Investigation of the oxidation mechanisms of superlattice Cr-CrN/TiSiN-Cr multilayer coatings on Zircaloy substrates under high-temperature steam atmospheres
Source abstract
Abstract
Abstract Cr-CrN/TiSiN-Cr multilayer coatings were deposited on Zircaloy substrates by multi-arc ion plating, and the microstructure and oxidation behavior of the as-deposited coatings, specifically the middle CrN/TiSiN layer, were investigated. The CrN/TiSiN layer exhibited a superlattice structure. The multilayer coatings effectively protected the Zircaloy substrates from oxidation. (Cr1-xTix)2O3 and Cr2TiO5 phases were produced in the coating after oxidation at 1200 °C for 1500 s. With oxidation time increases, most of the Cr atoms in these two phases were replaced by Ti atoms. Oxidation mechanisms of the as-deposited coatings are discussed and a decomposition model of the superlattice CrN/TiSiN layer is proposed.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Nuclear Materials and Properties · Metal and Thin Film Mechanics · High-Temperature Coating Behaviors
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (54)
Show source-provided references
1. Comprehensive nuclear materials!zirconium alloys: properties and characteristics10.1016/B978-0-08-056033-5.00015-X ↗
2. Review of stress fields in zirconium alloys corrosion scales10.1016/j.corsci.2015.03.004 ↗
3. Investigation of oxide layers formed on zircaloy-4 coarse-grained specimens corroded at 360° C in lithiated aqueous solution10.1016/j.corsci.2014.12.012 ↗
4. Phase transformation of oxide film in zirconium alloy in high temperature hydrogenated water10.1016/j.corsci.2015.06.034 ↗
5. A study of the breakaway oxidation behavior of zirconium cladding materials10.1016/j.jnucmat.2011.06.039 ↗
6. Corrosion and high-temperature steam oxidation of E110 alloy and its laser welds after ion irradiation10.1016/j.corsci.2019.02.031 ↗
7. Experimental study and numerical simulation of high temperature (1100–1250° C) oxidation of prior-oxidized zirconium alloy10.1016/j.corsci.2015.10.018 ↗
8. Enhanced high-temperature oxidation resistance of a zirconium alloy cladding by high-temperature preformed oxide on the cladding10.1016/j.corsci.2017.11.019 ↗
9. Accident tolerant fuel cladding development: promise, status, and challenges10.1016/j.jnucmat.2017.12.043 ↗
10. Preliminary assessment of accident-tolerant fuels on LWR performance during normal operation and under DB and BDB accident conditions10.1016/j.jnucmat.2013.09.052 ↗
11. Material selection for accident tolerant fuel cladding
12. Protective coatings on zirconium-based alloys as accident-tolerant fuel (ATF) claddings10.1515/corrrev-2017-0010 ↗
13. Corrosion of the bonding at FeCrAl/Zr alloy interfaces in steam10.1016/j.jnucmat.2018.05.071 ↗
14. An interesting oxidation phenomenon of Cr coatings on Zry-4 substrates in high temperature steam environment10.1016/j.corsci.2019.05.017 ↗
15. High temperature steam oxidation of chromium-coated zirconium-based alloys: kinetics and process10.1016/j.corsci.2020.108537 ↗
16. Oxidation behavior, thermal stability, and the coating/substrate interface evolution of CrN-coated Zircaloy under high-temperature steam10.1016/j.corsci.2021.109416 ↗
17. Investigation of oxidation behaviors of coated Zircaloy as accident-tolerant fuel with CrAlN and CrAlSiN coatings in high-temperature steam10.1016/j.corsci.2020.108896 ↗
18. Microstructure, corrosion resistance and oxidation behavior of Cr-coatings on Zircaloy-4 prepared by vacuum arc plasma deposition10.1016/j.corsci.2019.06.029 ↗
19. A systematic study of the oxidation behavior of Cr coatings on Zry4 substrates in high temperature steam environment10.1016/j.corsci.2020.108826 ↗
20. High temperature oxidation and microstructural evolution of cold spray chromium coatings on Zircaloy-4 in steam environments10.1016/j.jnucmat.2019.151737 ↗
21. Oxidation kinetics of Cr-coated zirconium alloy: Effect of coating thickness and microstructure10.1016/j.corsci.2020.108883 ↗
