Abstract The present work applied tensile testing to investigate the adhesion of thermal oxide scales to as-received hot-rolled carbon steels containing 0.04–0.18 wt.% C and to steels oxidised in the atmosphere relevant to the hot-rolling process which contained water vapour. Higher carbon content in the steel deteriorated the adhesion of scale formed during hot rolling which was related to the higher amount of carbon existed at scale-steel interface. For the steel with 0.14 wt.% C, increasing the coiling temperature could increase the carbon solubility in the matrix, thus reducing the interfacial carbon and improving the scale adhesion.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: High-Temperature Coating Behaviors · Metallurgical Processes and Thermodynamics · Metal Alloys Wear and Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (52)

Show source-provided references
1. Oxide scales on hot-rolled steel strips
2. Relationship between entry temperature and properties of thermal oxide scale on low carbon steel strips
3. Effects of process parameters on mechanical adhesion of thermal oxide scales on hot-rolled low carbon steels10.1007/s11085-013-9370-6 ↗
4. Bhadeshia · 2006
5. Oxidation of Fe–C alloys in the temperature range 600–850°C10.1007/BF00611348 ↗
6. Morphology of oxide scale and oxidation kinetics of low carbon steel10.1016/S1006-706X(14)60051-0 ↗
7. Oxide scale growth on high carbon steel at high temperatures10.1016/S1006-706X(13)60043-6 ↗
8. The oxidation and decarburizing of Fe–C alloys in air and the influence of relative humidity10.1007/BF00613495 ↗
9. Role of hematite formation on blister generation during high temperature oxidation of steel10.2355/isijinternational.52.2254 ↗
10. Effect of Si content and temperature on oxidation resistance of Fe–Si alloys10.1016/S1006-706X(15)60036-X ↗
11. Improved oxide scale adherence of low-Pt/Hf co-doped β-NiAlCrSi coating on superalloy IC21 at 1200°C10.1016/j.corsci.2016.01.005 ↗
12. Time and temperature dependence of the adhesion of oxide scales formed on phosphorus-containing steels during short term oxidation10.1016/j.matchemphys.2014.09.038 ↗
13. Quantification of growth kinetics and adherence of oxide scales formed on Ni-based superalloys at high temperature10.1016/j.corsci.2010.08.013 ↗
14. Adhesion of thermal oxide scales grown on ferritic stainless steels measured using the inverted blister test10.1016/S0921-5093(03)00355-1 ↗
15. Investigations for the validation of the defect based scale failure diagram − part I: nickel oxide10.1007/s11085-012-9317-3 ↗
16. Determination of mechanical adhesion energy of thermal oxide scales on AISI 430Ti alloy using tensile test10.1179/174328407X168964 ↗
17. Application of the micro-tensile testing to investigate the adhesion of thermal oxide scales grown on AISI 441 stainless steel sheet oxidised in air and water vapour10.4028/www.scientific.net/KEM.410-411.187 ↗
18. Comparison of damaging behaviour of oxide scales grown on austenitic stainless steels using tensile test and cyclic thermogravimetry10.1016/j.corsci.2015.11.012 ↗
19. Krzyzanowski · 2010
20. Descaling ability of low-alloy steel wires depending on composition and rolling process10.1016/j.corsci.2009.12.028 ↗
21. Adhesion of thermal oxide scales on hot-rolled conventional and recycled steels10.1007/s11085-012-9356-9 ↗
22. Quantification of adherence of thermal oxide scale on low carbon steel using tensile test10.1007/s11085-015-9583-y ↗
23. Effect of silicon on formation and mechanical adhesion of thermal oxide scale grown on low carbon steels in a hot-rolling line
24. Effects of the presence of water vapour on the oxidation behaviour of low carbon-low silicon steel in 1%O2–N2 at 1073K10.1007/s11085-012-9314-6 ↗
25. Kubaschewski · 1965
26. Review of the high-temperature oxidation of iron and carbon steels in air or oxygen10.1023/A:1023685905159 ↗
27. Einfluss von wasserdampf und kohlendioxyd auf die oxydation von eisen in sauerstoff bei hohen temperaturen10.1016/S0010-938X(65)90500-7 ↗
28. The oxidation of iron at 950°C in oxygen/water vapour mixtures10.1016/S0010-938X(69)80056-9 ↗
29. The influence of scale/metal interface characteristics on the oxidation behaviour of iron at elevated temperatures10.1016/0010-938X(79)90004-0 ↗
30. Oxidation of iron at 400–600°C in dry and wet O210.1016/j.corsci.2010.01.002 ↗
31. Young · 2008
32. Comparison between the oxidation of iron in oxygen and in steam at 650–750°C10.1016/j.corsci.2013.06.014 ↗
33. Oxidation of simulated recycled steels with 0.23 and 1.03wt.% Si in Ar-20%H2O at 900°C10.1016/j.corsci.2014.06.018 ↗
34. Effect of a grain-refined microalloyed steel substrate on the formation mechanism of a tight oxide scale10.1016/j.corsci.2014.04.006 ↗
35. Oxide-scale structure formed on commercial hot-rolled steel strip and their formation mechanisms10.1023/A:1010395419981 ↗
36. Birks · 2006
37. Equilibrium of iron-carbon alloys with mixtures of CO–CO2 and CH4–H210.1021/ja01211a010 ↗
38. Gaskell · 1981
39. Darken · 1953
40. Comparative oxidation behaviour of Fe–9Cr steel in CO2 and H2O at 550°C: detailed analysis of the inner oxide layer10.1016/j.corsci.2015.07.032 ↗
41. Corrosion of 9–12Cr ferritic-martensitic steels in high-temperature CO210.1016/j.corsci.2016.01.009 ↗
42. Oxidation of Fe–C alloys at 700°C10.1007/BF00603670 ↗
43. UV and VIS Raman spectra of natural lonsdaleites: towards a recognised standard10.1016/j.saa.2008.10.025 ↗
44. Lonsdaleite − a material stronger and stiffer than diamond10.1016/j.scriptamat.2011.04.013 ↗
45. Stress effects in high temperature oxidation of metals10.1179/imr.1995.40.1.1 ↗
46. Characteristics of scale/substrate interface area of Si-containing low-carbon steels at high temperatures10.1016/S0921-5093(00)01977-8 ↗
47. Effect of yttrium on the oxide scale adherence of pre-oxidized silicon-containing heat-resistant alloy10.1016/j.corsci.2011.07.002 ↗
48. Effects of silicon on the oxidation behavior of Ni-base chromia-forming alloys10.1007/s11085-006-9003-4 ↗
49. Stress and adhesion of chromia-rich scales on ferritic stainless steels in relation with spallation10.1590/S1516-14392004000100012 ↗
50. Adhesion of oxide scales grown on ferritic stainless steels in solid oxide fuel cells temperature and atmosphere conditions10.1016/j.jpowsour.2007.06.058 ↗
51. Effect of Dy on the adherence of Al2O3/NiAl interface: a combined first-principles and experimental studies10.1016/j.corsci.2012.09.002 ↗
52. Predicting oxide spallation from sulphur-contaminated oxide/metal interfaces10.1007/s11085-012-9322-6 ↗