journal article·2021-06

Studies on the degree of sensitization of hyper-duplex stainless steel 2707 at 900℃ using a modified DL-EPR test

Li Sun, Yangting Sun, Chenxi Lv, Yuanyuan Liu, Nianwei Dai, Yiming Jiang, Jin Li, Digby D. Macdonald

Corrosion Science· Volume 185
Publisher page

Abstract

Abstract The effects of thermal aging of hyper-duplex stainless steel (HDSS) 2707 at 900℃ for various aging times up to 26 h on the localized, selective corrosion were investigated by electrochemical methods. The results demonstrate that the optimum test condition is 2 M H2SO4 + 1.25 M HCl + 0 0.001 M KSCN with the scan rate of 1.5 mV·s−1 at 30℃. The degree of sensitization (DOS) of HDSS 2707 initially increases rapidly, because of particle precipitation (σ phase/Cr2N), and then decreases as a result of self-healing by back diffusion of Cr and Mo into the depleted areas, peaking at 10h.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Corrosion Behavior and Inhibition · Concrete Corrosion and Durability

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (50)

Show source-provided references
1. The applicability of duplex stainless steels in sour environments10.5006/1.3585312 ↗
2. The effect of phase compositions on the pitting corrosion of 25 Cr duplex stainless steel in chloride solutions10.1016/0010-938X(96)00022-4 ↗
3. X-ray tomographic characterisation of pitting corrosion in lean duplex stainless steel10.1016/j.corsci.2019.108406 ↗
4. Investigation of selective corrosion resistance of aged lean duplex stainless steel 2101 by non-destructive electrochemical techniques10.1016/j.electacta.2009.05.039 ↗
5. Phase transformation and mechanical behavior in annealed 2205 duplex stainless steel welds10.1016/j.matchar.2007.03.004 ↗
6. Effect of annealing temperature on pitting behavior and microstructure evolution of hyper‐duplex stainless steel 270710.1002/maco.201910801 ↗
7. Application of the modified electrochemical potentiodynamic reactivation method to detect susceptibility to intergranular corrosion of a newly developed lean duplex stainless steel LDX210110.1016/j.corsci.2009.11.020 ↗
8. Influence of isothermal phase transformations on toughness and pitting corrosion of super duplex stainless steel SAF 250710.1179/mst.1993.9.7.545 ↗
9. The low-temperature aging embrittlement in a 2205 duplex stainless steel10.1016/j.msea.2003.12.051 ↗
10. Influence of the microstructure on the toughness of a duplex stainless steel UNS S3180310.1007/s10853-005-5700-7 ↗
11. The effect of large heat input on the microstructure and corrosion behaviour of simulated heat affected zone in 2205 duplex stainless steel10.1016/j.corsci.2011.07.022 ↗
12. The effect of phase transformation route on the intergranular corrosion susceptibility of 2205 duplex stainless steel10.1016/j.matlet.2018.11.143 ↗
13. Fast testing of ambient temperature pitting corrosion in type 2205 duplex stainless steel by bipolar electrochemistry experiments10.1016/j.elecom.2020.106779 ↗
14. Bead by bead study of a multipass shielded metal arc-welded super-duplex stainless steel10.1007/s40194-019-00829-7 ↗
15. Element partitioning and electron backscatter diffraction analysis from feeding wire to as-deposited microstructure of wire and arc additive manufacturing with super duplex stainless steel10.1016/j.msea.2019.138856 ↗
16. Double loop electrochemical potentiokinetic reactivation test optimization in checking of duplex stainless steel intergranular corrosion susceptibility10.1007/s11661-004-0187-4 ↗
17. Effect of welding processes and conditions on the microstructure, mechanical properties and corrosion resistance of duplex stainless steel weldments—A review10.1016/j.jmapro.2016.11.003 ↗
18. Wen · 2001
19. Microstructures and element distributions in an aged hyper duplex stainless steel and corresponding hardness variation
20. Influence of sigma phase on corrosion and mechanical properties of 2707 hyper-duplex stainless steel aged for short periods10.1007/s42243-018-0175-3 ↗
21. Effect of Ce addition on the precipitation of deleterious phases and the associated intergranular corrosion resistance of 27Cr–7Ni hyper duplex stainless steels10.1016/j.corsci.2014.10.018 ↗
