journal article·2018-02

Copper transport and sulphide sequestration during copper corrosion in anaerobic aqueous sulphide solutions

J. Chen, Z. Qin, T. Martino, M. Guo, D.W. Shoesmith

Corrosion Science· Volume 131
Publisher page

Abstract

Abstract The corrosion of copper in aqueous solutions containing ≥5 × 10 −4 mol/L sulphide and the ensuing accumulation of corrosion product deposits (as chalcocite Cu 2 S) occurs non-uniformly indicating the occurrence of microgalvanic coupling between net anodic and net cathodic surface locations. A series of novel electrochemical experiments were designed to confirm the occurrence of this process and a series of analytical procedures used to identify the chemical nature of the transported Cu species. Transport was found to occur as copper sulphide complexes and clusters. It was also demonstrated that all the available sulphide was sequestered as deposited Cu 2 S.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Corrosion Behavior and Inhibition · Electrochemical Analysis and Applications · Concrete Corrosion and Durability

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (44)

Show source-provided references
1. Bird · 2007
2. Structure and growth mechanism of mineral dendrites10.1038/353409a0 ↗
3. The timing of mineral growth across a regional metamorphic sequence10.1038/357235a0 ↗
4. Annual growth banding in a cave stalagmite10.1038/364518a0 ↗
5. Nanominerals, mineral nanoparticles, and earth systems10.1126/science.1141134 ↗
6. Contribution to reproductive effort by photosynthesis of flowers and fruits10.1038/279554a0 ↗
7. Evidence of a feedback mechanism limiting plant response to elevated carbon dioxide10.1038/364616a0 ↗
8. Deformational mass transport and invasive processes in soil evolution10.1126/science.255.5045.695 ↗
9. Microorganisms and climate change: terrestrial feedbacks and mitigation options10.1038/nrmicro2439 ↗
10. Colloidal crystal films: advances in universality and perfection10.1021/ja0379969 ↗
11. Colloidal iron pyrite (FeS2) nanocrystal inks for thin-film photovoltaics10.1021/ja1096368 ↗
12. EPR evidence for Co (IV) species produced during water oxidation at neutral pH10.1021/ja1013344 ↗
13. Non-uniform film growth and micro/macro-galvanic corrosion of copper in aqueous sulphide solutions containing chloride10.1016/j.corsci.2016.10.024 ↗
14. Comparison of [Cu2+] measurements in lake water determined by ligand exchange and cathodic stripping voltammetry and by ion-selective electrode10.1021/es960551i ↗
15. Evidence for multinuclear Fe, Cu and Zn molecular sulfide clusters in oxic river waters10.1038/35022561 ↗
16. Copper (I) tert-butylthiolato clusters as single-source precursors for high-quality chalcocite thin films: film growth and microstructure control10.1021/cm0700495 ↗
17. Kinetics of corrosion film growth on copper in neutral chloride solutions containing small concentrations of sulfide10.1149/1.3478570 ↗
18. Long-term corrosion of copper in a dilute anaerobic sulfide solution10.1016/j.electacta.2011.04.086 ↗
19. Rate controlling reactions for copper corrosion in anaerobic aqueous sulphide solutions10.1179/1743278210Y.0000000007 ↗
20. The influence of sulphide transport on the growth and properties of copper sulphide films on copper10.1016/j.corsci.2014.06.027 ↗
21. The mechanism of accelerated corrosion of copper-nickel alloys in sulphide-polluted seawater10.1016/0010-938X(81)90030-5 ↗
22. The flow corrosion mechanism of copper base alloys in sea water in the presence of sulphide contamination10.1016/0010-938X(82)90057-9 ↗
23. The accelerated corrosion of Cu- Ni alloys in sulphide-polluted seawater: mechanism no. 210.1016/0010-938X(83)90104-X ↗
24. The use of high speed rotating disc electrodes for the study of erosion-corrosion of copper base alloys in sea water10.1016/0010-938X(88)90091-1 ↗
25. A study of the de-alloying of 70Cu-30Ni commercial alloy in sulphide polluted and unpolluted sea water10.1016/0010-938X(91)90137-E ↗
26. The corrosion of copper-nickel alloys in sulfide-polluted seawater: the effect of sulfide concentration10.1016/0010-938X(93)90266-J ↗
27. The atmospheric corrosion of copper by hydrogen sulphide in underground conditions10.1016/S0010-938X(03)00112-4 ↗
28. Corrosion of copper in 3% NaCl solution polluted by sulphide ions10.1016/j.corsci.2005.06.017 ↗
29. Assessing the corrosion performance of high-level nuclear waste containers10.5006/1.3278296 ↗
30. Corrosion issues in nuclear waste disposal10.1016/j.jnucmat.2008.06.023 ↗
31. Modelling long term corrosion behaviour of copper canisters in KBS-3 repository10.1179/18211Y.0000000004 ↗
32. The NBS tables of chemical thermodynamic properties
33. The electrochemical response of preoxidized copper in aqueous sulfide solutions10.1149/1.2745647 ↗
34. Potential-pH diagrams for sulfur and hydroxyl adsorbed on copper surfaces in water containing sulfides, sulfites or thiosulfates10.1016/S0010-938X(02)00210-X ↗
35. X-ray absorption spectroscopy of electrochemically oxidized Cu exposed to Na2S10.1016/j.corsci.2011.09.001 ↗
36. Studies on copper-semiconducting layer-electrolyte systems—II. Galvanostatic anodic polarization of Cu/Cu2S/S2− applying stationary and rectangular pulse techniques10.1016/0010-938X(73)90011-5 ↗
37. Ore solution chemistry; V, solubilities of chalcopyrite and chalcocite assemblages in hydrothermal solution at 200degrees to 350degreesC10.2113/gsecongeo.71.4.772 ↗
38. The hydrosulphide/sulphide complexes of copper (I): Experimental determination of stoichiometry and stability at 22°C and reassessment of high temperature data10.1016/S0016-7037(98)00288-9 ↗
39. Unification of the copper (I) binding affinities of the metallo-chaperones Atx1, Atox1, and related proteins detection probes and affinity standards10.1074/jbc.M110.213074 ↗
40. C-terminal domain of the membrane copper transporter Ctr1 from saccharomyces cerevisiae binds four Cu(I) ions as a cuprous-thiolate polynuclear cluster: sub-femtomolar Cu(I) affinity of three proteins involved in copper trafficking10.1021/ja0390350 ↗
41. Simple procedure for the single sample determination of serum copper and iron10.1016/0009-8981(58)90021-4 ↗
42. Voltammetry study of copper in chloride solution10.1016/0013-4686(88)80192-0 ↗
43. D.R. Lide, CRC Handbook of Chemistry and Physics, CRC press, 2003–2004.
44. Corrosion of copper-coated steel high level nuclear waste containers under permanent disposal conditions10.1016/j.electacta.2016.05.135 ↗