Effect of Ce on oxidation behaviour and microstructure evolution of a nickel-saving austenitic heat-resistant cast steel

Tianlong Liu, Kaihong Zheng, Juan Wang, Yingfei Lin, Zhibin Zheng, Jun Long

Corrosion Science· Volume 166
Publisher page

Abstract

Abstract The effect of Ce on the oxidation behaviour and microstructure evolution of nickel-saving austenitic heat-resistant cast steel in air at 900 °C was investigated by performing the isothermal oxidation tests. After 200 h of oxidation, the oxidation resistance of Ce-containing steel was about 20 % higher than that of Ce-free steel. In addition to its role as a reactive element, alloyed Ce slowed the rate of manganese depletion from the substrate and subsurface ferrite formation, leading to the improvement of the oxidation resistance of Ce-containing steel.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: High-Temperature Coating Behaviors · Metallurgical Processes and Thermodynamics · Corrosion Behavior and Inhibition

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (67)

Show source-provided references
1. Honeycombe · 1981
2. A review on nickel-free nitrogen containing austenitic stainless steels for biomedical applications10.1016/j.msec.2013.06.002 ↗
3. High-temperature oxidation studies of low-nickel austenitic stainless steel. Part I: Isothermal oxidation10.1023/A:1010329310030 ↗
4. High-temperature oxidation studies of low-nickel austenitic stainless steel. Part II: Cyclic oxidation10.1023/A:1010337530502 ↗
5. Efforts to save nickel in austenitic stainless steels10.2355/isijinternational.47.359 ↗
6. Effects of combined addition of carbon and nitrogen on pitting corrosion behavior of Fe–18Cr–10Mn alloys10.1016/j.scriptamat.2009.03.018 ↗
7. Low strain rate deformation behavior of a Cr–Mn austenitic steel at -80°C10.1016/j.actamat.2012.07.055 ↗
8. Breakaway oxidation of austenitic stainless steels induced by alloyed sulphur10.1016/j.corsci.2015.01.007 ↗
9. Oxidation of a Fe–18Cr–8Ni austenitic stainless steel at 850°C in O2: microstructure evolution during breakaway oxidation10.1016/j.corsci.2016.10.029 ↗
10. Characterization of refractory steel oxidation at high temperature10.1016/j.corsci.2017.12.029 ↗
11. The influence of manganese on the high-temperature oxidation of iron-chromium alloys10.1002/maco.19890400403 ↗
12. The air oxidation of an austenitic Fe-Mn-Cr stainless steel for fusion-reactor applications10.1007/BF00655899 ↗
13. Roles of manganese in the high-temperature oxidation resistance of alumina-forming austenitic steels at above 800°C10.1007/s11085-012-9311-9 ↗
14. The oxidation of Iron-chromium-manganese alloys at 900°C10.1007/BF00938460 ↗
15. Oxidation behaviour of an austenitic Fe-30Mn-5Al-0.5C alloy10.1016/S0010-938X(01)00043-9 ↗
16. Internal oxidation of Fe-Mn-Cr Steels, simulations and experiments10.1007/s11085-018-9836-7 ↗
17. Effect of Mn on oxide formation by Fe-Cr and Fe-Cr-Ni alloys in dry and wet CO2 gases at 650°C10.1016/j.corsci.2016.07.014 ↗
18. Effect of addition of 4%Al on the high temperature oxidation and nitridation of a 20Cr–25Ni austenitic stainless steel10.1007/s11085-014-9503-6 ↗
19. The Influence of temperature on the oxidation mechanism in air of HR3C and aluminum-aontaining 22Cr-25Ni austenitic stainless steels10.1007/s11085-017-9817-2 ↗
20. High temperature corrosion of Fe-Cr-(Mn/Si) alloys in CO2-H2O-SO2 gases10.1016/j.corsci.2016.07.026 ↗
21. Early stage oxidation behavior of Al- and Si-alloyed stainless steels as well as Ni-based alloys in air at elevated temperatures10.1002/maco.201709836 ↗
22. Si-rich phases and their distributions in the oxide scale formed on 304 stainless steel at high temperatures10.1016/j.jnucmat.2018.05.018 ↗
23. Oxidation of an austenitic stainless steel with or without alloyed aluminum in O2+10% H2O environment at 800°C10.1016/j.corsci.2017.03.015 ↗
24. Oxidation behavior of Mn and Mo alloyed Fe-16Ni-(5-8)Cr-3.2Si-1.0Al10.1007/BF00665674 ↗
25. The role of (FeCrSi)2(MoNb)-type laves phase on the formation of Mn-rich protective oxide scale on ferritic stainless steel10.1016/j.corsci.2017.12.026 ↗
26. Improvements in high temperature oxidation resistance by additions of reactive elements or oxide dispersions
27. J. Stringer. The reactive element effect in high-temperature corrosion
