The kinetics and mechanism of filiform corrosion occurring on zinc-aluminium-magnesium coated steel
Source abstract
Abstract
This paper describes a systematic study into the initiation and propagation of filiform corrosion (FFC) on industrially important Zinc-Aluminium-Magnesium (ZAM) alloy coatings for steels. An artificial scribe defect is created in model organic coatings applied to ZAM. Corrosion is initiated using HCl, NaCl, FeCl2 and acetic acid. Only acetic acid is able to reproducibly initiate FFC. The FFC (area) rate is shown to be proportional to the amount of acetic acid introduced. The FFC mechanism is explained in terms of the relative susceptibility of alloy phases to anodic dissolution, determined using scanning electron microscopy and scanning Kelvin probe force microscopy.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Corrosion Behavior and Inhibition · Concrete Corrosion and Durability · Anodic Oxide Films and Nanostructures
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (80)
Show source-provided references
1. Understanding corrosion via corrosion product characterization: II. Role of alloying elements in improving the corrosion resistance of Zn–Al–Mg coatings on steel10.1016/j.corsci.2011.03.016 ↗
2. The initial release of zinc and aluminium from non-treated Galvalume and the formation of corrosion products in chloride containing media10.1016/j.apsusc.2011.12.112 ↗
3. In situ monitoring of corrosion mechanisms and phosphate inhibitor surface deposition during corrosion of zinc–magnesium–aluminium (ZMA) alloys using novel time-lapse microscopy10.1039/C4FD00251B ↗
4. Nanoscopic view on the initial stages of corrosion of hot dip galvanized Zn–Mg–Al coatings10.1016/j.corsci.2014.02.027 ↗
5. The effect of pH on the selective dissolution of Zn and Al from Zn–Al coatings on steel10.1016/j.corsci.2012.09.042 ↗
6. Corrosion mechanisms of Zn(Mg,Al) coated steel: 2. The effect of Mg and Al alloying on the formation and properties of corrosion products in different electrolytes10.1016/j.corsci.2014.07.042 ↗
7. Composition of corrosion products formed on Zn–Mg, Zn–Al and Zn–Al–Mg coatings in model atmospheric conditions10.1016/j.corsci.2014.05.016 ↗
8. The effect of an artificially synthesized simonkolleite layer on the corrosion of electrogalvanized steel10.1016/j.corsci.2012.10.024 ↗
9. Aqueous corrosion of Mg-Al binary alloys: roles of Al and Mg10.5006/i0010-9312-68-6-557 ↗
10. Zr-based conversion layer on Zn-Al-Mg alloy coated steel sheets: insights into the formation mechanism10.1016/j.electacta.2014.05.163 ↗
11. Corrosion of zinc–magnesium coatings: mechanism of paint delamination10.1016/j.corsci.2009.05.042 ↗
12. Innovative steel strip coatings by means of PVD in a continuous pilot line: process technology and coating development10.1016/S0257-8972(02)00660-6 ↗
13. The effect of Mg concentration on the resistance of PVD Zn-Mg coatings to corrosion driven organic coating delamination10.1016/j.corsci.2015.08.036 ↗
14. XPS investigation on the surface chemistry of corrosion products on ZnMgAl-coated steel10.1007/s00216-013-7099-3 ↗
15. Corrosion behaviour of Zn–Al–Mg coated steel sheet in sodium chloride-containing environment10.1016/j.corsci.2009.06.019 ↗
16. Corrosion performance of Zn–Al–Mg coatings in open and confined zones in conditions simulating automotive applications10.1002/maco.200905425 ↗
17. Activation and inhibition of Zn–Al and Zn–Al–Mg coatings on steel by nitrate in phosphoric acid solution10.1016/j.corsci.2012.03.028 ↗
18. In situ monitoring of the microstructural corrosion mechanisms of zinc–magnesium–aluminium alloys using time lapse microscopy10.1016/j.corsci.2011.02.043 ↗
19. Microstructural changes in zinc aluminium alloy galvanising as a function of processing parameters and their influence on corrosion10.1016/j.corsci.2004.11.011 ↗
