The influence of a KCl-rich environment on the corrosion attack of 304 L: 3D FIB/SEM and TEM investigations
Source abstract
Abstract
This study investigates the intergranular corrosion of a stainless steel (304 L) in the presence of KCl(g)/KCl(s) at 600 °C by using a FIB/SEM to perform 3D reconstruction/tomography of grain boundary attacks in combination with TEM. The investigation shows that the combination of the 3D FIB/TEM offers a great potential for the study of complex features, i.e. intergranular corrosion. The initiation and propagation of the grain boundary attack occurred very rapidly below an intact secondary protection. No large accumulations of metal chlorides were observed at the grain boundary regions. Instead, indications of very rapid alloy diffusion in grain boundary regions were observed.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Corrosion Behavior and Inhibition · Non-Destructive Testing Techniques
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (64)
Show source-provided references
1. Värme · 2020
2. Reducing high-temperature corrosion on high-alloyed stainless steel superheaters by co-combustion of municipal sewage sludge in a fluidised bed boiler10.1016/j.fuel.2014.09.007 ↗
3. The importance of SO2 and SO3 for sulphation of gaseous KCl – An experimental investigation in a biomass fired CFB boiler10.1016/j.combustflame.2010.05.012 ↗
4. Measures to reduce chlorine in deposits: application in a large-scale circulating fluidised bed boiler firing biomass10.1016/j.fuel.2010.12.005 ↗
5. Two strategies to reduce gaseous KCl and chlorine in deposits during biomass combustion—injection of ammonium sulphate and co-combustion with peat10.1016/j.fuproc.2011.06.025 ↗
6. Characterising ash of biomass and waste10.1016/j.fuproc.2007.06.011 ↗
7. The implications of chlorine-associated corrosion on the operation of biomass-fired boilers10.1016/S0360-1285(00)00003-4 ↗
8. An overview of the organic and inorganic phase composition of biomass10.1016/j.fuel.2011.09.030 ↗
9. Potassium, chlorine, and sulfur in ash, particles, deposits, and corrosion during wood combustion in a circulating fluidized-bed boiler10.1021/ef060306c ↗
10. Fireside corrosion of stainless and low alloyed steels in a waste-fired CFB boiler; The effect of adding sulphur to the fuel10.4028/www.scientific.net/MSF.595-598.289 ↗
11. The effects of chlorides, hydrogen chloride, and sulfur dioxide in the oxidation of steels below deposits10.1016/0010-938X(95)00011-8 ↗
12. Oxidation after breakdown of the chromium-rich scale on stainless steels at high temperature: internal oxidation10.1007/s11085-016-9610-7 ↗
13. KCl-induced high temperature corrosion of selected commercial alloys10.1002/maco.201408213 ↗
14. High temperature corrosion of superheater steels by KCl and K2CO3 under dry and wet conditions10.1016/j.fuproc.2012.05.020 ↗
15. Effect of flue gas composition on deposit induced high temperature corrosion under laboratory conditions mimicking biomass firing. Part I: exposures in oxidizing and chlorinating atmospheres10.1002/maco.201609173 ↗
16. High temperature corrosion during biomass firing: improved understanding by depth resolved characterisation of corrosion products10.1179/0960340914Z.00000000081 ↗
17. KCl induced corrosion of a 304-type austenitic stainless steel at 600°C; the role of potassium10.1007/s11085-005-5704-3 ↗
18. The effects of KCl, K2SO4 and K2CO3 on the high temperature corrosion of a 304-type austenitic stainless steel10.1007/s11085-011-9240-z ↗
19. The effects of KCl, NaCl and K2CO3 on the high-temperature oxidation onset of sanicro 28 steel10.1007/s11085-016-9613-4 ↗
20. Deposition and high temperature corrosion in a 10 MW straw fired boiler10.1016/S0378-3820(97)00062-3 ↗
21. In‐situ corrosion investigation at Masnedø CHP plant–a straw‐fired power plant10.1002/(SICI)1521-4176(199910)50:10<579::AID-MACO579>3.0.CO;2-M ↗
22. A surface analytical approach to the high temperature chlorination behaviour of inconel 600 at 700 °C10.1016/S0010-938X(96)00112-6 ↗
23. Initial stages of the HCl-induced high-temperature corrosion of alloy 31010.1149/1.2754174 ↗
