Effect of Ni on the oxidation behavior of corrosion products that form on low alloy steel exposed to a thin electrolyte layer environment
Source abstract
Abstract
The oxidation behavior of corrosion products that form on Ni-containing low alloy steel was investigated by electrochemical polarization curves, scanning electron microscopy, electron probe micro-analyzer, X-ray diffraction, transmission electron microscopy, and X-ray photoelectron spectroscopy. The corrosion products were oxidized to Green Rust containing Cl - (Green Rust(Cl - )) and an amorphous substance, which were produced in an ordinary- and negative-pressure environment, respectively. The enrichment of Ni in the corrosion product could inhibit two oxidation reactions of the corrosion product, especially inhibiting the formation of amorphous substances. In addition, oxygen reduction could be also suppressed via the enrichment of Ni.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Corrosion Behavior and Inhibition · High-Temperature Coating Behaviors · Anodic Oxide Films and Nanostructures
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (52)
Show source-provided references
1. In situ observation of initial rust formation process on carbon steel under Na2SO4 and NaCl solution films with wet/dry cycles using synchrotron radiation X-rays10.1016/j.corsci.2004.10.021 ↗
2. An electrochemical study of the atmospheric corrosion of iron—II. Cathodic and anodic processes on uncorroded and pre-corroded iron10.1016/0010-938X(94)90142-2 ↗
3. Influences of metal ions on the formation of γ-FeOOH and magnetite rusts
4. Influences of metal ions on the formation of γ-FeOOH and magnetite rusts
5. The corrosion protection mechanism of rust converters: An electrochemical impedance spectroscopy study10.1016/j.electacta.2009.09.084 ↗
6. The role of rusts in corrosion and corrosion protection of iron and steel10.1016/j.corsci.2008.03.008 ↗
7. Airborne chloride deposit and its effect on marine atmospheric corrosion of mild steel10.1016/j.corsci.2015.04.015 ↗
8. Composition and protective ability of rust layer formed on weathering steel exposed to various environments10.1016/j.corsci.2005.10.004 ↗
9. In-depth distribution of rusts on a plain carbon steel and weathering steels exposed to coastal–industrial atmosphere for 17 years10.1016/S0010-938X(03)00070-2 ↗
10. Taxonomy for protective ability of rust layer using its composition formed on weathering steel bridge10.1016/j.corsci.2006.06.016 ↗
11. Weatherability of 09CuPCrNi steel in a tropical marine environment10.1016/j.corsci.2009.04.024 ↗
12. Evolution of rust layers on carbon steel and weathering steel in high humidity and heat marine atmospheric corrosion10.1016/j.jmst.2019.07.054 ↗
13. Insight into atmospheric pitting corrosion of carbon steel via a dual-beam FIB/SEM system associated with high-resolution TEM10.1016/j.corsci.2019.03.017 ↗
14. Atmospheric corrosion of different steels in marine, rural and industrial environments10.1016/S0010-938X(99)00005-0 ↗
15. Antony H., LeGreen Rustand L., Maréchal L., Perrin S., Dillmann P., Chaussé A., Electrochimica Acta, 51(4): 745–753. Study of lepidocrocite γ-FeOOH electrochemical reduction in neutral and slightly alkaline solutions at 25.10.1016/j.electacta.2005.05.049 ↗
16. Advances in understanding atmospheric corrosion of iron. II. Mechanistic modelling of wet–dry cycles10.1016/j.corsci.2003.09.028 ↗
17. XAS and XRD in situ characterisation of reduction and reoxidation processes of iron corrosion products involved in atmospheric corrosion10.1016/j.corsci.2013.10.012 ↗
18. An electrochemical study of phase-transitions in rust layers10.1016/0010-938X(83)90024-0 ↗
19. The influence of chromium on the atmospheric corrosion of steel
20. Corrosion behavior of steel under wet and dry cycles containing Cr3+ ion10.1016/S0010-938X(03)00023-4 ↗
21. Suzuki,I., Masuko,N., Hisamatsu,Y., Electrochemical properties of iron rust. Corros. Sci. 19, 521–535.10.1016/S0010-938X(79)80135-3 ↗
22. Localisation of oxygen reduction sites in the case of iron long term atmospheric corrosion10.1016/j.corsci.2011.04.002 ↗
