Investigation on the oxidation and ablation behaviors of HfB2-SiC-Si/SiC-Si coatings for carbon/carbon composites
Source abstract
Abstract
Abstract Oxidation and ablation behaviors of HfB2-SiC-Si/SiC-Si coatings fabricated by dipping-carbonization joint gaseous silicon infiltration on cubic and nose-shaped carbon/carbon substrates were investigated. After 30 thermal cycles between 1500 °C and room temperature, the mass gain of the coated sample was 0.91 %, and the mass gain was 2.62 % after oxidation at 1500 °C for 870 h. The coated nose-shaped sample exhibited good anti-ablation properties at 1800 °C–2000 °C under oxyacetylene flame. Especially at 1800 °C, the mass ablation rate was −0.073 mg/s. Although the nose tip suffered the most serious corrosion, HfO2 scale surrounded by Hf-Si-O glass could withstand the oxyacetylene torch scouring.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · Diamond and Carbon-based Materials Research
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (41)
Show source-provided references
1. Fitzer · 1998
2. A novel design of oxidation protective β-Y2Si2O7 nanowire toughened Y2SiO5/Y2O3-Al2O3-SiO2 glass ceramic coating for SiC coated carbon/carbon composites10.1016/j.corsci.2018.02.054 ↗
3. Computational modeling of carbon/carbon composites under thermal shock conditions10.1016/j.compstruct.2016.02.017 ↗
4. Oxidation microstructure studies of reinforced carbon/carbon10.1016/j.carbon.2005.11.013 ↗
5. Effect of yttrium carbide on ablation behavior of zirconium carbide modified carbon/carbon composites10.1016/j.corsci.2020.108675 ↗
6. Oxidation and ablation of 3D carbon-carbon composite at up to 3000 °C10.1016/0008-6223(94)00172-V ↗
7. Fabrication and characteristics of a HfC/TiC multilayer coating by a vacuum plasma spray process to protect C/C composites against oxidation10.1016/j.corsci.2020.109068 ↗
8. Effect of the incorporation of SiC nanowire on mullite/SiC protective coating for carbon/carbon composites10.1016/j.corsci.2016.02.022 ↗
9. The novel effect mechanism of Al2O3 nano-powder in the pack cementation process to prepare SiC coating on C/C composites10.1016/j.jeurceramsoc.2020.10.014 ↗
10. SiC-Si coating with micro-pores to protect carbon/carbon composites against oxidation10.1016/j.jeurceramsoc.2020.08.045 ↗
11. Long-term oxidation behaviors of C/SiC composites with a SiC/UHTC/SiC three-layer coating in a wide temperature range10.1016/j.corsci.2015.02.026 ↗
12. Effect of the ZrB2 content on the oxygen blocking ability of ZrB2-SiC coating at 1973 K10.1016/j.jeurceramsoc.2020.10.036 ↗
13. SiCnw/PyC core-shell networks to improve the bonding strength and oxyacetylene ablation resistance of ZrB2-ZrC coating for C/C-ZrB2-ZrC-SiC composites10.1016/j.carbon.2017.09.019 ↗
14. Dynamic oxidation protective ultrahigh temperature ceramic TaB2-20 wt% SiC composite coating for carbon material10.1016/j.compositesb.2018.10.080 ↗
15. Ablation behavior of sharp leading edge parts made of rare earth La compound modified ZrB2 coated C/C composites10.1016/j.corsci.2020.108895 ↗
16. High-temperature erosion resistance and aerodynamic oxidation mechanism of multi-layer MoSi2-CrSi2-Si/SiC coated carbon/carbon composites in a wind tunnel at 1873 K10.1016/j.carbon.2012.01.027 ↗
17. TaxHf1-xB2-SiC multiphase oxidation protective coating for SiC-coated carbon/carbon composites10.1016/j.corsci.2014.07.016 ↗
18. An inlaid interface of carbon/carbon composites to enhance the thermal shock resistance of SiC coating in combustion environment10.1016/j.surfcoat.2016.03.068 ↗
19. Oxidation and ablation protection of multiphase Hf0.5Ta0.5B2-SiC-Si coating for graphite prepared by dipping-pyrolysis and reactive infiltration of gaseous silicon10.1016/j.apsusc.2018.08.042 ↗
20. A CrSi2-HfB2-SiC coating providing oxidation and ablation protection over 1973 K for SiC coated C/C composites10.1016/j.corsci.2020.108536 ↗
21. Oxidation resistance of HfB2-SiC composites for protection of carbon-based materials10.1016/j.actaastro.2006.11.007 ↗
22. Review on ultra-high temperature boride ceramics10.1016/j.pmatsci.2020.100651 ↗
23. Ultra-high temperature HfB2-SiC ceramics consolidated by hotpressing and spark plasma sintering10.1016/j.jallcom.2006.01.107 ↗
24. Inherent anisotropy in transition metal diborides and microstructure/property tailoring in ultra-high temperature ceramics-A review10.1016/j.jeurceramsoc.2017.09.012 ↗
25. Oxidation resistance of HfB2-SiC coatings for protection of carbon Fiber Based composites10.4028/www.scientific.net/KEM.264-268.1047 ↗
26. Ultra-high-temperature ceramic HfB2-SiC coating for oxidation protection of SiC-coated carbon/carbon composites10.1111/ijac.12241 ↗
27. The effect of HfB2 content on the oxidation and thermal shock resistance of SiC coating10.1016/j.surfcoat.2018.02.029 ↗
28. Oxidation protection and mechanism of the HfB2-SiC-Si/SiC coatingsmodified by in-situ strengthening of SiC whiskers for C/C composite10.1016/j.ceramint.2018.04.025 ↗
29. The oxidation resistance of two-temperature synthetic HfB2-SiC coating for the SiC coated C/C composites10.1016/j.jallcom.2018.03.043 ↗
30. Dynamic oxidation protective behaviors and mechanisms of HfB2-20 wt%SiC composite coating for carbon materials10.1016/j.jeurceramsoc.2019.01.033 ↗
31. Oxidation protective SiC-Si coating for carbon/carbon composites by gaseous silicon infiltration and pack cementation: a comparative investigation10.1016/j.jeurceramsoc.2020.07.040 ↗
32. A dense ZrB2-SiC-Si/SiC-Si coating to protect carbon/carbon composites against oxidation at 1773 K and 1973 K10.1016/j.corsci.2021.109331 ↗
33. Ablation resistance of HfB2-SiC coating prepared by in-situ reaction method for SiC coated C/C composites10.1016/j.ceramint.2017.06.052 ↗
34. Oxidation and ablation protection of double layer HfB2-SiC-Si/SiC-Si coating for graphite materials10.1016/j.jallcom.2018.12.256 ↗
35. Oxidation protective ZrB2-MoSi2-SiC-Si coating for graphite materials prepared by slurry dipping and vapor silicon infiltration10.1016/j.surfcoat.2018.02.027 ↗
36. Chase · 1998
37. Börnstein · 1999
38. The resistance to oxidation of an HfB2-SiC composite10.1016/j.jeurceramsoc.2004.05.009 ↗
39. Determination of the active-to-passive transition in the oxidation of silicon carbide in standard and microwave-excited air10.1016/0955-2219(95)00104-2 ↗
40. Ablation behavior of nose-shaped HfB2-SiC modified carbon/carbon composites exposed to oxyacetylene torch10.1016/j.corsci.2019.02.015 ↗
41. Ablation behavior of ZrB2-SiC ultra hig temperature ceramics under simulated atmospheric re-entry conditions10.1016/j.compscitech.2008.02.009 ↗