journal article·2020-05

Versatility of potential protective layer material Ti2AlC on resisting CMAS corrosion to thermal barrier coatings

Zheng Yan, Lei Guo, Zhao Zhang, Xiaohui Wang, Fuxing Ye

Corrosion Science· Volume 167
Publisher page

Abstract

Abstract Alleviating calcium-magnesium-alumina-silicate (CMAS) hazard to thermal barrier coatings (TBCs) has attracted increasing attentions. Here, we demonstrate that Ti2AlC is a promising protective layer material for TBCs against CMAS attack, and clarify its corrosion resistance mechanisms. The results reveal that pre-oxidized Ti2AlC has obvious advantages over its non-oxidized counterpart on promoting CMAS crystallization and inhibiting the melt infiltration. Pre-oxidation produces a continuous Al2O3 layer and TiO2 particles on Ti2AlC surface, and Al2O3 reacts with molten CMAS to form anorthite crystals, while TiO2, in the form of either Ti-rich particles or Ti dissolution (there is a content threshold), promotes the crystallization.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: High-Temperature Coating Behaviors · Advanced ceramic materials synthesis · MXene and MAX Phase Materials

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (51)

Show source-provided references
1. Microstructure based material sand particulate interactions and assessment of coatings for high temperature turbine blades
2. Effect of semi-molten particulate on tailored thermal barrier coatings for gas turbine engine, 52nd AIAA/SAE/ASEE joint propulsion conference
3. Particle transport analysis of sand ingestion in gas turbine jet engines, 53rd AIAA/SAE/ASEE joint propulsion conference
4. Thermal-barrier coatings for more efficient gas-turbine engines10.1557/mrs.2012.232 ↗
5. High-entropy pyrochlores with low thermal conductivity for thermal barrier coating materials10.1007/s40145-019-0342-4 ↗
6. Role of environmental deposits and operating surface temperature in spallation of air plasma sprayed thermal barrier coatings10.1016/S0257-8972(96)02994-5 ↗
7. Fabrication and growing kinetics of highly dispersed gadolinium zirconate nanoparticles
8. Overview on advanced thermal barrier coatings10.1016/j.surfcoat.2010.08.151 ↗
9. The Chemistry of Saudi Arabian Sand: A Deposition Problem on Helicopter Turbine Airfoils
10. CMAS effects on ship gas-turbine Components/Materials
11. Environmental degradation of thermal-barrier coatings by molten deposits10.1557/mrs.2012.230 ↗
12. Calcia-magnesia-alumino-silicate (CMAS)-induced degradation and failure of air plasma sprayed yttria-stabilized zirconia thermal barrier coatings10.1016/j.actamat.2015.12.044 ↗
13. Silicate deposit degradation of engineered coatings in gas turbines: progress toward models and materials solutions10.1146/annurev-matsci-010917-105000 ↗
14. Mechanism of crack nucleation and growth in YSZ thermal barrier coatings corroded by CMAS at high temperatures: first-principles calculation10.1016/j.corsci.2018.07.033 ↗
15. Mechanisms of cracking and delamination within thick thermal barrier systems in aero-engines subject to calcium-magnesium-alumino-silicate (CMAS) penetration10.1016/j.msea.2008.01.006 ↗
16. A delamination mechanism for thermal barrier coatings subject to calcium-magnesium-alumino-silicate (CMAS) infiltration10.1016/j.actamat.2004.11.028 ↗
17. Microstructure and thermo-physical properties of yttria stabilized zirconia coatings with CMAS deposits, J. Eur10.1016/j.jeurceramsoc.2011.04.006 ↗
18. Jet engine coatings for resisting volcanic ash damage10.1002/adma.201004783 ↗
19. Thermochemical interaction of thermal barrier coatings with molten CaO-MgO-Al2O3-SiO2 (CMAS) deposits10.1111/j.1551-2916.2006.01209.x ↗
20. Infiltration-inhibiting reaction of gadolinium zirconate thermal barrier coatings with CMAS melts10.1111/j.1551-2916.2007.02175.x ↗
21. Plasma-sprayed La2Ce2O7 thermal barrier coatings against calcium-magnesium-alumina-silicate penetration10.1016/j.jeurceramsoc.2014.02.031 ↗
