Kinetics and mechanism of reaction between water vapor, carbon monoxide and a chromia-forming nickel base alloy
Source abstract
Abstract
Abstract The kinetic aspects of the competitive reaction of CO and H 2 O in the formation of chromia layer on a nickel base alloy at high temperature were studied by thermogravimetry combined to gas phase chromatography. It was shown that competitive adsorption occurred between both molecules and that whatever P CO / P H 2 O ratio, CO mainly reacted in the first instants of oxidation and H 2 O became the main long-term oxidant species. After an interfacial and diffusion mixed kinetic regime, the long-term oxidation rate was parabolic and did not depend on the water vapor content in the gas phase. The oxidation kinetics was well described by considering that the rate limiting step was the outwards diffusion of interstitial chromium cations in the oxide layer.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: High-Temperature Coating Behaviors · Catalytic Processes in Materials Science · nanoparticles nucleation surface interactions
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (31)
Show source-provided references
1. The development and application of a unified corrosion model for high-temperature gas-cooled reactor systems10.13182/NT84-A33443 ↗
2. High-temperature corrosion of the nickel-based alloy inconel-617 in helium containing small amounts of impurities10.1016/0025-5416(87)90374-0 ↗
3. Corrosion behavior of high-temperature alloys in impure helium environments10.1016/0022-3115(86)90237-0 ↗
4. thermodynamic and kinetic aspects of the corrosion of high-temperature alloys in high-temperature gas-cooled reactor helium10.13182/NT84-A33441 ↗
5. Corrosion of high-temperature alloys in the primary circuit helium of high-temperature gas-cooled reactors.1. theoretical background10.1002/maco.19850360402 ↗
6. Corrosion of high-temperature alloys in the primary circuit helium of high-temperature gas-cooled reactors.2. experimental results10.1002/maco.19850360802 ↗
7. High temperature reactivity of two chromium-containing alloys in impure helium10.1016/j.jnucmat.2007.11.006 ↗
8. Oxidation of a chromia-forming nickel base alloy at high temperature in mixed diluted CO/H2O atmospheres10.1016/j.corsci.2009.01.019 ↗
9. Oxide-layer formation and stability on a nickel-base alloy in impure helium at high temperature10.1007/s11085-007-9065-y ↗
10. High temperature corrosion of a nickel base alloy by helium impurities10.1016/j.jnucmat.2007.01.049 ↗
11. Thermodynamic modelling of the destruction of the surface Cr(2)O(3) on Alloy 230 in the impure helium atmosphere of a gas cooled reactor
12. Parameters governing the reduction of oxide layers on Inconel 617 in impure VHTR He atmosphere10.1002/maco.200804141 ↗
13. Influence of Al on the High Temperature corrosion behaviour of Inconel 617 in VHTR primary coolant atmosphere
14. Comparison of the high temperature surface reactivity in impure helium of two materials for gas cooled reactors10.4028/www.scientific.net/MSF.595-598.439 ↗
15. High-temperature oxidation of alloy 617 in helium containing part-per-million levels of CO and CO(2) as impurities10.1007/s11661-011-0603-5 ↗
16. Chromia-assisted decarburization of w-rich Ni-based alloys in impure helium at 1273 K (1000 degrees C)10.1007/s11661-010-0503-0 ↗
17. High temperature aging and corrosion study on alloy 617 and alloy 23010.1115/1.4002819 ↗
18. Assessing the kinetics of high temperature oxidation of Inconel 617 in impure helium by coupling TGA and GPC analysis
19. Intergranular oxidation and internal void formation in Ni-40% Cr alloys10.1016/0010-938X(81)90010-X ↗
20. Langmuir · J. Am. Chem. Soc. · 1918 · 40 · 136110.1021/ja02242a004 ↗
21. A comparison of the initial reaction of pure Fe, Cr and Al In (H216o/H218o/O2)-O-16-O-18 gas-mixtures at 300–730 K studied in-situ with sims10.1016/0010-938X(94)90195-3 ↗
22. B. Delmon, Introduction à la cinétique hétérogène, Paris, 1969.
23. Gas phase analysis of CO interactions with solid surfaces at high temperatures10.1016/j.apsusc.2004.04.001 ↗
24. Thermal oxidation of titanium by water vapour10.1016/S0167-2738(97)00400-1 ↗
25. Determination of parabolic rate constants from a local analysis of mass-gain curves10.1023/A:1018860909826 ↗
26. General relationship for thermal oxidation of silicon10.1063/1.1713945 ↗
27. Wagner · Zeitschrift Für Physikalische · 1933 · B21 · 2510.1515/zpch-1933-2105 ↗
28. P. Sarrazin, A. Galerie, J. Fouletier, Les mécanismes de la corrosion sèche. Une approche cinétique, Les Ulis, 2000.10.1051/978-2-7598-0243-2 ↗
29. Relations between the concentrations of imperfections in crystalline solids
30. Etude des mécanismes de corrosion de l’inconel 617 dans le circuit des réacteurs à haute température refroidis par l’hélium
31. Electrical conductivity of Cr2O3 doped with TiO210.1016/S0167-2738(98)00244-6 ↗