High strength and high ductility of a severely deformed high-entropy alloy in the presence of hydrogen
Source abstract
Abstract
High-strength materials usually exhibit low ductility, particularly in the presence of hydrogen embrittlement phenomena. In this study, three strategies are combined to achieve excellent strength-plasticity combinations in the presence of hydrogen: (i) selecting an FCC high-entropy alloy with slow hydrogen lattice diffusion, (ii) adding aluminum to the alloy to hinder surface-to-bulk hydrogen diffusion, and (iii) introducing low-mobility lattice defects like nanotwins and Lomer-Cottrell locks by severe plastic deformation to suppress hydrogen-enhanced localized plasticity and stress concentration. The Al0.1CrFeCoNi alloy severely deformed by high-pressure tor-sion exhibits an ultrahigh yield strength of 1.96 GPa and a high elongation to failure of 10%. ; 1 ; 1 ; N ; scie ; scopus
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: High Entropy Alloys Studies · Metal and Thin Film Mechanics · High-Temperature Coating Behaviors
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (76)
Show source-provided references
1. Paradox of strength and ductility in metals processed by severe plastic deformation10.1557/JMR.2002.0002 ↗
2. Transition from poor ductility to room-temperature superplasticity in a nanostructured aluminum alloy10.1038/s41598-018-25140-1 ↗
3. Nanomaterials by severe plastic deformation: review of historical developments and recent advances10.1080/21663831.2022.2029779 ↗
4. Ultrahigh strength and high electrical conductivity in copper10.1126/science.1092905 ↗
5. Simultaneously increasing the ductility and strength of ultra-fine grained pure copper10.1002/adma.200601472 ↗
6. Strengthening materials by engineering coherent internal boundaries at the nanoscale10.1126/science.1159610 ↗
7. Multifunctional alloys obtained via a dislocation-free plastic deformation mechanism10.1126/science.1081957 ↗
8. Spreading of dislocation cores in elastically anisotropic body-centered-cubic materials: the case of gum metal10.1103/PhysRevB.82.184202 ↗
9. High strength and high uniform ductility in a severely deformed iron alloy by lattice softening and multimodal-structure formation10.1080/21663831.2015.1050126 ↗
10. Mechanical behavior and microstructure of a thermally stable bulk nanostructured Al alloy10.1007/s11661-001-0207-6 ↗
11. High tensile ductility in a nanostructured metal10.1038/nature01133 ↗
12. Extra strengthening and work hardening in gradient nanotwinned metals10.1126/science.aau1925 ↗
13. Heterostructured materials: superior properties from hetero-zone interaction10.1080/21663831.2020.1796836 ↗
14. Inverse temperature dependence of toughness in an ultrafine grain-structure steel10.1126/science.1156084 ↗
15. Achieving high strength and high ductility in precipitation-hardened alloys10.1002/adma.200500069 ↗
16. Influence of Al content and precipitation state on the mechanical behavior of austenitic high-Mn low-density steels10.1016/j.scriptamat.2012.08.038 ↗
17. Brittle intermetallic compound makes ultrastrong low-density steel with large ductility10.1038/nature14144 ↗
18. Experimental and numerical analysis on formation of stable austenite during the intercritical annealing of 5Mn steel10.1016/j.actamat.2011.03.025 ↗
19. Recrystallization behavior, microstructure evolution and mechanical properties of biodegradable Fe-Mn-C(-Pd) TWIP alloys10.1016/j.actamat.2012.01.041 ↗
20. Enhanced strength and ductility in an ultrafine-grained Fe-22Mn-0.6C austenitic steel having fully recrystallized structure10.1007/s11661-014-2552-2 ↗
