Microstructural investigation of the nodular corrosion of 304NG stainless steel in supercritical water

Donghai Du, Kai Chen, Lefu Zhang, Zhao Shen

Corrosion Science· Volume 170
Publisher page

Abstract

Abstract 304NG stainless steel was exposed to deaerated 600 °C supercritical water for 300 h. The thin Cr-rich oxide film and corrosion nodules were characterized in detail by cutting edge techniques. The results show that the formation of MnCr2O4 is an important factor that deteriorates the protectiveness of the Cr-rich thin oxide film. Reaction zones ahead of the inner oxide are observed. The reaction zones are composed of oxide particles and remaining metal, indicating the occurrence of internal oxidation. The internal oxidation controls the further corrosion after the breakdown of Cr-rich thin oxide film, and subsequently the generation of corrosion nodules.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: High-Temperature Coating Behaviors · Subcritical and Supercritical Water Processes · Nuclear Materials and Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (31)

Show source-provided references
1. Materials challenges for generation IV nuclear energy systems10.13182/NT08-A3961 ↗
2. Corrosion and stress corrosion cracking in supercritical water10.1016/j.jnucmat.2007.05.017 ↗
3. Selection and corrosion evaluation tests of candidate SCWR fuel cladding materials10.1016/j.nucengdes.2011.08.086 ↗
4. Indication of chromium oxide hydroxide evaporation during oxidation of 304L at 873 K in the presence of 10% water vapor10.1023/A:1018875024306 ↗
5. A comparative study on the oxidation of austenitic alloys 304 and 304-oxide dispersion strengthened steel in supercritical water at 650 °C10.1016/j.supflu.2016.10.002 ↗
6. Microstructural investigation of the breakdown of the protective oxide scale on a 304 steel in the presence of oxygen and water vapour at 600 °C10.1016/j.corsci.2005.08.012 ↗
7. The effect of H2 and H2O on the oxidation of 304L-stainless steel at 600 °C: general behaviour (Part I)10.1007/s11085-015-9597-5 ↗
8. Oxidation behaviour of alloys 800H, 3033 and 304 in high-temperature supercritical water10.1007/s11085-017-9784-7 ↗
9. Oxidation after breakdown of the chromium-rich scale on stainless steels at high temperature: internal oxidation10.1007/s11085-016-9610-7 ↗
10. High-temperature oxidation of FeCr(Ni) alloys: the behaviour after breakaway10.1007/s11085-017-9731-7 ↗
11. Oxidation behaviour of Super 304H stainless steel in supercritical water10.1080/1478422X.2018.1459064 ↗
12. Early oxidation of Super304H stainless steel and its scales stability in supercritical water environments10.1016/j.ijhydene.2016.04.144 ↗
13. Beneficial effect of cold-working on high temperature oxidation resistance of austenitic stainless steel10.1016/j.corsci.2019.108149 ↗
14. Effect of grain refinement on the resistance of 304 stainless steel to breakaway oxidation in wet air10.1016/j.actamat.2005.07.019 ↗
15. Steam oxidation of Super 304H and shot-peened Super 304H10.3184/096034012X13316633785757 ↗
16. Effect of shot peening on the oxidation resistance of TP304H and HR3C steels in water vapor10.1007/s11085-011-9270-6 ↗
17. The oxidation behaviour of an austenitic steel in deaerated supercritical water at 600–700 °C10.1016/j.matchar.2017.07.023 ↗
18. On the oxidation of stainless steel alloy 304 in subcritical and supercritical water10.1016/j.jnucmat.2014.05.049 ↗
19. Chromium volatilization rates from Cr2O3 scales into flowing gases containing water vapor10.1007/s11085-006-9030-1 ↗
20. Was · 2006
21. Henry · 2001 · 353
22. The effect of water vapor on the oxidation behavior of 9%Cr steels in simulated combustion gases10.1007/s002160050942 ↗
23. High-temperature oxidation of Fe-Cr alloys in wet oxygen10.1007/BF01670507 ↗
24. The effect of temperature on the SSRT behavior of austenitic stainless steels in SCW10.1016/j.jnucmat.2014.08.006 ↗
25. The effect of surface finish on the scaling behavior of stainless steel in steam and supercritical water10.1007/s11085-013-9380-4 ↗
26. Diffusion of cations in chromia layers grown on iron-base alloys10.1007/BF00665632 ↗
27. Effects of Si, Mn on the corrosion behavior of ferritic-martensitic steels in supercritical water (SCW) environments10.1016/j.corsci.2020.108432 ↗
28. The oxidation of iron-chromium-Manganese alloys at 90010.1007/BF00938460 ↗
29. Characterization of the crack initiation and propagation in Alloy 600 with a cold-worked surface10.1016/j.corsci.2019.03.014 ↗
30. Effect of grain refinement on corrosion of ferritic-martensitic steels in supercritical water environment10.1002/maco.200905446 ↗
31. Effect of machining on stress corrosion crack initiation in warm-forged type 304L stainless steel in high temperature water10.1016/j.actamat.2018.11.046 ↗