porous anodic alumina on Al-0.5wt% Mn alloys10.4028/www.scientific.net/AMR.832.101 ↗
25. Self-ordering of anodic porous alumina formed in organic acid electrolytes10.1016/j.electacta.2005.05.058 ↗
26. Electropolishing of high-purity aluminium in perchloric acid and ethanol solutions10.1016/j.corsci.2009.01.030 ↗
27. Porous anodic alumina formed by anodization of aluminum alloy (AA1050) and high purity aluminum10.1016/j.electacta.2009.12.054 ↗
28. Switchable transparency and wetting of elastomeric smart windows10.1002/adma.201002320 ↗
29. Hybrid pulse anodization for the fabrication of porous anodic alumina films from commercial purity (99%) aluminum at room temperature10.1088/0957-4484/20/5/055301 ↗
30. Fabrication of enhanced anodic aluminum oxide performance at room temperatures using hybrid pulse anodization with effective cooling10.1016/j.electacta.2011.04.122 ↗
31. Anodic alumina membranes with defined pore diameters and thicknesses obtained by adjusting the anodizing duration and pore opening/widening time10.1007/s10008-011-1471-z ↗
32. Fast fabrication of long-range ordered porous alumina membranes by hard anodization10.1038/nmat1717 ↗
33. Effect of processing parameters on pore structure and thickness of anodic aluminum oxide (AAO) tubular membranes10.1016/j.memsci.2008.03.044 ↗
34. Anodization of nanoporous alumina on impurityinduced hemisphere curved surface of aluminum at room temperature10.1186/1556-276X-6-596 ↗
35. Heat capacities of magnesium oxide and hydroxide
36. Time-dependent surface speciation of oxalate at the water–boehmite (gamma-AlOOH) interface: implications for dissolution10.1016/S0016-7037(01)00750-5 ↗