journal article·2007-09

Hydrogen assisted cracking in progressively drawn pearlitic steel

J. Toribio, E. Ovejero

Corrosion Science· Volume 49· Issue 9
Publisher page

Abstract

This paper analyses the hydrogen assisted cracking (HAC) behaviour of cold drawn prestressing steels with different degrees of cold drawing. The experimental results showed a progressively anisotropic behaviour as the degree of cold drawing increases, with an evolution in the fracture behaviour from mode I (isotropic behaviour in slightly drawn steels) to mixed mode propagation (strongly anisotropic behaviour in heavily drawn steels). The fractographic analysis revealed changes in the microscopic topography depending on the fracture propagation mode, with evolution from pure tearing topography surface (TTS) in slightly drawn steels to a kind of very deformed TTS in heavily drawn steels.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Material Properties and Failure Mechanisms · Non-Destructive Testing Techniques

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (18)

Show source-provided references
1. The structure and properties of drawn pearlite10.1016/0001-6160(66)90296-3 ↗
2. A Study of the deformation of patented steel wire10.1007/BF02811557 ↗
3. Microstructure evolution in a pearlitic steel subjected to progressive plastic deformation10.1016/S0921-5093(97)00231-1 ↗
4. Microstructure orientation in a pearlitic steel subjected to progressive plastic deformation10.1023/A:1006647008543 ↗
5. Effect of cumulative cold drawing on the pearlite interlamellar spacing in eutectoid steel10.1016/S1359-6462(98)00166-3 ↗
6. Effect of cold drawing on microstructure and corrosion performance of high-strength steel10.1023/A:1009714222132 ↗
7. Pitting, crevice and stress corrosion cracking studies of cold drawn eutectoid steels10.1016/0010-938X(80)90089-X ↗
8. Hydrogen induced delayed failure of high strength alloy steel wires10.5006/1.3585987 ↗
9. Environment sensitive cracking of pre-stressing steels10.1016/0010-938X(82)90017-8 ↗
10. A. Valiente, Criterios de fractura para alambres. Ph. D Thesis, Polytechnic University of Madrid, Spain, 1980.
11. Identification of a fracture mode: the tearing topography surface10.1007/BF02811666 ↗
12. Hydrogen cracking in nominally pearlitic 1045 steel10.1007/BF02645516 ↗
13. Characteristics of the new tearing topography surface10.1016/0956-716X(91)90007-N ↗
14. The tearing topography surface as the zone associated with hydrogen embrittlement processes in pearlitic steel10.1007/BF02647339 ↗
15. Fracture mechanics approach to hydrogen assisted microdamage in eutectoid steel10.1007/s11661-997-0095-5 ↗
16. Hydrogen-assisted micro-damage evolution in pearlitic steel10.1023/A:1018520218360 ↗
17. Tensile fractures in carbon steels
18. W.W. Gerberich, P. Marsh, J. Hoehn, S. Venkataraman, H. Huang, Hydrogen/ plasticity interactions in stress corrosion cracking, in: T. Magnin, J.M. Gras (Eds.), Corrosion–Deformation Interactions (CDI’92), Les Editions de Physique, Les Ulis, 1993, pp. 325–353.