22. Effects of Cu on the precipitation of intermetallic compounds and the intergranular corrosion of hyper duplex stainless steels10.1016/j.corsci.2012.09.023 ↗
23. Investigation of the sensitization and intergranular corrosion of tube-to-tubesheet welds of hyper duplex stainless steel using an electrochemical reactivation method10.1016/j.corsci.2014.06.005 ↗
24. Effects of inclusions on the precipitation of chi phases and intergranular corrosion resistance of hyper duplex stainless steel10.1016/j.corsci.2014.06.019 ↗
25. Haynes · 1985
26. Corrosion tests and standards: application and interpretation
27. Etching method for determining susceptibility to intergranular attack in ferritic stainless steels10.5006/1.3581933 ↗
28. An electrochemical test for detecting the intergranular corrosion susceptibility of a duplex stainless steel10.5006/1.3583064 ↗
29. The electrochemical reactivation test (ERT) to detect the susceptibility to intergranular corrosion10.1016/S0010-938X(03)00062-3 ↗
30. On the development of the electrochemical potentiokinetic method10.1016/S0013-4686(01)00674-0 ↗
31. Electrochemical potentiodynamic reactivation: development and applications of the EPR test, in: key eng
32. Evaluation of IGSCC susceptibility of austenitic stainless steels using electrochemical reactivation method10.3323/jcorr1974.29.4_163 ↗
33. Trends in the electrochemical polarization potentiodynamic reactivation method–EPR
34. Use of EPR test to study the degree of sensitization in resistance spot welding joints of AISI 304 austenitic stainless steel10.1016/j.corsci.2011.01.036 ↗
35. Corrosion assessment of ASME qualified welding procedures for grade 2101 lean duplex stainless steel10.5006/3257 ↗
36. Evaluation of intergranular corrosion susceptibility of UNS S31803 duplex stainless steel with an optimized double loop electrochemical potentiokinetic reactivation method10.1016/j.electacta.2010.03.086 ↗
37. Studies on the degree of sensitization of welded 2507 super duplex stainless steel using a modified DL-EPR test procedure
38. Application of double loop electrochemical potentiodynamic reactivation test to austenitic and duplex stainless steels10.1016/S0921-5093(97)00008-7 ↗
39. Evaluation of aged duplex stainless steel UNS S32750 susceptibility to intergranular corrosion by optimized double loop electrochemical potentiokinetic reactivation method10.1016/j.corsci.2012.11.024 ↗
40. Correlation between critical pitting temperature and degree of sensitisation on alloy 2205 duplex stainless steel10.1016/j.corsci.2010.10.009 ↗
41. Evaluation of selective corrosion in UNS S31803 duplex stainless steel with electrochemical impedance spectroscopy10.1016/j.electacta.2005.02.105 ↗
42. ASTM A923-14 · 2014
43. Influence of Ti, C and N concentration on the intergranular corrosion behaviour of AISI 316Ti and 321 stainless steels10.1016/j.actamat.2006.11.021 ↗
44. Resistance to sensitization and intergranular corrosion through extreme randomization of grain boundaries10.1016/S1359-6454(02)00306-3 ↗
45. Investigation on ultra-pure ferritic stainless steel 436L susceptibility to intergranular corrosion using optimised double loop electrochemical potentiokinetic reactivation method10.1080/1478422X.2018.1512222 ↗
46. Intergranular corrosion of Low Cr ferritic stainless steel 429 evaluated by the optimized double loop electrochemical potentiokinetic reactivation test10.1155/2015/249348 ↗
47. Precipitation behavior and phase transformation of hyper duplex stainless steel UNS S32707 at nose temperature10.1016/j.matchar.2017.04.018 ↗
48. Influence of the grain size on deleterious phase precipitation in superduplex stainless steel UNS S3275010.1016/j.matchar.2008.08.007 ↗
49. Effect of laser surface melting on intergranular corrosion behaviour of aged austenitic and duplex stainless steels10.1016/j.corsci.2011.01.048 ↗
50. Evaluation of the intergranular corrosion susceptibility of UNS S31803 duplex stainless steel with thermoelectric power measurements10.1016/j.corsci.2012.12.008 ↗