journal article·2021-06

Synergistic effect of irradiation and molten salt corrosion: Acceleration or deceleration?

Zhenbo Zhu, Hefei Huang, Guanhong Lei, Yanping Wu, Cuilan Ren, Awen Liu, Zhiyong Zhu

Corrosion Science· Volume 185
Publisher page

Abstract

Abstract The effect of helium ion irradiation with low and high ion fluences on the corrosion behaviour of nickel-based alloys in FLiNaK molten salt at 700 °C was investigated. The microstructure and element distribution were characterized to explore the corrosion behaviour of matrix and grain boundaries. The results showed that irradiation accelerates matrix corrosion in both Inconel 617 and GH3535 alloys. Moreover, the irradiation decelerated and accelerated intergranular corrosion were respectively observed under irradiation with low and high helium ion fluence, which is caused by the combined effects of the self-healing mechanism and diffusion of interstitials and helium atoms.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Fusion materials and technologies · Nuclear Materials and Properties · Nuclear materials and radiation effects

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (34)

Show source-provided references
1. The molten salt reactor (MSR) in generation IV: overview and perspectives10.1016/j.pnucene.2014.02.014 ↗
2. Materials corrosion in molten LiF–NaF–KF salt10.1016/j.jfluchem.2008.05.008 ↗
3. Intergranular corrosion of high temperature alloys in molten fluoride salts10.3184/096034010X12743509428336 ↗
4. Corrosion in the molten fluoride and chloride salts and materials development for nuclear applications10.1016/j.pmatsci.2018.05.003 ↗
5. Corrosion behavior of a wear resistant Co-Mo-Cr-Si alloy in molten fluoride salts10.1016/j.jnucmat.2020.152529 ↗
6. Metallic impurities induced corrosion of a Ni-26W-6Cr alloy in molten fluoride salts at 850 ℃10.1016/j.corsci.2020.109079 ↗
7. Corrosion issues in current and next-generation nuclear reactors
8. Xenon ion irradiation induced hardening in inconel 617 containing experiment and numerical calculation10.1016/j.jnucmat.2019.07.032 ↗
9. Corrosion issues in molten salt reactor (MSR) systems10.1533/9780857095343.6.842 ↗
10. Nanoindentation study on the creep characteristics and hardness of ion-irradiated alloys10.3390/ma13143132 ↗
11. Helium-induced damage behavior in high temperature nickel-based alloys with different chemical composition10.1016/j.jnucmat.2020.152419 ↗
12. Analysis of displacement damage and defect production under cascade damage conditions10.1016/0022-3115(93)90140-T ↗
13. Mitigation of He embrittlement and swelling in nickel by dispersed SiC nanoparticles10.1016/j.matdes.2015.10.147 ↗
14. Effects of bubbles on high-temperature corrosion of helium ion-irradiated Ni-based alloy in fluoride molten salt10.1016/j.corsci.2017.06.027 ↗
15. Irradiation accelerated fluoride molten salt corrosion of nickel-based UNS N10003 alloy revealed by X-ray absorption fine structure10.1016/j.corsci.2019.108408 ↗
16. Corrosion-driven outward migration and growth of helium bubbles in a nickel-based alloy in high-temperature molten salt environment10.1016/j.corsci.2019.03.026 ↗
17. Effects of He ion irradiation on the corrosion performance of alloy GH3535 welded joint in molten FLiNaK10.1016/j.corsci.2018.10.038 ↗
18. Proton irradiation-decelerated intergranular corrosion of Ni-Cr alloys in molten salt10.1038/s41467-020-17244-y ↗
19. Determination of mechanical properties and fracture behavior of hot-rolled Inconel 617/Ni bimetal composite plate10.1007/s11665-020-04885-9 ↗
20. Considerations of alloy 617 application in the Gen IV nuclear reactor systems: part II—metallurgical property challenges10.1115/PVP2009-78146 ↗
21. Muralidharan · 2011
22. On the irradiation tolerance of nano-grained Ni–Mo–Cr alloy: 1 MeV He+ irradiation experiment10.1016/j.jnucmat.2020.152694 ↗
23. In situ TEM observation of the evolution of helium bubbles in Hastelloy N alloy during annealing10.1016/j.jnucmat.2020.152184 ↗
24. SRIM – the stopping and range of ions in matter (2010)10.1016/j.nimb.2010.02.091 ↗
25. Temperature dependence of nickel ion irradiation damage in GH3535 alloy weld metal10.1016/j.jnucmat.2017.06.005 ↗
26. Effect of SO42−on the corrosion of 316L stainless steel in molten FLiNaK salt10.1016/j.corsci.2018.08.057 ↗
27. Effect of TiN diffusion barrier on elements interdiffusion behavior of Ni/GH3535 system in LiF-NaF-KF molten salt at 700 °C10.1016/j.jmst.2019.11.023 ↗
28. Effects of exposing duration on corrosion performance in weld joint of Ni-Mo-Cr alloy in FLiNaK molten salt10.1016/j.jfluchem.2016.07.007 ↗
29. Microstructural evolution and hardening of GH3535 alloy under energetic Xe ion irradiation at room temperature and 650 °C10.1016/j.jnucmat.2017.12.006 ↗
30. Helium accumulation in metals during irradiation – where do we stand?10.1016/j.jnucmat.2003.09.001 ↗
31. Diffusion of helium in nickel10.1016/0022-3115(82)90425-1 ↗
32. Solute‐vacancy interaction model and the effect of minor alloying elements on the initiation of pitting corrosion10.1149/1.2113886 ↗
33. Nickel-plating for active metal dissolution resistance in molten fluoride salts10.1016/j.jnucmat.2011.01.032 ↗
34. Novel features of radiation-induced segregation and radiation-induced precipitation in austenitic stainless steels10.1016/j.actamat.2010.10.055 ↗