Corrosion behaviour of several aluminium alloys in contact with a thermal storage phase change material based on Glauber’s salt
Source abstract
Abstract
Abstract This article presents the results of a study about the corrosion behaviour of four aluminium alloys (EN AW 2024, 3003, 6063, and 1050) in contact with a commercial thermal storage material based in the Glauber’s salt (Na 2 SO 4 ·10 H 2 O). Results indicate that the Al 2024 alloy is not compatible with this material due to the extense formation of NaAlCO 3 ·(OH) 2 in contact with air. The aluminium alloys 3003, 6063 and 1050 showed to be fully compatible with the material.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Phase Change Materials Research · Thermodynamic and Structural Properties of Metals and Alloys · Thermal Expansion and Ionic Conductivity
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (17)
Show source-provided references
1. Low temperature latent heat thermal energy storage materials: heat storage materials10.1016/0038-092X(83)90186-X ↗
2. Salt hydrates used for latent heat storage: corrosion of metals and reliability of thermal performance10.1016/0038-092X(88)90136-3 ↗
3. Corrosion of steels in contact with salt eutectics as latent heat storage materials: influence of water and other impurities10.1016/0890-4332(90)90207-Z ↗
4. Immersion corrosion tests on metal–salt hydrate pairs used for latent heat storage in the 32 to 36 Deg temperature range10.1002/1521-4176(200102)52:2<140::AID-MACO140>3.0.CO;2-R ↗
5. Middle term immersion corrosion tests on metal–salt hydrate pairs used for latent heat storage in the 32 to 36 Deg temperature range10.1002/1521-4176(200110)52:10<748::AID-MACO748>3.0.CO;2-S ↗
6. Immersion corrosion tests on metal–salt hydrate pairs used for latent heat storage in the 48 to 58 DegC temperature range10.1002/maco.200290004 ↗
7. Performance of heat charge/discharge of magnesium nitrate hexahydrate and magnesium chloride hexahydrate mixture to a single vertical tube for a latent heat storage system10.1016/j.applthermaleng.2003.09.002 ↗
8. Long term immersion corrosion tests on metal–PCM pairs used for latent heat storage in the 24 to 29 DegC temperature range10.1002/maco.200403806 ↗
9. Corrosive effects of salt hydrate phase change materials used with aluminium and copper10.1016/j.jmatprotec.2005.04.058 ↗
10. The role of precipitates enriched with copper on the susceptibility to pitting corrosion of the 2024 aluminium alloy10.1016/S0010-938X(97)86099-4 ↗
11. J. Moran, Effects of metallurgical variables on the corrosion of aluminum alloys in: ASM Handbook, vol. 13A, Corrosion: Fundamentals, Testing, and Protection, ASM International, 2003, pp. 275–278.10.31399/asm.hb.v13a.a0003618 ↗
12. Corrosion behaviour of aluminium in copper containing environment10.1016/j.corsci.2007.06.002 ↗
13. J.G. Kaufman, Corrosion of aluminum and aluminum alloys, in: ASM Handbook, vol. 13B, Corrosion: Materials, ASM International, 2005, pp. 95–124.10.31399/asm.hb.v13b.a0003815 ↗
14. G.S. Frankel, Pitting corrosion, in: ASM Handbook, vol. 13A, Corrosion: Fundamentals, Testing, and Protection, ASM International, 2003, pp. 236–241.10.31399/asm.hb.v13a.a0003612 ↗
15. Pitting corrosion of aluminum10.1016/S0010-938X(99)00012-8 ↗
16. Hydrothermal synthesis and thermodynamic analysis of dawsonite-type compounds10.1016/j.jssc.2003.09.019 ↗
17. The influence of CO2, AlCl3·6H2O, MgCl2·6H2O, Na2SO4 and NaCl on the atmospheric corrosion of aluminum10.1016/j.corsci.2005.05.027 ↗