Hydrogen-assisted failure of laser melting additive manufactured IN718 superalloy
Source abstract
Abstract
Abstract A nickel-based superalloy IN718 was fabricated by laser melting additive manufacturing process and hydrogen embrittlement (HE) behavior of this alloy was assessed via slow strain rate tensile tests. The results reveal that hydrogen-charged as-deposited samples along vertical plane exhibit the lowest susceptibility to HE, followed by as-deposited samples along horizontal plane and then heat-treated samples. Additionally, hydrogen-assisted cracking of as-deposited samples initiates from γ-matrix/Laves phase interfaces, whereas γ-matrix/δ phase interfaces along grain boundaries act as preferable damage sites for hydrogen charged heat-treated samples. These hydrogen-assisted cracking can be explained by synergistic effect of HELP mechanism and HEDE mechanism.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Additive Manufacturing Materials and Processes · Nuclear Materials and Properties · Hydrogen embrittlement and corrosion behaviors in metals
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (65)
Show source-provided references
1. Metal fabrication by additive manufacturing using laser and electron beam melting technologies10.1016/S1005-0302(12)60016-4 ↗
2. Wang · 2017
3. Additive manufacturing of metals10.1016/j.actamat.2016.07.019 ↗
4. Micro-and meso-structures and their influence on mechanical properties of selectively laser melted Ti-6Al-4V10.1016/j.actamat.2018.05.044 ↗
5. Microstructures and mechanical behavior of Inconel 718 fabricated by selective laser melting10.1016/j.actamat.2011.12.032 ↗
6. Effect of heat treatment on the microstructure and mechanical properties of Inconel 718 processed by selective laser melting10.1016/j.msea.2015.05.035 ↗
7. The microstructure and mechanical properties of deposited-IN718 by selective laser melting10.1016/j.jallcom.2011.10.107 ↗
8. Rationalization of microstructure heterogeneity in Inconel 718 builds made by the direct laser additive manufacturing process10.1007/s11661-014-2370-6 ↗
9. Additive layer manufacturing of titanium matrix composites using the direct metal deposition laser process10.1016/j.msea.2016.09.002 ↗
10. Dendritic microstructure and hot cracking of laser additive manufactured Inconel 718 under improved base cooling10.1016/j.jallcom.2016.01.250 ↗
11. Tensile mechanical properties and fracture behaviors of nickel-based superalloy 718 in the presence of hydrogen10.1016/j.ijhydene.2018.08.179 ↗
12. Corrosion in the oil and gas industry: an increasing challenge for materials10.1007/s11837-013-0675-3 ↗
13. Alloy 718 for oilfield applications10.1007/s11837-012-0238-z ↗
14. Slow strain rate testing for hydrogen embrittlement susceptibility of alloy 718 in Substitute Ocean Water10.1007/s11665-017-2675-x ↗
15. Hydrogen assisted crack initiation and propagation in a nickel-based superalloy10.1016/j.actamat.2016.05.003 ↗
16. Decrease in hydrogen embrittlement sensitivity of INCONEL 718 by laser surface softening10.1016/S0921-5093(96)10384-1 ↗
17. Omiya, Saitama, Japan, SPIEFirst International Symposium on Laser Precision Microfabrication : 14-16 June 20002000
18. Effects of precipitation phases on the hydrogen embrittlement sensitivity of Inconel 71810.1016/S1468-6996(02)00039-6 ↗
19. Study of the effect of δ phase on hydrogen embrittlement of Inconel 718 by notch tensile tests10.1016/j.corsci.2004.06.008 ↗
20. Study of the effect of hydrogen charging on the tensile properties and microstructure of four variant heat treatments of nickel alloy 71810.1016/j.ijhydene.2017.02.149 ↗
21. Hydrogen-assisted failure in Ni-based superalloy 718 studied under in situ hydrogen charging: the role of localized deformation in crack propagation10.1016/j.actamat.2017.02.059 ↗
22. Effect of temperature on hydrogen embrittlement susceptibility of alloy 718 in Light Water Reactor environment10.1016/j.ijhydene.2017.06.211 ↗
23. Hydrogen embrittlement in nickel-based superalloy 718: relationship between g′ þ g 00 precipitation and the fracture mode
24. Hydrogen embrittlement: the game changing factor in the applicability of nickel alloys in oilfield technology
25. An investigation of micro-mechanisms in hydrogen induced cracking in nickel-based superalloy 71810.1016/j.jallcom.2016.01.033 ↗
26. Multi-scale and spatially resolved hydrogen mapping in a Ni–Nb model alloy reveals the role of the δ phase in hydrogen embrittlement of alloy 71810.1016/j.actamat.2016.02.053 ↗
27. Hydrogen-induced intergranular failure in nickel revisited10.1016/j.actamat.2012.01.040 ↗
28. Effect of microstructure and alloy chemistry on hydrogen embrittlement of precipitation-hardened Ni-Based alloys10.1007/s11661-018-4483-9 ↗
29. Effect of hydrogen on the mechanical properties of alloy 945X (UNS N09945) and influence of microstructural features10.1016/j.msea.2016.12.088 ↗
