Abstract

Abstract The high temperature oxidation behavior of three SiBCN monoliths: carbon-lean SiBCN with substantial Si metal, carbon-moderate SiBCN and carbon-rich SiBCN with excessive carbon, was investigated at 1500 °C for times up to15 h. Scale growth for carbon-lean and −moderate monoliths at 1500 °C cannot be described by a linear or parabolic rate law, while the carbon-rich monoliths oxidize according to a approximately linear weight loss equation. The microstructures of the oxide scale compose of three distinct layers. The passivating layer of carbon and boron containing amorphous SiO 2 and increased oxidation resistance of BN(C) both benefit the oxidation resistance.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Semiconductor materials and devices · MXene and MAX Phase Materials

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (62)

Show source-provided references
1. Material property requirements for analysis and design of UHTC components in hypersonic applications10.1016/j.jeurceramsoc.2010.01.026 ↗
2. The hypersonic environment: required operating conditions and design challenges10.1023/B:JMSC.0000041688.68135.8b ↗
3. Synthesis, processing and properties of TaC-TaB2-C ceramics10.1016/j.jeurceramsoc.2010.01.032 ↗
4. Ablation mechanism of SiC coated C/C composites at 0° angle in two flame conditions under an oxyacetylene flame10.1016/j.corsci.2014.03.009 ↗
5. Oxidation behaviour of SiC-a review
6. Oxidation behavior of silicon carbide10.1111/j.1151-2916.1958.tb12932.x ↗
7. Improvements in mechanical properties in SiC by the addition of TiC particles10.1111/j.1151-2916.1984.tb19174.x ↗
8. High temperature properties of Si3N4 materials10.1016/0955-2219(91)90109-D ↗
9. A silicoboron carbonitride ceramic stable to 2,000 °C10.1038/382796a0 ↗
10. Amorphous silicoboron carbonitride monoliths resistant to flowing air up to 1800 C°10.1016/j.corsci.2016.03.026 ↗
11. Oxidation behavior of a fully dense polymer-derived amorphous silicon carbonitride ceramic10.1111/j.1551-2916.2004.00483.x ↗
12. Surface studies of potentially oxidation protective Si-BNC films for carbon fibers10.1021/cm960365b ↗
13. Si-B-(N,C) a new ceramic material for high performance applications
14. Characterization of oxidized polymer-derived SiBCN fibers10.1111/j.1151-2916.2001.tb00987.x ↗
15. Precursor-derived Si-B-C-N ceramics: oxidation kinetics10.1111/j.1151-2916.2001.tb00985.x ↗
16. Ceramic fibers for matrix composites in high-temperature applications10.1126/science.285.5428.699 ↗
17. Microstructural features and properties of the nano-crystalline SiC/BN(C) composite ceramic prepared from the mechanically alloyed SiBCN powder10.1016/j.jallcom.2012.05.073 ↗
18. Effect of Si/C ratio and their content on the microstructure and properties of Si-B-C-N ceramics prepared by spark plasma sintering techniques10.1016/j.msea.2010.11.032 ↗
19. Ablation behavior of graphene reinforced SiBCN ceramics in an oxyacetylene combustion flame10.1016/j.corsci.2015.07.006 ↗
20. Microstructure, oxidation and thermal shock resistance of graphene reinforced SiBCN ceramics10.1016/j.ceramint.2015.11.127 ↗
21. Enhancement of photoluminescence in SiCxNy nanoparticle films by addition of a Ni buffer layer10.1016/j.jnoncrysol.2006.09.010 ↗
22. Highly dense amorphous Si2BC3N monoliths with excellent mechanical Properties prepared by high pressure sintering10.1111/jace.13802 ↗
23. Perspectives on carbon nanotubes and graphene Raman spectroscopy10.1021/nl904286r ↗
24. Processing route Dramatically influencing the nanostructure of carbon-rich SiCN and SiBCN polymer-derived ceramics, part I: low temperature thermal transformation10.1016/j.jeurceramsoc.2011.09.012 ↗
25. Carbon-rich SiCN ceramics derived from phenyl-containing poly(silylcarbodiimides)10.1016/j.jeurceramsoc.2009.03.026 ↗
26. Effect of precursor on speciation and nanostructure of SiBCN polymer-derived ceramics10.1111/jace.12192 ↗
27. Correlation between X-ray diffraction and Raman spectra of 16 commercial graphene?based materials and their resulting classification10.1016/j.carbon.2016.10.010 ↗
28. Diamond/carbon nanotube composites: raman, FTIR and XPS spectroscopic studies10.1016/j.carbon.2016.09.064 ↗
