Influences of alloyed Si on the corrosion resistance of Co–Cr–Mo alloy to molten Al by iso-thermal oxidation in air
Source abstract
Abstract
The corrosion resistance of Co–Cr–Mo alloys with various Si concentrations after oxidation to molten Al was investigated. Si was helpful in forming a more homogeneous, compact Cr2O3 film after oxidation. Correspondingly, the Cr2O3-dominant film was more effective in enhancing the corrosion resistance than the duplex film of CoO and Cr2O3 of alloy with low Si concentration. In addition, local defects such as the cracks acted as initiation sites of failure in oxide film. Ascribed to its higher stability, Si-rich layer beneath the oxide film delayed the reaction between Al and matrix even after the failure of oxide film.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: High-Temperature Coating Behaviors · Nuclear Materials and Properties · Advanced materials and composites
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (24)
Show source-provided references
1. Interfacial reactions of solid Co and solid Fe with liquid Al10.1016/j.corsci.2012.04.015 ↗
2. Characterisation of oxide films formed on Co–29Cr–6Mo alloy used in die-casting moulds for aluminium10.1016/j.corsci.2013.03.026 ↗
3. Interfacial reactions between molten Al and a Co-Cr-Mo alloy with and without oxidation treatment10.1016/j.corsci.2011.08.015 ↗
4. Experimental and theoretical research on interfacial reaction of solid Co with liquid Al10.1016/j.corsci.2013.03.024 ↗
5. Effects of Al, Ti, and Zr doping on oxide film formation in Co-29Cr-6Mo alloy used as mould material for Al die-casting10.1016/j.corsci.2014.03.020 ↗
6. Effects of sigma phase and carbide on the wear behavior of CoCrMo alloys in Hanks’ solution10.1016/j.wear.2013.12.010 ↗
7. Effect of nitriding treatment on corrosion behaviour of Co–Cr–Mo alloy in liquid Al10.1016/j.corsci.2013.10.004 ↗
8. Inconel 617 and Stellite 6 alloys for tooling in thixoforming of steels10.1016/S1003-6326(09)60354-X ↗
9. Thermal fatigue testing of Inconel 617 and Stellite 6 alloys as potential tooling materials for thixoforming of steels10.1016/j.msea.2009.11.021 ↗
10. Thermal fatigue testing of Stellite 6-coated hot work tool steel10.1016/j.msea.2010.06.015 ↗
11. A novel C-free Co-based alloy for high temperature tooling applications10.1016/j.msea.2010.10.037 ↗
12. Research on the microstructure, fatigue and corrosion behavior of permanent mold and die cast aluminum alloy10.1016/j.matdes.2013.10.012 ↗
13. Study on stainless steel electrode based on dynamic aluminum liquid corrosion mechanism10.1016/S1001-0742(09)60066-8 ↗
14. Interfacial reaction between Co-Cr-Mo alloy and liquid Al10.1016/j.corsci.2013.06.009 ↗
15. Enhancement of corrosion resistance of Fe-Cr-Mo alloy to molten Al by thermal oxidation in air10.1016/j.corsci.2013.07.031 ↗
16. Effects of alloyed Si on the oxidation behaviour of Co–29Cr–6Mo alloy for solid-oxide fuel cell interconnects10.1016/j.corsci.2015.02.036 ↗
17. Surface characterisation of Ni-free Co-Cr-W-based dental alloys exposed to high temperatures and the effects of adding silicon10.1016/j.corsci.2015.02.030 ↗
18. Thermo-Calc Software, Ni-based Alloy Database, TCW 5.0. .
19. The effect of alloyed nickel on the short-term high temperature oxidation behaviour of Co–Re–Cr-based alloys10.1016/j.corsci.2015.01.004 ↗
20. The oxidation of alloys10.1088/0034-4885/39/5/001 ↗
21. Effects of liquid aluminium on hot-work tool steel10.1016/0301-679X(93)90021-R ↗
22. JANAF thermochemical tables, 1974 supplement10.1063/1.3253143 ↗
23. NIST-JANAF themochemical tables, fourth edition
24. The role of silicon in the reactive-elements effect on the oxidation of conventional austenitic stainless steel10.1007/s11085-006-9046-6 ↗