Synthesis and high temperature corrosion behaviour of nearly monolithic Ti3AlC2 MAX phase in molten chloride salt
Source abstract
Abstract
Nearly monolithic MAX phase containing 95 wt.% Ti3AlC2 and 5 wt.% TiCx was synthesized by spark plasma sintering under vacuum sintering conditions. Corrosion behaviour of Ti3AlC2 was investigated in molten LiCl–KCl salt at 600 °C under a dry Ar atmosphere. Evolution of microstructure and surface chemistry of the exposed sample was characterized by scanning electron microscopy (SEM), X-ray diffraction (XRD) and glancing angle X-ray diffraction (GAXRD). Results showed that Al dissolution led to delamination of the layered structure which favoured the ingress of chlorine and its subsequent intercalation into the Al–site plane to form a Ti3C2Cl2 exfoliation layer. De-twinning of the Ti3C2 layers possibly due to Cl- anions substitution by O results in non-stoichiometric TiC0.67 formation.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: MXene and MAX Phase Materials · Aluminum Alloys Composites Properties · Advanced ceramic materials synthesis
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (53)
Show source-provided references
1. Flanagan · 2012
2. Holcomb · 2013
3. Corrosion of structural alloys in high-temperature molten fluoride salts for applications in molten salt reactors10.1007/s11837-018-2981-2 ↗
4. Molten fluorides for nuclear applications10.1016/S1369-7021(10)70222-4 ↗
5. Materials corrosion in molten LiF–NaF–KF salt10.1016/j.jfluchem.2008.05.008 ↗
6. Busby · 2019
7. The high-temperature corrosion of Hastelloy N alloy (UNS N10003) in molten fluoride salts analysed by STXM, XAS, XRD, SEM, EPMA, TEM/EDS10.1016/j.corsci.2016.02.010 ↗
8. Ren · 2011
9. Koger · 1972
10. Corrosion behavior of Hastelloy-N alloys in molten salt fluoride in Ar gas or in air10.1080/00223131.2015.1043155 ↗
11. Wright · 2018
12. MAX phase carbides and nitrides: properties for future nuclear power plant in-core applications and neutron transmutation analysis10.1016/j.nucengdes.2011.12.009 ↗
13. Investigations on radiation tolerance of Mn+1AXn phases: study of Ti3SiC2, Ti3AlC2, Cr2AlC, Cr2GeC, Ti2AlC, and Ti2AlN10.1111/jace.13450 ↗
14. Irradiation resistance of MAX phases Ti3SiC2 and Ti3AlC2: characterization and comparison10.1016/j.jnucmat.2015.06.056 ↗
15. Barsoum · 2013
16. Progress in research and development on MAX phases: a family of layered ternary compounds10.1179/1743280410Y.0000000001 ↗
17. Barsoum · 2011 · 195
18. The MAX Phases: unique New Carbide and Nitride Materials: ternary ceramics turn out to be surprisingly soft and machinable, yet also heat-tolerant, strong and lightweight10.1511/2001.28.334 ↗
19. The stability of irradiation-induced defects in Zr3AlC2, Nb4AlC3 and (Zr0.5,Ti0.5)3AlC2 MAX phase-based ceramics10.1016/j.actamat.2019.10.049 ↗
20. Effect of neutron irradiation on select MAX phases10.1016/j.actamat.2014.10.068 ↗
21. Tallman · 2015
22. Synthesis of Ti3SiC2 powders: reaction mechanism10.1111/j.1551-2916.2007.01501.x ↗
23. Chemical bonding and electronic-structure in MAX phases as viewed by X-ray spectroscopy and density functional theory10.1016/j.tsf.2016.11.005 ↗
24. High-temperature oxidation behavior of Ti2AlC in air10.1023/A:1023092027697 ↗
25. Tribological behavior of select MAX phases against Al2O3 at elevated temperatures10.1016/j.wear.2007.11.018 ↗
26. Corrosion behavior of Ti3AlC2 in molten KOH at 700 °C10.1007/s40145-013-0077-6 ↗
27. Corrosion behavior of Ti3AlC2 in NaOH and H2SO410.1016/j.jeurceramsoc.2010.07.002 ↗
28. Comparison of corrosion behavior of Ti3SiC2 and Ti3AlC2 in NaCl solutions with Ti10.1016/j.ceramint.2017.01.111 ↗
29. Corrosion behaviour of Ti3SiC2 and Ti3AlC2 with LiF-NaF-KF molten salt
30. On the topotactic transformation of Ti2AlC into a Ti–C–O–F cubic phase by heating in molten Lithium fluoride in air10.1111/j.1551-2916.2011.04896.x ↗
31. Cooper · 2019
32. Jantzen · 2019
33. Crystallographic relations between Ti3SiC2 and TiC10.1007/PL00010876 ↗
34. Microstructural characterization of bulk Ti3AlC2 ceramics10.1080/14786430410001716197 ↗
35. Influence of sintering environment on the spark plasma sintering of Maxthal 312 (nominally-Ti3SiC2) and the role of powder particle size on densification10.1016/j.jallcom.2019.06.076 ↗
36. The lubricating properties of spark plasma sintered (SPS) Ti3SiC2 MAX phase compound and composite
37. Element replacement approach by reaction with lewis acidic molten salts to synthesize nanolaminated MAX phases and MXenes10.1021/jacs.9b00574 ↗
38. Ti3C2 MXene: a promising microwave absorbing material10.1039/C7RA12616F ↗
39. On the topotactic transformation of Ti2AlC into a Ti-C-O-F cubic phase by heating in molten Lithium fluoride in air10.1111/j.1551-2916.2011.04896.x ↗
40. Synthesis of carbide-derived carbon by chlorination of Ti2AlC10.1021/cm047739i ↗
41. Micro and mesoporosity of carbon derived from ternary and binary metal carbides10.1016/j.micromeso.2007.10.033 ↗
42. Two-dimensional nanocrystals produced by exfoliation of Ti3AlC210.1002/adma.201102306 ↗
43. Synthesis of two-dimensional titanium nitride Ti4N3 (MXene)10.1039/C6NR02253G ↗
44. 25th anniversary article: MXenes: a new family of two-dimensional materials10.1002/adma.201304138 ↗
45. The topotactic transformation of Ti3SiC2 into a partially ordered cubic Ti(C0.67Si0.06) phase by the diffusion of Si into molten cryolite10.1149/1.1392573 ↗
46. Thermal stability of Ti3SiC2 thin films10.1016/j.actamat.2006.10.010 ↗
47. A general Lewis acidic etching route for preparing MXenes with enhanced electrochemical performance in non-aqueous electrolyte10.1038/s41563-020-0657-0 ↗
48. Synthesis and formation mechanism of high-purity Ti3AlC2 powders by microwave sintering10.1111/ijac.13452 ↗
49. Anisotropic corrosion of Ti2AlC and Ti3AlC2 in supercritical water at 500ºC10.1016/j.ceramint.2017.02.153 ↗
50. High-temperature oxidation behavior of Ti3AlC2 in air10.1016/S1003-6326(06)60318-X ↗
51. Hot corrosion and protection of Ti2AlC against Na2SO4 salt in air10.1016/j.jeurceramsoc.2005.12.004 ↗
52. Internal oxidation of Fe–Al alloys in a KCl-Air atmosphere at 650°C10.1023/B:OXID.0000025337.64394.bf ↗
53. Tin+1Cn MXenes with fully saturated and thermally stable Cl terminations10.1039/C9NA00324J ↗