Durability of platinum coating anode in molten carbonate electrolysis cell
Source abstract
Abstract
Abstract The performance and durability of a noble metal coating anode for oxygen evolution was investigated in molten Li2CO3-Na2CO3-K2CO3 at 450 °C for the first time. The consuming rate of Pt was evaluated to be below 4.1 × 10−2 mm/a under anodic polarization by weight-loss and melt analysis measurements. The metallic substrate, titanium can be anodically passivated by forming a dense Li2TiO3 film in the melt. Platinum coated titanium (Pt/Ti) anode exhibited excellent durability within 100h electrolysis, but slight oxygen penetration under the coating was observed, which might lead to the failure of the material for much longer term application.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Molten salt chemistry and electrochemical processes · Advanced Battery Materials and Technologies · Advancements in Battery Materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (29)
Show source-provided references
1. Capture and electrochemical conversion of CO2 to value-added carbon and oxygen by molten salt electrolysis10.1039/c3ee24132g ↗
2. Abundance and isotopic composition of gases in the martian atmosphere from the curiosity rover10.1126/science.1237966 ↗
3. Effect of BaCO3 addition on the CO2-derived carbon deposition in molten carbonates electrolyzer10.1039/C7NJ03546B ↗
4. High-temperature oxidation behavior of Ni-11Fe-10Cu alloy: growth of a protective oxide scale10.1016/j.corsci.2016.07.010 ↗
5. Rearrangement of oxide scale on Ni-11Fe-10Cu alloy under anodic polarization in molten Na2CO3-K2CO310.1016/j.corsci.2018.07.014 ↗
6. Electrochemical impedance studies of the initial-stage corrosion of 310S stainless steel beneath thin film of molten (0.62Li,0.38K)2CO3 at 650 °C10.1016/j.corsci.2010.11.036 ↗
7. Corrosion behaviour of austenitic stainless steels in carbonate melt at 923 K under controlled CO2 – O2 environment10.1016/j.corsci.2018.01.031 ↗
8. Inert anodes for the Hall-Heroult cell: the ultimate materials challenge10.1007/s11837-001-0206-5 ↗
9. Layer growth mechanisms on metallic electrodes under anodic polarization in cryolite-alumina melt10.1016/j.corsci.2013.10.040 ↗
10. Electrochemical growth of a corrosion-resistant multi-layer scale to enable an oxygen-evolution inert anode in molten carbonate10.1016/j.electacta.2018.05.095 ↗
11. Nickel-iron-copper alloy as inert anode for ternary moltencarbonate electrolysis at 650 °C10.1149/2.1211811jes ↗
12. Unusual temperature effect on the stability of nickel anodes in molten carbonates10.1016/j.electacta.2017.05.149 ↗
13. Oxygen overpotential in molten carbonates10.1149/1.2427778 ↗
14. Preparation of carbon and oxygen by carbon dioxide electrolysis in LiF-Li2CO3 eutectic molten salt10.1149/2.0601602jes ↗
15. Corrosion testing of platinum metals CVD coated titanium anodes in seawater-simulated solutions10.1016/S0011-9164(01)00190-4 ↗
16. Studies on the durability of platinum and ruthenium oxide coated titanium anodes in the d -ribono-γ-lactone electro-reduction process10.1016/0010-938X(81)90070-6 ↗
17. Electrochemical formation of carbon nano-powders with various porosities in molten alkali carbonates10.1016/j.electacta.2009.03.049 ↗
18. Potentiostatic polarization studies in fused carbonates—I. The noble metals, silver and nickel10.1016/0013-4686(64)87003-1 ↗
19. A. Association · 1998
20. Production of oxygen gas and liquid metal by electrochemical decomposition of molten iron oxide10.1149/1.3560477 ↗
21. The galvanic corrosion behavior of coupled nickel-platinum in molten Na2CO310.1016/S0010-938X(96)00043-1 ↗
22. Degradation mechanism of long service life Ti/IrO–TaO oxide anodes in sulphuric acid10.1016/S0010-938X(01)00165-2 ↗
23. Determination of diffusion in polycrystalline platinum thin films10.1063/1.371458 ↗
24. Structure and Raman spectra of titanium oxides
25. Quantitative analysis of the content of rutile TiO2 by Raman spectrum
26. Diffusivity and solubility of oxygen in platinum and Pt-Ni alloys10.1007/BF02680586 ↗
27. Electrical conductivity of plasma-sprayed titanium oxide (rutile) coatings10.1016/0040-6090(91)90149-R ↗
28. The contribution of grain boundary barriers to the electrical conductivity of titanium oxide thin films10.1063/1.2970034 ↗
29. Solute diffusion of platinum in rutile titanium dioxide10.1111/jace.12130 ↗