Suppression of hydrogen-induced damage in friction stir welded low carbon steel joints
Source abstract
Abstract
Abstract Hydrogen-induced damage including blister and cracking in friction stir welded low carbon steel were evaluated by the cathodic hydrogen charging method. After hydrogen charging for 2 h, irreversible dome-shaped blisters and internal cracking began to appear on the surface of the base metal. However, after hydrogen charging for 16 h, cracking formed along the thermo-mechanically affected zone boundary, while the blisters or cracking were hardly observed in the stir zone. In addition, the stir zone showed a plasticity reduction from 38% to 28%, much less than that of the base metal reduced from 48% to 2%.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Advanced Welding Techniques Analysis · Corrosion Behavior and Inhibition
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (34)
Show source-provided references
1. Hydrogen embrittlement of welded joints for the heat-treatable XABO 960 steel heavy plates
2. Mechanism of hydrogen enhanced cracking of high-strength steel welded joints
3. Hydrogen diffusion and hydrogen influenced critical stress intensity in an API X70 pipeline steel welded joint-experiments and FE simulations10.1016/j.ijhydene.2012.05.005 ↗
4. A new understanding of intergranular stress corrosion cracking resistance of pipeline steel through grain boundary character and crystallographic texture studies10.1016/j.corsci.2008.10.006 ↗
5. Role of copper and aluminum additions on the hydrogen embrittlement susceptibility of austenitic Fe–Mn–C TWIP steels10.1016/j.corsci.2014.01.022 ↗
6. Effect of low temperature on hydrogen-assisted crack propagation in 304L/308L austenitic stainless steel fusion welds10.1016/j.corsci.2013.08.004 ↗
7. Hydrogen embrittlement assessment of ultra-high strength steel 30CrMnSiNi10.1016/j.corsci.2013.08.013 ↗
8. Hydrogen embrittlement of ferritic steels: observations on deformation microstructure, nanoscale dimples and failure by nanovoiding10.1016/j.actamat.2012.06.014 ↗
9. The role of hydrogen in hydrogen embrittlement fracture of lath martensitic steel10.1016/j.actamat.2012.06.040 ↗
10. W.M. Thomas, E.D. Nicholas, J.C. Needham, International Patent Application No. PCT/GB92/02203, 1991.
11. Friction stir welding and processing10.1016/j.mser.2005.07.001 ↗
12. Recent advances in friction stir welding – process, weldment structure and properties10.1016/j.pmatsci.2008.05.001 ↗
13. Investigation of the welding parameter dependent microstructure and mechanical properties in friction stir welded pure copper10.1016/j.msea.2010.07.030 ↗
14. Investigation of welding parameter dependent microstructure and mechanical properties in friction stir welded pure Ti joints10.1016/j.msea.2010.02.023 ↗
15. Evaluation of microstructure and properties in friction stir welded superaustenitic stainless steel10.1179/136217108X386518 ↗
16. Friction stir welding of carbon steel10.1016/j.msea.2006.04.118 ↗
17. Friction stir welding of a high carbon steel10.1016/j.scriptamat.2006.12.004 ↗
18. Three-dimensional visualization of materials flow during friction stir welding by two pairs of X-ray transmission system10.1016/j.scriptamat.2011.09.021 ↗
19. Suppression of hydrogen-induced blisters in SK4 carbon steel alloy by friction stir processing10.1007/s10853-013-7246-4 ↗
20. Hydrogen-induced intergranular failure of iron10.1016/j.actamat.2014.01.060 ↗
21. Effect of ferrite grain size on tensile behavior of a hydrogenated low alloy steel10.2355/isijinternational.39.371 ↗
22. Hydrogen embrittlement of ferritic steels: observations on deformation microstructure, nanoscale dimples and failure by nanovoiding10.1016/j.actamat.2012.06.014 ↗
23. Hydrogen-assisted failure in a twinning-induced plasticity steel studied under in situ hydrogen charging by electron channeling contrast imaging10.1016/j.actamat.2013.04.030 ↗
24. Hydrogen-induced cracking of low carbon-low alloy steel weldments
25. Hydrogen trapping in ferritic steel weld metal10.1179/095066002225006548 ↗
26. Lai · 2012
27. Effect of hydrogen on stability of micro cracks in iron and steel10.1016/0001-6160(60)90103-6 ↗
28. Hydrogen-assisted crack propagation in 304L/308L and 21Cr–6Ni–9Mn/308L austenitic stainless steel fusion welds10.1016/j.corsci.2012.03.046 ↗
29. Computational model for carbon diffusion and methane formation in a ferritic steel during hydrogen attack10.1016/S1359-6462(02)00008-8 ↗
30. Role of crystallographic texture in hydrogen-induced cracking of low carbon steels for sour service piping10.1007/s11661-007-9130-9 ↗
31. Effect of atomic scale plasticity on hydrogen diffusion in iron: quantum mechanically informed and on-the-fly kinetic Monte Carlo simulations10.1557/JMR.2008.0340 ↗
32. Interaction of hydrogen with external stress fields10.1016/0001-6160(86)90229-4 ↗
33. Role of grain boundary solutes and structure on yielding and intergranular cracking of iron10.1007/BF02668006 ↗
34. Hydrogen assisted ductile fracture of spheroidized carbon-steels10.1007/BF02655195 ↗