28. The formation of aluminum oxide scales on high-temperature alloys10.1007/BF00666913 ↗
29. Progress in understanding the reactive element effect since the whittle and stringer literature review
30. What did we learn on the reactive element effect in chromia scale since Pfeil’s patent?10.1002/maco.201307310 ↗
31. The effects of small additions of yttrium on the high-temperature oxidation resistance of a Si-containing austenitic stainless steel10.1023/A:1023061814413 ↗
32. Influence of cerium addition on high temperature oxidation property of austenitic stainless steel
33. The effect of cerium on the oxidation resistance of Fe-20Cr-1.7C-1Si
34. High temperature oxidation behavior of ferritic stainless steel containing W and Ce10.1016/j.corsci.2018.07.017 ↗
35. Oxidation behavior of cerium and tungsten-containing ferritic stainless steels at 1200°C in air10.1016/j.promfg.2018.07.308 ↗
36. The oxidation of Fe-19.6Cr-15.1Mn stainless steel10.1007/BF00751800 ↗
37. High temperature oxidation performance of the annealed 430 stainless steel after hot rolling
38. Birks · 2006
39. Resolving surface chemical states in XPS analysis of first row transition metals, oxides and hydroxides: Cr, Mn, Fe, Co and Ni10.1016/j.apsusc.2010.10.051 ↗
40. Resolving surface chemical states in XPS analysis of first row transition metals, oxides and hydroxides: Sc, Ti, V, Cu and Zn10.1016/j.apsusc.2010.07.086 ↗
41. XPS characterization of the oxide scale on fully processed non-oriented electrical steel sheet10.1016/j.matchar.2011.03.011 ↗
42. Moulder · 1995
43. Evolution of surface chemistry and morphology of oxide scale formed during initial stage oxidation of modified 9Cr–1Mo steel10.1016/j.corsci.2013.10.026 ↗
44. Thermodynamic and kinetic aspects on the selective surface oxidation of binary, ternary and quaternary model alloys10.1016/j.apsusc.2006.10.031 ↗
45. Effect of alloy composition on the selective oxidation of ternary Fe-Si-Cr and Fe-Mn-Cr model alloys10.1002/sia.2732 ↗
46. Oxidation after breakdown of the chromium-rich scale on stainless steels at high temperature: internal oxidation10.1007/s11085-016-9610-7 ↗
47. Observations of the metal oxide interface for a Fe-Cr alloy10.1016/S0010-938X(68)90159-5 ↗
48. Metal-oxide interface morphology for a range of Fe-Cr alloys10.1016/S0010-938X(70)80071-3 ↗
49. Raman spectroscopy of Fe-Ti-Cr-oxides, case study: martian meteorite EETA7900110.2138/am-2004-5-601 ↗
50. Insight into a high temperature selective oxidation of HP40 alloy under a H2-H2O environment10.1039/C6RA25933B ↗
51. A Raman study of the systems Fe3-xCrxO4 and Fe2-xCrxO310.1016/0022-4596(89)90245-4 ↗
52. Theoretical analysis of the diffusion processes determining the oxidation rate of alloys10.1149/1.2779605 ↗
53. Effect of intergranular precipitation on the internal oxidation behaviour of Cr-Mn-N austenitic stainless steel10.1007/s40195-015-0288-7 ↗
54. Effects of Mn on the mechanical properties and high temperature oxidation of 9Cr2WVTa steel10.1016/j.jnucmat.2017.07.024 ↗
55. Diffusion of chromium, manganese, and iron in MnCr2O4 spinel10.1007/s11669-005-0051-2 ↗
56. Reaktionstypen bei der oxydatoin von legierungen
57. The transition from internal to external oxidation and the formation of interruption bands in silver-indium alloys10.1016/0001-6160(61)90103-1 ↗
58. Determination of diffusion coefficient of oxygen in γ-iron from measurements of internal oxidation in Fe-Al alloys10.1007/BF02643898 ↗
59. Modelling Cr depletion under a growing Cr2O3 layer on austenitic stainless steel: the influence of grain boundary diffusion10.1088/0965-0393/17/3/035009 ↗
60. Diffusion of chroumium in ferritic and austenitic 9-20 wt-% chromium steels10.1179/026708300101507055 ↗
61. Young · 2008
62. The influence of implanted yttrium on the mechanisms of growth of chromia scales10.4028/www.scientific.net/MSF.43.1 ↗
63. Li · 2003
64. Critical evaluation and thermodynamic modeling of the Mn-Cr-O system for the oxidation of SOFC interconnect10.1016/j.ssi.2006.01.012 ↗
65. The oxidation of iron-chromium-manganese alloys at 900ºC10.1007/BF00938460 ↗
66. The high temperature oxidation behaivour of austenitic stainless steel10.1002/maco.19780290603 ↗
67. Determination of diffusion coefficient of oxygen in α-iron from internal oxidation measurements in Fe-Si alloys10.1007/BF00547959 ↗