24. Acceleration of the high temperature oxidation of metals by chlorine
25. Accelerated oxidation rate of chromium induced by sodium chloride10.1007/BF00659274 ↗
26. Morphological development of subscale formation in Fe–Cr–(Ni) alloys with chloride and sulfates coating10.1023/A:1020119107724 ↗
27. Chloridation and oxidation of iron, chromium, nickel and their alloys in chloridizing and oxidizing atmospheres at 400–700°C10.1016/S0010-938X(99)00142-0 ↗
28. Oxidation driven permeation of Iron oxide scales by chloride from experiment guided first-principles modeling10.1021/acs.jpcc.9b06497 ↗
29. An ESEM in situ investigation of initial stages of the KCl induced high temperature corrosion of a Fe–2.25Cr–1Mo steel at 400°C10.1016/j.corsci.2011.03.007 ↗
30. Continuous KCl addition in high temperature exposures of 304 L – a way to mimic a boiler environment10.1016/j.corsci.2020.108511 ↗
31. Increased steam temperature in grate fired boilers - steamboost
32. FactSage thermochemical software and databases10.1016/S0364-5916(02)00035-4 ↗
33. The CT scan standard reconstruction technique for reliable jaw bone volume determination
34. A CT scan technique for quantitative volumetric assessment of the mandible after distraction osteogenesis10.1097/00006534-199705000-00005 ↗
35. A novel technique for the determination of body fat by computed tomography
36. Three-dimensional analysis of porous BaTiO3 ceramics using FIB nanotomography10.1111/j.0022-2720.2004.01397.x ↗
37. 3D determination of grain shape in a FeAl-based nanocomposite by 3D FIB tomography10.1016/S1359-6462(01)01090-9 ↗
38. Formation of corrosion pockets in FeNiCrAl at high temperatures investigated by 3D FIB-SEM tomography10.1002/maco.201911386 ↗
39. Tomographic spectral imaging with multivariate statistical analysis: comprehensive 3D microanalysis10.1017/S1431927606060193 ↗
40. Effects of boundary migration and pinning particles on intergranular oxidation revealed by 2D and 3D analytical electron microscopy10.1016/j.actamat.2017.04.003 ↗
41. Understanding surface oxidation in stainless steels through 3D FIB sequential sectioning10.1088/1742-6596/371/1/012086 ↗
42. Three-dimensional characterization of stress corrosion cracks10.1016/j.jnucmat.2010.11.068 ↗
43. Focussed ion beam sectioning for the 3D characterisation of cracking in oxide scales formed on commercial ZIRLOTM alloys during corrosion in high temperature pressurised water10.1016/j.corsci.2011.08.013 ↗
44. Development of an ion and Electron Dual focused beam apparatus for three-dimensional microanalysis10.1143/JJAP.37.2051 ↗
45. Three dimensional microstructural characterization of nanoscale precipitates in AA7075-T651 by focused ion beam (FIB) tomography10.1016/j.matchar.2016.05.009 ↗
46. Fiji: an open-source platform for biological-image analysis10.1038/nmeth.2019 ↗
47. The ImageJ ecosystem: an open platform for biomedical image analysis10.1002/mrd.22489 ↗
48. NIH Image to ImageJ: 25 years of image analysis10.1038/nmeth.2089 ↗
49. (ORS) ORS · 2019
50. Image segmentation methods: a comparative study
51. Kaur · 2014
52. Bhadeshia · 2017
53. Callister · 2007
54. Jones · 1996
55. Khanna · 2002
56. Kofstad · 1988
57. Lai · 2007
58. PERSDOTTER A. Beyond Breakaway Corrosion: Secondary Corrosion Protection of Iron-based Alloys.
59. KCl-Induced High Temperature Corrosion of the Austenitic Stainless Steel 304L–The Influence of SO210.4028/www.scientific.net/MSF.696.224 ↗
60. Time and temperature effects on alkali chloride induced high temperature corrosion of superheaters during biomass firing10.1021/acs.energyfuels.8b01232 ↗
61. Microstructural investigation of the KCl-induced corrosion of the austenitic alloy Sanicro 28 (35Fe27Cr31Ni) at 600 C10.3184/096034009X464339 ↗
62. Effective reduction of chromium-oxy-hydroxide evaporation from Ni-base alloy 69010.1007/s11085-019-09935-9 ↗
63. Alkali induced high temperature corrosion of stainless steel: the influence of NaCl, KCl and CaCl 210.1007/s11085-012-9293-7 ↗
64. KCl-induced corrosion of Ni-based alloys containing 35–45 wt% Cr10.1002/maco.201810658 ↗