22. Hot corrosion behavior of La2(Zr0.7Ce0.3)2O7 thermal barrier coating ceramics exposed to molten calcium magnesium aluminosilicate at different temperatures10.1016/j.corsci.2015.08.031 ↗
23. La2(Zr0.7Ce0.3)2O7 thermal barrier coating prepared by electron beam-physical vapor deposition that are resistant to high temperature attack by molten silicate10.1016/j.corsci.2016.11.015 ↗
24. Plasma sprayed nanostructured GdPO4 thermal barrier coatings: preparation microstructure and CMAS corrosion resistance10.1111/jace.14924 ↗
25. CMAS resistance characteristics of LaPO4/YSZ thermal barrier coatings at 1250°C-1350°C10.1016/j.corsci.2019.04.014 ↗
26. Composition-microstructure-mechanical property relationships and toughening mechanisms of GdPO4-doped Gd2Zr2O7 composites10.1016/j.compositesb.2018.12.135 ↗
27. Thermal cycling failure of new LaMgAl11O19/YSZ double ceramic top coat thermal barrier coating systems10.1016/j.surfcoat.2010.11.059 ↗
28. Thermal shock behavior of toughened gadolinium zirconate/YSZ double-ceramic-layered thermal barrier coating10.1016/j.jallcom.2014.01.060 ↗
29. Novel thermal barrier coatings that are resistant to high-temperature attack by glassy deposits10.1016/j.actamat.2007.08.028 ↗
30. Air-plasma-sprayed thermal barrier coatings that are resistant to high-temperature attack by glassy deposits10.1016/j.actamat.2010.09.013 ↗
31. Protectiveness of Pt and Gd2Zr2O7 layers on EB-PVD YSZ thermal barrier coatings against calcium-magnesium-alumina-silicate (CMAS) attack10.1016/j.ceramint.2015.05.128 ↗
32. CMAS-resistant thermal barrier coatings (TBC)10.1111/j.1744-7402.2009.02373.x ↗
33. Electrophoretically deposited alumina as protective overlay for thermal barrier coatings against CMAS degradation10.1016/j.surfcoat.2009.09.055 ↗
34. In situ synthesis of α-alumina layer on thermal barrier coating for protection against CMAS (CaO-MgO-Al2O3-SiO2) corrosion10.1016/j.surfcoat.2014.11.064 ↗
35. Ti2AlC MAX phase for resistance against CMAS attack to thermal barrier coatings10.1016/j.ceramint.2019.01.059 ↗
36. Solid-liquid reaction synthesis and simultaneous densification of polycrystalline Ti2AlC10.3139/146.020066 ↗
37. Effects of laser glazing on CMAS corrosion behavior of Y2O3 stabilized ZrO2 thermal barrier coatings10.1016/j.corsci.2019.06.025 ↗
38. Microstructural evolution during high-temperature oxidation of Ti2AlC ceramics10.1016/j.actamat.2011.03.035 ↗
39. Microstructure characteristics of EB-PVD YSZ thermal barrier coatings corroded by molten volcanic ash10.1016/j.surfcoat.2015.12.003 ↗
40. Microstructure and residual stress of alumina scale formed on Ti2AlC at high temperature in air10.1007/s11085-007-9063-0 ↗
41. Microstructures and adhesion of the oxide scale formed on titanium aluminum carbide substrates10.1111/j.1551-2916.2006.01141.x ↗
42. Alumina forming high temperature silicides and carbides10.1016/j.ceramint.2003.12.046 ↗
43. Equilibrium relationships between thermal barrier oxides and silicate melts10.1016/j.actamat.2016.08.077 ↗
44. FactSage thermochemical software and databases-recent developments10.1016/j.calphad.2008.09.009 ↗
45. The effect of TiO2 additions on CaO-MgO-Al2O3-SiO2 (CMAS) crystallization behavior from the melt10.1111/jace.16180 ↗
46. High temperature viscosity of calcium-magnesium aluminosilicate glass from synthetic sand10.1016/j.scriptamat.2016.07.020 ↗
47. Microstructure characteristics for anorthite composite glass with nucleating agents of TiO2 under non-isothermal crystallization10.1016/S0025-5408(02)00873-5 ↗
48. Solubility reactivity and nucleation effect of Cr2O3 in the CaO-MgO-Al2O3-SiO2 glassy system10.1007/BF00354571 ↗
49. Effect of Cr2O3, Fe2O3 and TiO2 nucleants on the crystallization behaviour of SiO2-Al2O3-CaO-MgO (R2O) glass-ceramics10.1016/j.ceramint.2004.03.037 ↗
50. Microstructure of high velocity oxy-fuel sprayed Ti2AlC coatings10.1007/s10853-010-4263-4 ↗
51. Cold spraying of Ti2AlC MAX-phase coatings10.1007/s11666-012-9843-1 ↗