Desulfurized flue gas corrosion coupled with deposits in a heating boiler
Source abstract
Abstract
Abstract In-plant corrosion tests of five steels were conducted in a heating boiler in China to study the desulfurized flue gas corrosion coupled with deposits after the FGD (flue gas desulfurization) unit. The surface temperature of the steel was the key factor in the deposition and corrosion process. As the surface temperature increased, the corrosion of the steels was first exacerbated due to the increase in the Cl− concentration in the deposits and then mitigated due to the lack of the electrolyte. The stainless steels in this work showed much better performance than did the low alloy steel.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Industrial Gas Emission Control · High-Temperature Coating Behaviors · nanoparticles nucleation surface interactions
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (49)
Show source-provided references
1. Flue gas desulfurization: the state of the art10.1080/10473289.2001.10464387 ↗
2. Status of Flue Gas Desulphurisation (FGD) systems from coal-fired power plants: overview of the physic-chemical control processes of wet limestone FGDs10.1016/j.fuel.2014.12.065 ↗
3. Environmental impact of a coal combustion-desulphurisation plant: abatement capacity of desulphurisation process and environmental characterisation of combustion by-products10.1016/j.chemosphere.2006.06.070 ↗
4. Detailed modelling of a flue-gas desulfurisation plant10.1016/j.compchemeng.2006.12.004 ↗
5. A model for performance optimization of wet flue gas desulfurization systems of power plants10.1016/j.fuproc.2008.04.004 ↗
6. Corrosion experience with carbon steel in spray absorption FGD plant10.1002/maco.19920430612 ↗
7. Corrosion in flue gas desulfurization plants and other low temperature equipment10.1002/maco.19920430610 ↗
8. Corrosion-resistant special steels for flue gas desulphurisation plants10.1002/maco.19920430605 ↗
9. Crum · 1996
10. Durability evaluation of Ni-Cr-Mo super alloys in a simulated scrubbed flue gas environment10.1108/00035599910252703 ↗
11. Phull · 2000
12. Effect of antimony on the corrosion behavior of low-alloy steel for flue gas desulfurization system10.1016/j.corsci.2007.11.027 ↗
13. Experience in effective application of metallic materials for construction of FGD systems
14. A comparative study on several anti-corrosion materials for power FGD system10.4236/eng.2011.36078 ↗
15. Shoemaker · 2011
16. Montgomery · 2015
17. Influence of temperature on the electrochemical and passivation behavior of 2507 super duplex stainless steel in simulated desulfurized flue gas condensates10.1016/j.corsci.2017.01.016 ↗
18. Corrosion of austenitic and duplex stainless steels in flue gas cleaning systems for waste combustion processes
19. Full-scale measurements of SO2 gas phase concentrations and slurry compositions in a wet flue gas desulphurisation spray absorber10.1016/j.fuel.2003.12.007 ↗
20. Failure analysis of enamel-coated carbon steel heating elements of gas–gas heater for flue gas desulfurization system10.1016/j.engfailanal.2006.02.009 ↗
21. Deposits on heat transfer tubes during co-combustion of biofuels and sewage sludge10.1016/j.fuel.2006.01.001 ↗
22. The effect of chlorine and sulfur on the composition of ash deposits in a fluidized bed combustion system10.1021/ef990197k ↗
23. Pitting corrosion mechanism of Type 304 stainless steel under a droplet of chloride solutions10.1016/j.corsci.2006.08.016 ↗
24. Corrosion behaviour of 316L stainless steel and anti-corrosion materials in a high acidified chloride solution10.1016/j.apsusc.2014.09.205 ↗
25. Study of localized corrosion of 304 stainless steel under chloride solution droplets using the wire beam electrode10.1016/j.corsci.2011.05.051 ↗
26. Corrosion behaviour of ferrite and austenite phases on super duplex stainless steel in a modified green-death solution10.1016/j.corsci.2014.08.014 ↗
27. Corrosion of low carbon steel in atmospheric environments of different chloride content10.1016/j.corsci.2009.02.009 ↗
28. Electrochemical behavior of rust formed on carbon steel in a wet/dry environment containing chloride ions10.5006/1.3280597 ↗
29. In situ observation of initial rust formation process on carbon steel under Na2SO4 and NaCl solution films with wet/dry cycles using synchrotron radiation X-rays10.1016/j.corsci.2004.10.021 ↗
30. In-depth distribution of rusts on a plain carbon steel and weathering steels exposed to coastal-industrial atmosphere for 17 years10.1016/S0010-938X(03)00070-2 ↗
31. On the formation of β-FeOOH (akaganéite) in chloride-containing environments10.1016/j.corsci.2006.06.003 ↗
32. Corrosion analysis and characteristics of discarded military munitions in ocean waters10.1016/j.corsci.2015.09.014 ↗
33. Low temperature stress corrosion cracking of stainless steels in the atmosphere in presence of chloride deposits10.5006/1.3319115 ↗
34. The influence of airborne salinity on the atmospheric corrosion of steel10.1016/0010-938X(95)00058-R ↗
35. Holmes · 1985
36. Estimation of combustion flue gas acid dew point during heat recovery and efficiency gain10.1016/j.applthermaleng.2011.01.020 ↗
37. Application of a low pressure economizer for waste heat recovery from the exhaust flue gas in a 600MW power plant10.1016/j.energy.2012.01.045 ↗
38. A numerical study of the deposition characteristics of sulfuric acid vapor on heat exchanger surfaces10.1016/j.ces.2013.07.024 ↗
39. Prediction of acid dew point in flue gas of boilers burning fossil fuels10.1021/acs.energyfuels.6b00491 ↗
40. Coupling mechanism of dew point corrosion and viscous ash deposits10.1002/maco.201307042 ↗
41. Mechanism research on coupling effect between dew point corrosion and ash deposition10.1016/j.applthermaleng.2012.12.013 ↗
42. Low-temperature ash deposition and dewpoint corrosion of a coal-fired travelling grate boiler10.1016/j.applthermaleng.2017.02.052 ↗
43. A review on the use of calcium chloride in applied thermal engineering10.1016/j.applthermaleng.2014.09.047 ↗
44. Temperature effect in the corrosion resistance of Ni−Fe−Cr alloy in chloride medium10.1016/j.corsci.2008.06.030 ↗
45. Passivation of stainless steels in hydrochloric acid10.1149/1.1391777 ↗
46. Formation of magnetite rust particles by reacting iron powder with artificial α-, β- and γ-FeOOH in aqueous media10.1016/j.corsci.2013.08.023 ↗
47. The mechanisms of oxidation of ferrous hydroxychloride β-Fe2(OH)3Cl in aqueous solution: the formation of akaganeite vs goethite10.1016/S0010-938X(97)86102-1 ↗
48. Pitting corrosion evaluation of austenitic stainless steel type 304 in acid chloride media
49. Passive films on stainless steels—chemistry, structure and growth10.1016/S0013-4686(02)00841-1 ↗