20. The effect of magnesium additions on the microstructure and cut edge corrosion resistance of zinc aluminium alloy galvanised steel10.1016/j.corsci.2008.02.005 ↗
21. Corrosion mechanism of model zinc–magnesium alloys in atmospheric conditions10.1016/j.corsci.2008.06.008 ↗
22. Atmospheric corrosion of ZnAlMg coated steel during long term atmospheric weathering at different worldwide exposure sites10.1016/j.corsci.2018.12.033 ↗
23. Effect of the microstructure of Zn-Al and Zn-Al-Mg model alloys on corrosion stability10.1016/j.corsci.2016.04.022 ↗
24. Chemistry of corrosion products of Zn and MgZn pure phases under atmospheric conditions10.1016/j.corsci.2012.08.014 ↗
25. Investigation of the corrosion behaviors of continuously hot-dip galvanizing Zn-Mg coating10.1016/j.surfcoat.2012.03.079 ↗
26. Understanding corrosion via corrosion product characterization: I. Case study of the role of Mg alloying in Zn-Mg coating on steel10.1016/j.corsci.2009.03.005 ↗
27. Corrosion resistance of zinc-magnesium coated steel10.1016/j.corsci.2007.03.032 ↗
28. Delamination resistant zinc alloys: simple concept and results on the system zinc‐magnesium10.1002/srin.200300212 ↗
29. The physical meaning of electrode potentials at metal surfaces and Polymer/Metal interfaces: consequences for delamination corrosion, passivation, and anodic films10.1149/1.2926589 ↗
30. Zn-Mg and Zn-Mg-Al alloys for improved corrosion protection of steel: some new aspects10.1002/maco.201307586 ↗
31. Underfilm/coating corrosion
32. The delamination of polymeric coatings from steel. Part 1: calibration of the Kelvinprobe and basic delamination mechanism10.1016/S0010-938X(98)00166-8 ↗
33. The delamination of polymeric coatings from steel. Part 2: first stage of delamination, effect of type and concentration of cations on delamination, chemical analysis of the interface10.1016/S0010-938X(98)00167-X ↗
34. Chromate inhibition of corrosion-driven organic coating delamination studied using a scanning kelvin probe technique10.1149/1.1396336 ↗
35. Investigation of the delamination of polymer films from galvanized steel with the Scanning Kelvinprobe
36. The delamination of polymeric coatings from electrogalvanised steel – a mechanistic approach.: part 1: delamination from a defect with intact zinc layer10.1016/S0010-938X(00)00047-0 ↗
37. The delamination of polymeric coatings from electrogalvanized steel – a mechanistic approach.: part 2: delamination from a defect down to steel10.1016/S0010-938X(00)00048-2 ↗
38. The delamination of polymeric coatings from electrogalvanized steel – a mechanistic approach.: part 3: delamination kinetics and influence of CO210.1016/S0010-938X(00)00049-4 ↗
39. Electrochemical studies of the inhibition of the cathodic delamination of organically coated galvanised steel by thin conversion films10.1016/j.electacta.2007.05.045 ↗
40. Nanoscale analysis of surface oxides on ZnMgAl hot-dip-coated steel sheets10.1007/s00216-011-5507-0 ↗
41. Microstructural characterization and quantification of Zn–Al–Mg surface coatings10.1016/j.matchar.2010.06.008 ↗
42. Filiform corrosion in polymer-coated metals10.1016/0300-9440(95)00555-2 ↗
43. An analysis of mass transfer in filiform corrosion10.5006/1.3581907 ↗
44. Corrosion protection by organic coatings: electrochemical mechanism and novel methods of investigation10.1016/S0013-4686(00)00348-0 ↗
45. The effect of oxygen partial pressure on the filiform corrosion of organic coated iron10.1016/j.corsci.2014.08.004 ↗
46. Mechanism of filiform corrosion10.1021/ie50533a053 ↗
47. Scanning kelvinprobe investigations of filiform corrosion on aluminum alloy 2024-t310.1016/S0010-938X(98)00044-4 ↗
48. New knowledge on localized corrosion obtained from local measuring techniques10.1016/S0013-4686(01)00642-9 ↗
49. Effect of climatic parameters on filiform corrosion of coated aluminum alloys10.5006/1.3287763 ↗
50. The kinetics of chloride-induced filiform corrosion on aluminum alloy AA2024-T310.1149/1.1589020 ↗
