Ablation behavior of Y2SiO5/SiC coating for C/C composites under oxyacetylene torch
Source abstract
Abstract
Abstract The ablation behavior of a Y 2 SiO 5 /SiC coating was investigated under oxyacetylene torch with two different heat fluxes. Applying the Y 2 SiO 5 /SiC coating, the ablation resistant property of C/C composites was improved obviously with heat flux of 2.38 MW/m 2 , and the linear and mass ablation rates were reduced by 56% and 90% after ablation for 60 s, respectively. The good ablation resistance is attributed to the glassy protective layer of SiO 2 and Y 2 O 3 that reduces heat transfer and oxidizing species transport. As heat flux increased to 4.18 MW/m 2 , increase of mechanical denuding and chemical erosion resulted in the degradation of the ablation resistance.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · Diamond and Carbon-based Materials Research
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (22)
Show source-provided references
1. Carbon–carbon composites10.1146/annurev.ms.24.080194.000315 ↗
2. Oxidation behavior of oxidation protective coatings for C/C-SiC Composites at 1500°C10.1016/S1003-6326(08)60229-0 ↗
3. Oxidation microstructure studies of reinforced carbon/carbon10.1016/j.carbon.2005.11.013 ↗
4. SiC/SiC–YAG–YSZ oxidation protective coatings for carbon/carbon composites10.1016/j.corsci.2013.01.013 ↗
5. Microstructure and oxidation of multi-layer MoSi2–CrSi2–Si coatings for SiC coated carbon/carbon composites10.1016/j.corsci.2010.05.020 ↗
6. Preparation and oxidation protection of CVD SiC/a-BC/SiC coatings for 3D C/SiC composites10.1016/j.corsci.2009.01.026 ↗
7. Oxidation protection coatings for C/SiC based on yttrium silicate10.1016/S0955-2219(98)00241-6 ↗
8. Yttrium silicate coatings for oxidation protection of carbon–silicon carbide composites10.1111/j.1151-2916.2000.tb01392.x ↗
9. Yttrium silicate coating system for oxidation protection of C/C–Si–SiC composites: electrophoretic deposition and oxygen self-diffusion measurements10.1016/j.jeurceramsoc.2006.05.026 ↗
10. Celsian/yttrium silicate protective coating prepared by microwave sintering for C/SiC composites against oxidation10.1016/j.msea.2008.11.008 ↗
11. Microstructures, mechanical properties and tribological behaviors of Cr–Al–N, Cr–Si–N, and Cr–Al–Si–N coatings by a hybrid coating system10.1016/j.surfcoat.2006.07.118 ↗
12. Porosity, mechanical properties, residual stresses of supersonic plasma-sprayed Ni-based alloy coatings prepared at different powder feed rates10.1016/j.apsusc.2007.12.023 ↗
13. Improved ablation resistance of C–C composites using zirconium diboride and boron carbide10.1016/j.jeurceramsoc.2010.02.025 ↗
14. A SiC/glass oxidation protective coating for carbon/carbon composites for application at 1173K10.1016/j.carbon.2006.12.014 ↗
15. Phase equilibria and thermodynamics in the Y2O3–Al2O3–SiO2 system
16. Comparison of thermal and ablation behaviour of C/SiC composites and C/ZrB2–SiC composites10.1016/j.corsci.2008.09.037 ↗
17. Amorphous silica nanowires grown by the vapor-solid mechanism10.1016/S0009-2614(03)01019-4 ↗
18. Effect of heat flux on ablation behaviour and mechanism of C/C–ZrB2–SiC composite under oxyacetylene torch flame10.1016/j.corsci.2013.04.052 ↗
19. Effect of oxidation on elastic modulus of C/C–SiC composites10.1016/j.msea.2007.09.078 ↗
20. The effect of zirconium carbide on ablation of carbon/carbon composites under an oxyacetylene flame10.1016/j.corsci.2010.09.028 ↗
21. Ablation in different heat fluxes of C/C composites modified by ZrB2–ZrC and ZrB2–ZrC–SiC particles10.1016/j.corsci.2013.04.038 ↗
22. On the oxidation behaviour of MoSi210.1016/S0966-9795(00)00114-X ↗