21. Enumeration of the hydrogen-enhanced localized plasticity mechanism for hydrogen embrittlement in structural materials10.1016/j.actamat.2018.12.014 ↗
22. Resistance of CoCrFeMnNi high-entropy alloy to gaseous hydrogen embrittlement10.1016/j.scriptamat.2017.03.029 ↗
23. Interaction of aluminium with hydrogen in twinning-induced plasticity steel10.1016/j.scriptamat.2014.06.007 ↗
24. Effect of aluminium on hydrogen permeation of high-manganese twinning-induced plasticity steel10.1016/j.scriptamat.2014.11.023 ↗
25. Overview of hydrogen embrittlement in high-Mn steels10.1016/j.ijhydene.2017.02.214 ↗
26. Beating hydrogen with its own weapon: Nano-twin gradients enhance embrittlement resistance of a high-entropy alloy10.1016/j.mattod.2018.07.015 ↗
27. Nanostructured high‐entropy alloys with multiple principal elements: novel alloy design concepts and outcomes10.1002/adem.200300567 ↗
28. Microstructural development in equiatomic multicomponent alloys10.1016/j.msea.2003.10.257 ↗
29. High-entropy alloys10.1038/s41578-019-0121-4 ↗
30. High-entropy ceramics: review of principles, production and applications10.1016/j.mser.2021.100644 ↗
31. Microstructures and properties of high-entropy alloys10.1016/j.pmatsci.2013.10.001 ↗
32. Recent progress in our understanding of phase stability, atomic structures and mechanical and functional properties of high-entropy alloys10.2320/matertrans.MT-M2021234 ↗
33. A critical review of high entropy alloys and related concepts10.1016/j.actamat.2016.08.081 ↗
34. Effect of grain refinement on the hydrogen embrittlement of 304 austenitic stainless steel10.1016/j.jmst.2019.03.043 ↗
35. Effect of grain refinement on hydrogen embrittlement behaviors of high-Mn TWIP steel10.1016/j.msea.2015.11.017 ↗
36. Grain refinement effect on hydrogen embrittlement resistance of an equiatomic CoCrFeMnNi high-entropy alloy10.1016/j.ijhydene.2019.04.280 ↗
37. Hydrogen embrittlement of ultrafine-grained austenitic stainless steels processed by high-pressure torsion at moderate temperature10.2355/isijinternational.ISIJINT-2015-664 ↗
38. The synergistic action and interplay of hydrogen embrittlement mechanisms in steels and iron: localized plasticity and decohesion
39. Ultrahigh hardness in nanostructured dual-phase high-entropy alloy AlCrFeCoNiNb developed by high-pressure torsion10.1016/j.jallcom.2021.161101 ↗
40. Microstructure and microhardness of dual-phase high-entropy alloy by high-pressure torsion: twins and stacking faults in FCC and dislocations in BCC10.1016/j.jallcom.2021.162413 ↗
41. An example of the effect of hydrogen trapping on hydrogen embrittlement10.1007/BF02648348 ↗
42. Hydrogen-assisted failure in a twinning-induced plasticity steel studied under in situ hydrogen charging by electron channeling contrast imaging10.1016/j.actamat.2013.04.030 ↗
43. Influence of nanotwins on hydrogen embrittlement of TWIP (twinning-induced plasticity) steel processed by high-pressure torsion10.1016/j.msea.2020.139273 ↗
44. Dynamic mechanical responses of the Al0.1CoCrFeNi high entropy alloy at cryogenic temperature10.1016/j.msea.2020.140125 ↗
45. Effects of high pressure torsion on microstructures and properties of an Al0.1CoCrFeNi high-entropy alloy10.1016/j.msea.2015.12.085 ↗
46. Hydrogen embrittlement of the equi-molar FeNiCoCr alloy10.1016/j.actamat.2018.07.032 ↗
47. Resistance sintering of CoCrFeNiAlx (x=0.7, 0.85, 1) high entropy alloys: Microstructural characterization, oxidation and corrosion properties10.1016/j.jallcom.2021.160180 ↗
48. Effect of valence electron concentration on stability of fcc or bcc phase in high entropy alloys10.1063/1.3587228 ↗
