Oxidation and corrosion of silicon nitride ceramics with different sintering additives at 1200 and 1500°C in air, water vapour, SO2 and HCl environments – A comparative study
Source abstract
Abstract
Abstract The effect of different sintering additives on the high temperature oxidation and corrosion behaviour of silicon nitride based ceramics was investigated. Comparative tests were conducted at 1200 and 1500 °C in air, in water vapour, and with the highly corrosive gases HCl and SO2. Si3N4 was prepared with MgO, Al2O3, Y2O3 and Al2O3 + Y2O3 sintering additives. Hot pressed discs were tested for a total time of up to 128 h. The electrically conductive ceramic composites Si3N4 + TiN and Si3N4 + MoSi2 were also tested under the same conditions. The effects that the different corrosion environments have on the different ceramics are presented. SEM studies of the oxidised ceramics show the direct transformation of Si3N4 grains into SiO2 through a reaction interface layer.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced ceramic materials synthesis · MXene and MAX Phase Materials · Semiconductor materials and devices
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (11)
Show source-provided references
1. Low-additive Si3N4 in high temperature combustion gases10.1016/S0955-2219(98)00238-6 ↗
2. Additive Effects on Si3N4 oxidation/volatilization in water napor10.1111/j.1151-2916.2003.tb03462.x ↗
3. Review Particulate silicon nitride-based composites10.1007/BF00356803 ↗
4. Fractography, mechanical properties, and microstructure of commercial silicon nitride-titanium nitride composites10.1111/j.1551-2916.2005.00186.x ↗
5. Paralinear Oxidation of Silicon Nitride in a Water-Vapor/Oxygen Environment10.1111/j.1151-2916.2003.tb03461.x ↗
6. The effect of different sintering additives on the electrical and oxidation properties of Si3N4-MoSi2 composites10.1016/j.jeurceramsoc.2006.07.009 ↗
7. Failure behaviour of high toughness multi-layer Si3 N4 and Si3 N4-TiN based laminates10.4028/www.scientific.net/KEM.290.175 ↗
8. Factors inducing degradation of properties after long term oxidation of Si3N4-TiN electroconductive composites10.1016/S0169-4332(02)00498-1 ↗
9. Corrosion of silicon nitride materials in gas turbine environment10.1016/S0955-2219(02)00143-7 ↗
10. Long-term stability of non-oxide ceramics in an oxidative environment at 1500°C10.1016/S0955-2219(02)00267-4 ↗
11. Hot gas corrosion of structural ceramics