Oxidation and hot corrosion behavior of NiCrAlYSi+NiAl/cBN abrasive coating
Source abstract
Abstract
Abstract In order to improve the oxidation and hot corrosion resistance of blades tip as well as the sealing performance of gas turbine engine, a NiCrAlYSi + NiAl/cBN abrasive coating was prepared by combining arc ion plating, electroplating and above-pack aluminisation. Oxidation and hot corrosion behavior of the abrasive coating were investigated. Results indicated that the abrasive coating showed lower oxidation and degradation rate at 900 °C. NaCl aggravated the corrosion extent via cyclic chlorination/oxidation reaction, and the cBN/metallic coating interface also played a crucial role as a shortcut of the corrosive media. Besides, the oxidation and hot corrosion mechanisms were discussed.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: High-Temperature Coating Behaviors · Metal and Thin Film Mechanics · Intermetallics and Advanced Alloy Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (42)
Show source-provided references
1. NiCrAl/bentonite thermal spray powder for high temperature abradable seals10.1016/0257-8972(88)90090-4 ↗
2. Friction and wear behaviour and abradability of abradable seal coating10.1016/S0043-1648(99)00093-9 ↗
3. Oxidation behavior of a CoNiCrAlY/h-BN based abradable coating10.1016/j.corsci.2019.02.030 ↗
4. Corrosion mechanism of an Al-BN abradable seal coating system in chloride solution10.1016/j.corsci.2013.11.007 ↗
5. The influence of composition and microstructure on the abradability of aluminum-based abradable coatings10.1007/s11666-017-0526-9 ↗
6. Effect of APS process parameters on high-temperature wear behavior of nickel-graphite abradable seal coatings10.1016/j.surfcoat.2017.05.004 ↗
7. Material needs for turbine sealing at high temperature10.1179/1743284714Y.0000000527 ↗
8. Scrinzi · 2013
9. B.B. Seth, G.P. Wagner, Mixed powder deposition of components for wear, erosion and abrasion resistant applications. U.S. Patent. 6706319 B2.
10. L.E. Brown, D.L. Clingman, M.J. Barber, J.F. Kroemer, K.R. Cross, Method for bonding abrasive blade tips to the tip of a gas turbine blade. U.S. Patent. 5359770.
11. L.E. Brown, T.P. Fuesting, J.J. Beaman, J. Suman Das, Method and apparatus for making components by direct laser processing. U.S. Patent. 6355086 B2.
12. Preparation and oxidation behavior of NiCrAlYSi coating on a cobalt-base superalloy K40S10.1016/j.corsci.2008.01.033 ↗
13. Hot corrosion behaviour of a cobalt-base super-alloy K40S with and without NiCrAlYSi coating10.1016/j.corsci.2011.02.022 ↗
14. Thr oxidation behaviour of NiAl-I. Phase transformations in the alumina scale during oxidation of NiAl and NiAl-Cr alloys10.1016/0010-938X(92)90002-K ↗
15. Enhanced cBN blade tip systems for inproving engine efficiency
16. Oxidation behaviour of Pt modified aluminized NiCrAlYSi coating on a Ni-based single crystal superalloy10.1016/j.corsci.2018.02.007 ↗
17. Cyclic oxidation and rumpling behaviour of single phase b-(Ni,Pt)Al coatings with different thickness of initial Pt plating10.1016/j.corsci.2016.05.011 ↗
18. Effect of the θ-α-Al2O3 transformation on the oxidation behavior of β-NiAl+Zr10.1007/BF00846690 ↗
19. The reaction mechanism and kinetics of α-BN powder in we air at 1273K10.1111/jace.12276 ↗
20. Mechanism of oxidation of β-BN10.1007/BF00797809 ↗
21. The control of the composition and structure of aluminide layers formed by vapour aluminising10.1016/S0257-8972(99)00347-3 ↗
22. High-temperature stability of polycrystalline cubic boron nitride cutting tool materials in air10.1016/j.corsci.2012.07.002 ↗
23. High-temperature corrosion performance of HVAF-sprayed NiCr, NiAl, and NiCrAlY coatings with alkali sulfate/chloride exposed to ambient air10.1016/j.corsci.2019.06.021 ↗
24. Oxidation of NiAl and FeAl10.1016/S0966-9795(99)00037-0 ↗
25. Transient-alumina transformations during the oxidation of magnetron-sputtered CoCrAl nanocrystalline coatings10.1023/A:1026015101783 ↗
26. Stress development in alumina scales formed upon oxidation of (111) NiAl single crystals10.1016/S0010-938X(97)83344-6 ↗
27. Effect of water vapor on the phase transformation of alumina grown on NiAl at 950 °C10.1016/j.corsci.2011.05.029 ↗
28. Growth and microstructure of α-Al2O3 on β-NiAl10.1149/1.2129965 ↗
29. The system Al2O3-B2O310.1038/195069a0 ↗
30. Barin · 1995
31. The alumina scale growth and interdiffusion behaviour of Pt modified AlSiY coating during cyclic oxidation10.1016/j.corsci.2016.11.020 ↗
32. Stresses and microstructural development of thermal barrier coating using AIP/D-gun two-step processing10.1111/j.1551-2916.2007.01496.x ↗
33. NaCl-induced hot corrosion of stainless steels10.1016/0025-5416(87)90404-6 ↗
34. NaCl induced corrosion of Ti-6Al-4V alloy at high temperature10.1016/j.corsci.2016.04.016 ↗
35. Hot corrosion behavior of porous nickel-based alloys containing molybdenum in the presence of NaCl at 750 °C10.1016/j.engfailanal.2017.05.009 ↗
36. Corrosion behavior of pure Cr with a solid NaCl deposit in O2 plus water vapor10.1023/A:1004690518225 ↗
37. Effects of alloying elements on NaCl-induced hot corrosion of Stainless Steels10.1016/0921-5093(89)90757-0 ↗
38. NaCl-induced hot corrosion of Fe-Mn-Al-C alloys10.1016/S0254-0584(01)00515-6 ↗
39. High temperature corrosion behaviour of aluminized-coated and uncoated alloy 718 under cyclic oxidation and corrosion in NaCl vapour at 750 °C10.1007/s11085-018-9865-2 ↗
40. Hot corrosion properties of composite coatings in the presence of NaCl at 700 and 900 °C10.1016/j.corsci.2013.01.004 ↗
41. Preparation and hot corrosion behaviour of Pt modified AlSiY coating on a Ni-based superalloy10.1016/j.corsci.2015.12.007 ↗
42. Chemical reactions involved in the initiation of hot corrosion of B-1900 and NASA-TRW VIA10.1149/1.2123928 ↗