49. Transmission electron microscopy characterization of dislocation structure in a face-centered cubic high-entropy alloy Al0.1CoCrFeNi10.1016/j.actamat.2017.10.050 ↗
50. A review on high-pressure torsion (HPT) from 1935 to 198810.1016/j.msea.2015.11.074 ↗
51. Microstructure and defect effects on strength and hydrogen embrittlement of high-entropy alloy CrMnFeCoNi processed by high-pressure torsion10.1016/j.msea.2022.143179 ↗
52. On the minimum grain size obtainable by high- pressure torsion10.1016/j.msea.2012.07.066 ↗
53. Saturation of grain refinement during severe plastic deformation of single phase materials: reconsiderations, current status and open questions10.2320/matertrans.MF201918 ↗
54. Effect of dislocation cell walls on hydrogen adsorption, hydrogen trapping and hydrogen embrittlement resistance10.1016/j.corsci.2020.108428 ↗
55. Influence of hydrogen on dislocation self-organization in Ni10.1016/j.actamat.2017.05.073 ↗
56. Hydrogen embrittlement of the equi-molar FeNiCoCr alloy10.1016/j.actamat.2018.07.032 ↗
57. Effects of hydrogen on the properties of iron and steel10.1007/BF02654700 ↗
58. Hydrogen delayed fracture properties and internal hydrogen behavior of a Fe–18Mn–1.5Al–0.6C TWIP steel10.2355/isijinternational.49.1952 ↗
59. Effect of grain size on the susceptibility of martensitic steel to hydrogen-related failure10.1080/09500830500482316 ↗
60. Effect of grain size on the resistance to hydrogen embrittlement of API 2W grade 60 steels using in situ slow-strain-rate testing10.1016/j.corsci.2017.08.032 ↗
61. Resistance of CoCrFeMnNi high-entropy alloy to gaseous hydrogen embrittlement10.1016/j.scriptamat.2017.03.029 ↗
62. A nanotwinned austenite stainless steel with high hydrogen embrittlement resistance10.1016/j.jallcom.2019.02.312 ↗
63. Hydrogen-assisted failure in a bimodal twinning-induced plasticity steel: Delamination events and damage evolution10.1016/j.ijhydene.2017.11.177 ↗
64. The effect of Si on hydrogen embrittlement of Fe-18Mn-0.6C-xSi twinning-induced plasticity steels10.1016/j.actamat.2015.10.015 ↗
65. Effects of grain size on hydrogen embrittlement in a Fe-22Mn-0.6C TWIP steel10.1016/j.ijhydene.2015.06.112 ↗
66. Grain boundary engineering approach to improve hydrogen embrittlement resistance in FeMnC TWIP steel10.1016/j.ijhydene.2018.04.048 ↗
67. Hydrogen embrittlement in a Fe–Mn–C ternary twinning-induced plasticity steel10.1016/j.corsci.2011.09.022 ↗
68. Role of Cu on hydrogen embrittlement behavior in Fe-Mn-C-Cu TWIP steel, Int. J. Hydrog
69. Improving hydrogen embrittlement resistance of Hadfield steel by thermo-mechanical flash-treatment10.1016/j.msea.2017.11.036 ↗
70. An investigation of micro-mechanisms in hydrogen induced cracking in nickel-based superalloy 71810.1016/j.jallcom.2016.01.033 ↗
71. Effects of Mn content and grain size on hydrogen embrittlement susceptibility of face-centered cubic high-entropy alloys10.1007/s11661-020-05966-z ↗
72. Effects of interstitial C and N on hydrogen embrittlement behavior of non-equiatomic metastable FeMnCoCr high-entropy alloys10.1016/j.corsci.2021.109933 ↗
73. Comparative study of hydrogen embrittlement in stable and metastable high-entropy alloys10.1016/j.scriptamat.2018.03.003 ↗
74. Hydrogen embrittlement and associated surface crack growth in fine-grained equiatomic CoCrFeMnNi high-entropy alloys with different annealing temperatures evaluated by tensile testing under in situ hydrogen charging10.1016/j.ijhydene.2021.07.136 ↗
75. Influence of pre-strain on the gaseous hydrogen embrittlement resistance of a high-entropy alloy10.1016/j.msea.2018.01.107 ↗
76. Gradient-structured high-entropy alloy with improved combination of strength and hydrogen embrittlement resistance10.1016/j.corsci.2022.110253 ↗