23. The mechanism of the oxygen reduction on rust-covered metal substrates10.1016/0010-938X(94)90161-9 ↗
24. Electrochemical reduction of ferric corrosion products and evaluation of galvanic coupling with iron10.1016/j.corsci.2005.06.013 ↗
25. Electrochemical study of indoor atmospheric corrosion layers formed on ancient iron artefacts10.1016/j.electacta.2007.04.029 ↗
26. Control of Fe(O,OH)6 nano-network structures of rust for high atmospheric-corrosion resistance10.1016/j.corsci.2005.04.005 ↗
27. A new method for describing the atomic-scale structure of rusts formed on the iron based alloy surfaces10.2355/isijinternational.43.366 ↗
28. Characterization of corrosion products formed on Ni 2.4 wt%–Cu 0.5 wt%–Cr 0.5 wt% weathering steel exposed in marine atmospheres10.1016/j.corsci.2014.07.011 ↗
29. Magnetic property based characterization of rust on weathering steels10.1016/j.corsci.2004.10.017 ↗
30. Atmospheric corrosion of Ni-advanced weathering steels in marine atmospheres of moderate salinity10.1016/j.corsci.2013.06.053 ↗
31. Benefit of the corrosion product film formed on a new weathering steel containing 3% nickel under marine atmosphere in Maldives10.1016/j.corsci.2019.108416 ↗
32. Effect of Co and Ni on the corrosion behavior of low alloy steels in wetdry environments.pdf10.1016/S0010-938X(00)00018-4 ↗
33. Insight into the product film formed on Ni-advanced weathering steel in a tropical marine atmosphere10.1016/j.apsusc.2017.12.018 ↗
34. Kimura, M., Ohta, N., Kihira, H., n.d., State of Chlorides in Rusts Formed on 3 mass% Ni-added Weathering Steel. ECS Trans. 43, 63–69.10.1149/1.3114949 ↗
35. Electrochemical impedance of thin rust film of low-alloy steels10.1016/j.corsci.2003.08.002 ↗
36. Effect of chloride ion on corrosion resistance of Ni-advanced weathering steel in simulated tropical marine atmosphere10.1016/j.conbuildmat.2020.120937 ↗
37. Long-term monitoring of atmospheric corrosion at weathering steel bridges by an electrochemical impedance method10.1016/j.corsci.2014.06.007 ↗
38. Corrosion monitoring of nickel-containing steels in marine atmospheric environment10.1016/j.corsci.2004.10.009 ↗
39. Five-year atmospheric corrosion of Cu, Cr and Ni weathering steels in a wide range of environments10.1016/j.corsci.2018.06.039 ↗
40. Optimizing the nickel content in weathering steels to enhance their corrosion resistance in acidic atmospheres10.1016/j.corsci.2016.11.016 ↗
41. In situ investigation of atmospheric corrosion behavior of PCB-ENIG under adsorbed thin electrolyte layer10.1016/S1003-6326(16)64213-9 ↗
42. In Situ Study the Electrochemical MiGreen Rustation of Tin under Unipolar Square Wave Electric Field10.1149/2.014311jes ↗
43. The corrosion of tin under thin electrolyte layers containing chloride10.1016/j.corsci.2012.08.040 ↗
44. Electrochemical miGreen Rustation of tin in thin electrolyte layer containing chloride ions10.1016/j.corsci.2013.04.015 ↗
45. The effect of electrolyte layer thickness on electrochemical miGreen Rustation of tin10.1016/j.corsci.2015.04.014 ↗
46. Elimination of the charge effect on zirconia coatings using a focused ion beam for characterization of the three-dimensional microstructure10.1016/j.matchar.2022.111769 ↗
47. The mechanisms of oxidation of ferrous hydroxychloride the β-Fe2(OH)3Cl in aqueous solution: the formation of akaganeite vs goethite10.1016/S0010-938X(97)86102-1 ↗
48. The oxidation of ferrous hydroxide in chloride-containing aqueous media and pourbaix diaGreen Rustams of Green Rusteen rust one10.1016/0010-938X(93)90101-L ↗
49. Mechanisms of formation and structure of Green Rusteen rust one in aqueous corrosion of iron in the presence of chloride ions10.1016/S0010-938X(98)00066-3 ↗
50. Oxidation behavior of NixFe1-x(OH)2 in Cl-containing solution10.1016/S0010-938X(02)00065-3 ↗
51. Formation of ‘ferric Green Rusteen rust’ and/or ferrihydrite by fast oxidation of iron(II–III) hydroxychloride Green Rusteen rust10.1016/S0010-938X(03)00073-8 ↗
52. The oxidation of Ni(II)-Fe(II) hydroxides in chloride-containing aqueous media10.1016/0010-938X(93)90060-T ↗