journal article·2017-04

Effect of pre-deformation on the oxidation resistance of a high Si ferritic/martensitic steel in oxygen-saturated stagnant lead-bismuth eutectic at 550 °C

Hong Dong, Pei Wang, Dianzhong Li, Yiyi Li

Corrosion Science· Volume 118
Publisher page

Abstract

Abstract The oxidation resistance of a high Si ferritic/martensitic steel with and without pre-deformation in oxygen-saturated stagnant lead-bismuth eutectic at 550 °C has been investigated. It is found that pre-deformation changes the morphology of the oxide scale locally. In some positions, the internal oxidation zone beneath the inner oxide layer disappears and/or the thickness of the inner oxide layer decreases. These changes are related to the formation of an enhanced Cr-rich belt locally in the inner oxide layer. Additionally, the local enhanced Cr-rich belt induces many voids at the inner/outer oxide layer interface, which deteriorates the oxidation resistance of the material.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Nuclear Materials and Properties · Nuclear reactor physics and engineering · Fusion materials and technologies

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (58)

Show source-provided references
1. OECD/NEA Nuclear Science Committee · 2007
2. Review of the studies on fundamental issues in LBE corrosion10.1016/j.jnucmat.2007.06.019 ↗
3. A review of steel corrosion by liquid lead and lead-bismuth10.1016/j.corsci.2009.03.013 ↗
4. Mechanisms of liquid metal corrosion
5. Temperature effect in the maximum propagation rate of a liquid metal filled crack: the T91 martensitic steel/Lead–Bismuth Eutectic system10.1016/j.corsci.2009.06.049 ↗
6. Influence of LBE long term exposure and simultaneous fast neutron irradiation on the mechanical properties of T91 and 316L10.1016/j.jnucmat.2016.02.008 ↗
7. Bending tests on T91 steel in Pb?Bi eutectic, Bi and Pb-Li eutectic10.1016/j.jnucmat.2004.07.027 ↗
8. Low cycle fatigue behavior of a modified 9Cr-1Mo ferritic-martensitic steel in lead-bismuth eutectic at 350 °C—Effects of oxygen concentration in the liquid metal and strain rate10.1016/j.corsci.2015.02.022 ↗
9. Multiscale investigation of quasi-brittle fracture characteristics in a 9Cr-1Mo ferritic-martensitic steel embrittled by liquid lead-bismuth under low cycle fatigue10.1016/j.corsci.2015.10.003 ↗
10. Liquid metal embrittlement of the T91 steel in lead bismuth eutectic: the role of loading rate and of the oxygen content in the liquid metal10.1016/j.msea.2014.04.082 ↗
11. Corrosion behaviour of stainless steels in flowing LBE at low and high oxygen concentration10.1016/j.jnucmat.2004.07.011 ↗
12. Oxidation and dissolution of iron in flowing lead-bismuth eutectic at 450°C10.1016/j.corsci.2012.04.022 ↗
13. Comparison of swelling and irradiation creep behavior of fcc-austenitic and bcc-ferritic/martensitic alloys at high neutron exposure10.1016/S0022-3115(99)00225-1 ↗
14. Nickel solubility limit in liquid lead–bismuth eutectic10.1016/j.jnucmat.2010.03.008 ↗
15. Changes in the phase composition of an oxide film on EP-823 steel in contact with stagnant lead melt10.1007/s11003-005-0054-5 ↗
16. Experimental studies on the corrosion of Fe-Si Fe-Cr, and Fe-Cr-Si alloys in Pb-Bi eutectic
17. Effects of chromium and silicon on corrosion of iron alloys in lead-bismuth eutectic
18. Corrosion behavior of steels in flowing lead–bismuth10.1016/S0022-3115(01)00521-9 ↗
19. On the mechanism of sulphide scale formation on iron10.1016/S0010-938X(65)80018-X ↗
20. A model for mild steel oxidation in CO210.1007/BF00610578 ↗
21. Active control of oxygen in molten lead–bismuth eutectic systems to prevent steel corrosion and coolant contamination10.1016/S0022-3115(01)00713-9 ↗
22. Oxidation mechanism of steels in liquid-lead alloys10.1007/s11085-005-4392-3 ↗
23. Oxidation mechanism of an Fe-9Cr-1Mo steel by liquid Pb-Bi eutectic alloy at 470°C (Part II)10.1016/j.corsci.2008.06.051 ↗
24. Oxidation mechanism of a Fe-9Cr-1Mo steel by liquid Pb-Bi eutectic alloy (Part III)10.1016/j.corsci.2008.06.049 ↗
25. Oxidation mechanism of T91 steel in liquid lead-bismuth eutectic: with consideration of internal oxidation10.1038/srep35268 ↗
26. Corrosion resistance of Si-and Al-rich steels in flowing lead-bismuth10.1016/j.jnucmat.2006.05.019 ↗