22. High temperature Cr-Zr interaction of two types of Cr-coated Zr alloys in inert gas environment10.1016/j.jnucmat.2021.152806 ↗
23. Study of the oxidation behavior of CrN coating on Zr alloy in air10.1016/j.jnucmat.2019.01.006 ↗
24. Long-term high temperature oxidation of CrAl (Y) N coatings in steam atmosphere10.1016/j.corsci.2013.11.066 ↗
25. Synthesis and oxidation resistance of TiAlSiN and multilayer TiAlSiN/CrAlN coating10.1016/j.surfcoat.2009.04.027 ↗
26. Thermally induced transitions of CrN thin films10.1016/j.scriptamat.2007.03.058 ↗
27. Comparative study of CrAlSiN monolayer and CrN/AlSiN superlattice multilayer coatings: behavior at high temperature in steam atmosphere10.1016/j.jallcom.2018.11.199 ↗
28. A superhard CrAlSiN superlattice coating deposited by multi-arc ion plating: I. Microstructure and mechanical properties10.1016/j.surfcoat.2012.05.144 ↗
29. A superhard CrAlSiN superlattice coating deposited by a multi-arc ion plating: II. Thermal stability and oxidation resistance10.1016/j.surfcoat.2012.05.143 ↗
30. Wear and corrosion resistance of CrN/TiN superlattice coatings deposited by a combined deep oscillation magnetron sputtering and pulsed dc magnetron sputtering10.1016/j.apsusc.2015.05.110 ↗
31. Corrosion mechanism investigation of TiAlN/CrN superlattice coating by multi-arc ion plating in 3.5 wt% NaCl solution10.1016/j.surfcoat.2020.125660 ↗
32. Helium irradiation induced ultra-high strength nanotwinned Cu with nanovoids10.1016/j.actamat.2019.07.003 ↗
33. Comparative study on protective properties of CrN coatings on the ABS substrate by DCMS and HiPIMS techniques10.1016/j.surfcoat.2020.125890 ↗
34. Effects of multi-layer structure on microstructure, wear and erosion performance of the Cr/CrN films on Ti alloy substrate10.1016/j.apsusc.2019.04.008 ↗
35. Oxidation behavior of Si-doped nanocomposite CrAlSiN coatings. Surface and coatings technology
36. CrAlSiN nanocomposite thin films for high-speed machining applications10.1080/10426914.2017.1303157 ↗
37. Stresses in NiO, Cr2O3 and Al2O3 oxide scales10.1016/0921-5093(94)09747-X ↗
38. High temperature oxidation behavior of quaternary ordered (Cr2/3Ti1/3)3AlC2-based MAX ceramic10.1016/j.corsci.2021.109317 ↗
39. Thermal stability and oxidation resistance of Ti–Al–N coatings10.1016/j.surfcoat.2011.12.028 ↗
40. Deposition, characterization and high-temperature steam oxidation behavior of single-phase Ti2AlC-coated Zircaloy-410.1016/j.corsci.2018.02.035 ↗
41. Breakaway oxidation of Ti3AlC2 during long-term exposure in air at 1100 °C10.1016/j.corsci.2015.12.001 ↗
42. Thickness-dependent oxidation behaviors of Ti3AlC2 foils at 1100 °C in air10.1016/j.corsci.2021.109431 ↗
43. Synthesis of CrN/AlN superlattice coatings using closed-field unbalanced magnetron sputtering process10.1016/S0257-8972(03)00244-5 ↗
44. Corrosion mechanism investigation of TiAlN/CrN superlattice coating by multi-arc ion plating in 3.5 wt% NaCl solution10.1016/j.surfcoat.2020.125660 ↗
45. The crystalline structure, hardness and thermal stability of AlN/CrN superlattice coating prepared by D.C. magnetron sputtering10.1016/j.surfcoat.2005.08.099 ↗
46. Thermal stability of CrN/AlN superlattice coatings10.1016/j.surfcoat.2013.12.035 ↗
47. Growth mechanism of Cr2O3 scales: oxygen and chromium diffusion, oxidation kinetics and effect of yttrium10.1016/0921-5093(96)10173-8 ↗
48. Diffusion of 54Cr and 18O in Cr2O 3 scales and growth mechanism10.4028/www.scientific.net/DDF.143-147.1195 ↗
49. High temperature oxidation of TiCrN coatings deposited on a steel substrate by ion plating10.1016/S0257-8972(01)01237-3 ↗
50. Experimental observations in support of the dynamic-segregation theory to explain the reactive-element effect10.1007/BF01046818 ↗
51. Oxidation kinetics of TiN thin films10.1063/1.328659 ↗
52. High-temperature oxidation behaviors of the (Ti 1− x Cr x) N coatings10.1023/A:1014992125235 ↗
53. TEM study on oxidized TiCrN coatings ion-plated on a steel substrate10.1016/S0257-8972(03)00519-X ↗
54. The compound Cr2TiO5 in the system Cr2O3·TiO210.1016/0022-4596(79)90054-9 ↗