51. Chromate inhibition of filiform corrosion on organic coated AA2024-T3 studied using the scanning kelvin probe10.1149/1.1757460 ↗
52. Chloride-induced filiform corrosion of organic-coated magnesium10.1016/j.electacta.2010.09.005 ↗
53. The mechanism of group (I) chloride initiated filiform corrosion on iron10.1016/j.elecom.2003.08.008 ↗
54. The kinetics and mechanisms of filiform corrosion on aluminium alloy AA611110.1016/j.electacta.2010.04.035 ↗
55. The role of chromate in filiform corrosion inhibition10.1016/S0013-4686(03)00256-1 ↗
56. The role of chromate in filiform corrosion inhibition10.1016/S0013-4686(02)00829-0 ↗
57. Award lecture: molecular in situ studies of atmospheric corrosion10.5006/1.3278420 ↗
58. Atmospheric corrosion of zinc by organic constituents: I. The role of the Zinc/Water and Water/Air interfaces studied by infrared Reflection/Absorption spectroscopy and vibrational sum frequency spectroscopy10.1149/1.2164788 ↗
59. Atmospheric corrosion of zinc by organic constituents: II. Reaction routes for zinc-acetate formation10.1149/1.2360740 ↗
60. GILDES model simulations of the atmospheric corrosion of zinc induced by low concentrations of carboxylic acids10.1149/2.072203jes ↗
61. Initial atmospheric corrosion of zinc induced by carboxylic acids: a quantitative in situ study10.1149/1.3240878 ↗
62. Molecular structural information of the atmospheric corrosion of zinc studied by vibrational spectroscopy techniques: I. Experimental approach10.1149/1.3479207 ↗
63. Molecular structural information of the atmospheric corrosion of zinc studied by vibrational spectroscopy techniques: II. Two and three-dimensional growth of reaction products induced by formic and acetic acid10.1149/1.3479255 ↗
64. Metal carboxylate formation during indoor atmospheric corrosion of Cu, Zn, and Ni10.1149/1.2048598 ↗
65. Characterisation of corrosivity in indoor atmospheres with different metals and evaluation techniques10.1179/bcj.1998.33.1.59 ↗
66. Polyaniline inhibition of corrosion-driven organic coating cathodic delamination on Iron10.1149/1.1850857 ↗
67. Latent fingerprint detection using a scanning Kelvin microprobe10.1520/JFS15103J ↗
68. Resolution and contrast in Kelvin probe force microscopy10.1063/1.368181 ↗
69. Evaluation of the capacitive force between an atomic force microscopy tip and a metallic surface10.1007/s100510050219 ↗
70. Electrostatic forces acting on the tip in atomic force microscopy: modelization and comparison with analytic expressions10.1063/1.363884 ↗
71. Characterization of AA2024‐T3 by scanning kelvin probe force microscopy10.1149/1.1838633 ↗
72. Probe diameter and probe-specimen distance dependence in the lateral resolution of a scanning Kelvin probe10.1063/1.1430546 ↗
73. The kinetics and mechanism of cathodic oxygen reduction on zinc and zinc–aluminium alloy galvanized coatings10.1016/j.corsci.2005.05.036 ↗
74. The introduction of magnesium and hydrogen introduction in sputtered zinc oxide thin films10.1016/j.tsf.2005.07.066 ↗
75. A semiempirical correlation between the optical band gap of hydroxides and the electronegativity of their constituents10.1007/BF02757695 ↗
76. Corrosion performance of Zn–Mg–Al coated steel in accelerated corrosion tests used in the automotive industry and field exposures10.1002/maco.201206959 ↗
77. Cathodic self-healing at cut-edges: the effect of Zn2+ and Mg2+ ions10.1016/j.corsci.2012.08.008 ↗
78. Dealloying of MgZn2Intermetallic in slightly alkaline chloride electrolyte and its significance in corrosion resistance10.1149/2.0341714jes ↗
79. In situ detection of differences in the electrochemical activity of Al2Cu IMPs and investigation of their effect on FFC by scanning Kelvin probe force microscopy10.1016/j.corsci.2012.02.006 ↗
80. Layered zinc hydroxide monolayers by hydrolysis of organozincs10.1039/C7SC04256F ↗