27. Effect of silicon on the oxidation resistance of 9 wt.% Cr heat resistance steels in 550°C lead-bismuth eutectic10.1016/j.corsci.2016.04.020 ↗
28. Liquid metal corrosion of T91 and A316L materials in Pb-Bi eutectic at temperatures 400–600°C10.1016/j.corsci.2005.04.001 ↗
29. Influence of temperature on the interaction mode of T91 and AISI 316L steels with Pb-Bi melt saturated by oxygen10.1016/j.corsci.2008.02.006 ↗
30. Effect of cold-work on the radiation-induced deformation of austenitic stainless steels10.1016/j.jnucmat.2007.03.063 ↗
31. Residual strain measurement and grain boundary characterization in the heat-affected zone of a weld joint between Alloy 690TT and Alloy 5210.1016/j.jnucmat.2009.12.016 ↗
32. Effect of prior machining deformation on the development of tensile residual stresses in weld-fabricated nuclear components10.1007/BF02647269 ↗
33. Texture, residual strain, and plastic deformation around scratches in alloy 600 using synchrotron X-ray Laue micro-diffraction10.1016/j.jnucmat.2007.10.015 ↗
34. Effects of scratching on corrosion and stress corrosion cracking of Alloy 690TT at 58°C and 330°C10.1016/j.corsci.2009.07.015 ↗
35. Effects of pre-formed nanostructured surface layer on oxidation behaviour of 9Cr2WVTa steel in air and liquid Pb-Bi eutectic alloy10.1016/j.corsci.2015.10.021 ↗
36. Effect of cold rolling on the oxidation resistance of T91 steel in oxygen-saturated stagnant liquid lead-bismuth eutectic at 450°C and 550°C10.1016/j.jnucmat.2016.04.046 ↗
37. Corrosion scales on various steels after exposure to liquid lead-bismuth eutectic10.1016/j.jnucmat.2013.09.034 ↗
38. Oxidation of steel T91 in flowing lead-bismuth eutectic (LBE) at 550°C10.1016/j.jnucmat.2006.05.009 ↗
39. Oxidation behavior of ferritic-martensitic and ODS steels in supercritical water10.1016/j.jnucmat.2012.03.009 ↗
40. Corrosion behavior of a ferritic/martensitic steel HCM12A exposed to harsh environments10.1016/j.jnucmat.2007.05.001 ↗
41. Oxidation mechanism of a Fe-9Cr-1Mo steel by liquid Pb-Bi eutectic alloy (Part I)10.1016/j.corsci.2008.06.050 ↗
42. Effect of Al and Si on mechanical properties and corrosion resistance in liquid Pb-Bi eutectic of 9Cr2WVTa steel
43. Corrosion behavior of Si-enriched steels for nuclear applications in liquid lead-bismuth10.1016/j.jnucmat.2013.02.022 ↗
44. EFTEM and EELS analysis of the oxide layer formed on HCM12A exposed to SCW10.1016/j.jnucmat.2012.06.017 ↗
45. Oxidation behavior of iron-based alloy HCM12A exposed in supercritical water10.1016/j.corsci.2005.10.010 ↗
46. TEM/HREM observations of nanostructured superplastic Ni3AI10.1080/01418610108216615 ↗
47. Grain boundary structure in Al-Mg and Al-Mg-Sc alloys after equal-channel angular pressing10.1557/JMR.2001.0084 ↗
48. An investigation of grain boundaries in submicrometer-grained Al-Mg solid solution alloys using high-resolution electron microscopy10.1557/JMR.1996.0239 ↗
49. Effects of cold working degrees on grain boundary characters and strain concentration at grain boundaries in Alloy 60010.1016/j.corsci.2010.11.022 ↗
50. Effect of single-step strain and annealing on grain boundary character distribution and intergranular corrosion in Alloy 69010.1007/s10853-007-2164-y ↗
51. Diffusion along grain boundaries with non-equilibrium structure10.1002/pssa.2211390206 ↗
52. Diffusion of chromium in nanocrystalline iron produced by means of surface mechanical attrition treatment10.1016/S1359-6454(03)00260-X ↗
53. Subsurface depletion and enrichment processes during oxidation of a high chromium, Laves-phase strengthened ferritic steel10.1149/1.3590258 ↗
54. Factors affecting chromium carbide precipitate dissolution during alloy oxidation10.1023/A:1018880019395 ↗
55. Alloy phase transformations driven by high temperature corrosion processes10.1016/S0010-938X(01)00065-8 ↗
56. Dislocation engineering and its effect on the oxidation behaviour10.3184/096034012X13322687148749 ↗
57. M23C6 precipitates induced inhomogeneous distribution of silicon in the oxide formed on a high-silicon ferritic/martensitic steel10.1016/j.scriptamat.2014.10.028 ↗
58. Anomalous temperature dependence of oxidation kinetics during steam oxidation of ferritic steels in the temperature range 550–650°C10.1016/j.corsci.2004.01.010 ↗