29. Ablation mechanism and properties of SiCf/SiBCN ceramic composites under an oxyacetylene torch environment10.1016/j.corsci.2014.01.006 ↗
30. Si/B/C/N/Al precursor-derived ceramics: synthesis, high temperature behavior and oxidation resistance10.1016/j.jeurceramsoc.2003.10.018 ↗
31. Oxidation behavior of SiC-SiBCN ceramics10.1016/j.ceramint.2014.09.025 ↗
32. Oxidation behavior of amorphous Si-(B)-C-N ceramic in ambient air10.1007/s12598-011-0346-z ↗
33. Preparation and anti-oxidation characteristics of ZrSiO4-SiBCN(O) amorphous coating10.1016/j.apsusc.2015.01.119 ↗
34. Passivity during the oxidation of silicon at elevated temperatures10.1063/1.1723429 ↗
35. Oxidation transition for SiC part I. active-to-passive transitions10.1111/jace.12108 ↗
36. Oxidation transitions for SiC part II. Passive to-active transitions10.1111/jace.12104 ↗
37. Oxidation behavior of SiC/SiC ceramic matrix composites in air10.1016/j.jeurceramsoc.2016.05.051 ↗
38. Active oxidation of SiC10.1007/s11085-010-9216-4 ↗
39. Mechanism of ablation of 3D C/ZrC-SiC composite under an oxyacetylene flame10.1016/j.corsci.2012.11.009 ↗
40. Effect of reaction melt infiltration temperature on the ablation properties of 2D C/C-SiC-ZrC composites10.1016/j.corsci.2012.01.001 ↗
41. Effect of surface ablation products on the ablation resistance of C/C-SiC composites under oxyacetylene torch10.1016/j.corsci.2012.10.003 ↗
42. Comparison of morphology and microstructure of ablation centre of C/SiC composites by oxy-acetylene torch at 2900 and 3550 °C10.1016/j.corsci.2008.07.019 ↗
43. Ablation behavior of rare earth La-modified ZrC coating for SiC-coated carbon/carbon composites under an oxyacetylene torch10.1016/j.corsci.2015.11.030 ↗
44. Ablation behaviour of C/C and C/C?ZrC?SiC composites with cone-shaped holes under an oxyacetylene flame10.1016/j.corsci.2015.09.022 ↗
45. High-temperature oxidation of boron nitride10.1016/S0272-8842(86)80006-2 ↗
46. High-temperature oxidation of boron nitride: i, monolithic boron nitride10.1111/j.1551-2916.1999.tb20075.x ↗
47. High-temperature oxidation of boron nitride: II boron nitride layer in composites10.1111/j.1151-2916.1999.tb01944.x ↗
48. Corrosion mechanism of an Al?BN abradable seal coating system in chloride solution10.1016/j.corsci.2013.11.007 ↗
49. Corrosion kinetics and corrosion mechanisms of BN-ZrO2-SiC composites in molten steel10.1016/j.corsci.2014.08.009 ↗
50. Investigation of the oxidation pyrolysis of binary metal nitrides, and particularly of boron nitride10.1016/0165-2370(95)00902-Q ↗
51. On the rates of oxidation of silicon and silicon carbide in oxygen, and correction with permeability of silica glass10.3891/acta.chem.scand.18-1596 ↗
52. The high-temperature oxidation reduction, and volatilization reactions of silicon and silicon carbide10.1007/BF00613092 ↗
53. Fibrous monolithic ceramics: III, mechanical properties and oxidation behavior of the silicon carbide/boron nitride system10.1111/j.1151-2916.1994.tb05399.x ↗
54. Sealing role of B2O3 in MoSi2CrSi2-Si/B-modified SiC coating for C/C composites10.1016/j.corsci.2012.04.018 ↗
55. Reactions of silicon carbide and silicon(IV) oxide at elevated temperatures10.1111/j.1151-2916.1992.tb04232.x ↗
56. Oxidation of BN-coated SiC fibers in ceramic matrix composites10.1111/j.1151-2916.1996.tb08163.x ↗
57. Degradation of CVD SiC coated C/SiC composites exposed to the monopropellant combustion products based on Hydroxylammonium nitrate (HAN)10.1016/j.corsci.2013.04.036 ↗
58. C/SiC/MoSi2-Si multilayer coatings for carbon/carbon composites for protection against oxidation10.1016/j.corsci.2011.07.036 ↗
59. Processing, microstructure and ablation behavior of C/SiC-Ti3SiC2 composites fabricated by liquid silicon infiltration10.1016/j.corsci.2013.04.029 ↗
60. Oxidation protection of carbon/carbon composites by a novel SiC10.1016/j.corsci.2014.12.013 ↗
61. Effects of in situ amorphous graphite coating on ablation resistance of SiC fiber reinforced SiBCN ceramics in an oxyacetylene flame10.1016/j.corsci.2016.10.002 ↗
62. Oxidative and hydrolytic stability of boron nitride-a new approach to improving the oxidation resistance of carbonaceous structures10.1016/0008-6223(94)00163-T ↗