30. Correlation of mechanical properties to microstructure in Metal Laser Sintering Inconel 71810.1016/j.msea.2017.11.125 ↗
31. Anisotropy and heterogeneity of microstructure and mechanical properties in metal additive manufacturing: a critical review10.1016/j.matdes.2017.11.021 ↗
32. Microstructure and mechanical properties of Inconel 718 produced by selective laser melting: sample orientation dependence and effects of post heat treatments10.1016/j.msea.2017.12.043 ↗
33. Effect of standard heat treatment on the microstructure and mechanical properties of selective laser melting manufactured Inconel 718 superalloy10.1016/j.msea.2015.06.021 ↗
34. Microstructure and mechanical properties of Inconel 718 produced by SLM and subsequent heat treatment10.4028/www.scientific.net/KEM.651-653.665 ↗
35. On the microstructural and mechanical properties of post-treated additively manufactured Inconel 718 superalloy under quasi-static and cyclic loading10.1016/j.msea.2016.05.089 ↗
36. Effects of Post-processing on microstructure and mechanical properties of SLM-processed IN-718
37. Microstructure and directional fatigue behavior of Inconel 718 produced by selective laser melting10.1016/j.prostr.2016.06.298 ↗
38. Bending fatigue life characterisation of direct metal laser sintering nickel alloy 71810.1111/ffe.12286 ↗
39. Selective laser melting additive manufactured Inconel 718 superalloy parts: high-temperature oxidation property and its mechanisms10.1016/j.optlastec.2014.03.008 ↗
40. High temperature oxidation of IN 718 manufactured by Laser Beam Melting and Electron beam Melting: effect of surface topography10.1016/j.corsci.2018.07.005 ↗
41. Microstructure and hardness studies of Inconel 718 manufactured by selective laser melting before and after solution heat treatment10.1016/j.msea.2017.02.062 ↗
42. Hydrogen diffusion coefficients through Inconel 718 in different metallurgical conditions10.1016/j.corsci.2013.11.002 ↗
43. The advantage of grain refinement in the hydrogen embrittlement of Fe–18Mn–0.6C twinning-induced plasticity steel10.1016/j.corsci.2015.01.012 ↗
44. Variation of hardness, microstructure, and laves phase distribution in direct laser deposited alloy 718 cuboids10.1016/j.matdes.2017.01.031 ↗
45. Laves phase control of Inconel 718 alloy using quasi-continuous-wave laser additive manufacturing10.1016/j.matdes.2017.03.004 ↗
46. Hydrogen embrittlement behavior of Inconel 718 alloy at room temperature10.1016/j.jmst.2018.10.002 ↗
47. Effect of heat treatment on hydrogen-assisted fracture behavior of PH13-8Mo steel10.1016/j.corsci.2017.09.018 ↗
48. The role of hydrogen and other interstitials in the mechanical behavior of metals10.1007/s13632-016-0319-4 ↗
49. The role of localized deformation in hydrogen-assisted crack propagation in 21Cr–6Ni–9Mn stainless steel10.1016/j.actamat.2009.04.027 ↗
50. Effect of strain rate on the hydrogen embrittlement property of ultra high-strength low alloy TRIP-aided steel10.2355/isijinternational.ISIJINT-2017-576 ↗
51. Hydrogen embrittlement of AISI 4130 steel with an alternate ferrite/pearlite banded structure10.1016/0921-5093(91)90658-A ↗
52. Effects of microstructure banding on hydrogen assisted fatigue crack growth in X65 pipeline steels10.1016/j.ijfatigue.2015.09.004 ↗
53. Effects of ferrite/pearlite alignment on the hydrogen permeation in a AISI 4130 steel10.1016/S0167-577X(96)00140-1 ↗
54. The effect of nanosized (Ti, Mo) C precipitates on hydrogen embrittlement of tempered lath martensitic steel10.1016/j.actamat.2014.04.051 ↗
55. Suppression of hydrogen embrittlement by formation of a stable austenite layer in metastable austenitic stainless steel10.1016/j.scriptamat.2014.07.005 ↗
56. Suppression of hydrogen-assisted fatigue crack growth in austenitic stainless steel by cavitation peening10.1016/j.ijhydene.2011.12.035 ↗
57. The behavior of sensitized 309S stainless steel in hydrogen10.1016/0025-5416(74)90106-2 ↗
58. Hydrogen compatibility of austenitic stainless steel tubing and orbital tube welds10.1016/j.ijhydene.2014.03.229 ↗
59. Effect of microstructure on hydrogen diffusion and notch tensile strength of large steel forging10.1016/j.msea.2015.01.040 ↗
60. The dual role of shot peening in hydrogen-assisted cracking of PSB1080 high strength steel10.1016/j.matdes.2016.07.121 ↗
61. Microstructural and fractographic features of hydrogen-accelerated fatigue-crack growth in steels
62. Hydrogen-assisted decohesion and localized plasticity in dual-phase steel10.1016/j.actamat.2014.01.048 ↗
63. Hydrogen-induced intergranular failure of iron10.1016/j.actamat.2014.01.060 ↗
64. Mechanical properties and fracture behavior of hydrogen charged AHSS/UHSS grades at high-and low strain rate tests10.1016/j.msea.2013.10.044 ↗
65. The role of hydrogen in hydrogen embrittlement fracture of lath martensitic steel10.1016/j.actamat.2012.06.040 ↗