Computational simulation and efficient evaluation on corrosion inhibitors for electrochemical etching on aluminum foil
Source abstract
Abstract
Abstract The tunnel density and capacitance of etched aluminum foils would be significantly decreased for excessive dissolution during electrochemical etching process. The addition of low-concentration corrosion inhibitor solutions effectively improved the tunnel distribution. Various organic molecules as 8HQ, BTA, MBT, Citric Acid and Oleic Acid were analyzed using DFT and MD simulations and etching solutions with corrosion inhibitors at concentration of 0.10 mmol L −1 were designed. Relationship of physicochemical parameter and experimental tunnel density was established. The results indicate that Oleic Acid presents excellent corrosion inhibiting performance on the improvement of tunnel density as ρ = 1.5925 × 10 7 cm −2 and predicted capacitance as C = 0.72 μF cm −2 at 520 V.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Corrosion Behavior and Inhibition · Anodic Oxide Films and Nanostructures · Concrete Corrosion and Durability
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (48)
Show source-provided references
1. Modelling specific capacitance of D.C. Etched aluminium foil for aluminium electrolytic capacitor
2. Anodizing of etched aluminum foil coated with modified hydrous oxide film for aluminum electrolytic capacitor10.1007/s10854-013-1561-z ↗
3. Effect of pretreatment on electrochemical etching behavior of Al foil in HCl–H2SO410.1016/S1003-6326(13)62564-9 ↗
4. Effect of placement of aluminium foil on growth of etch tunnels during DC etching10.1016/j.corsci.2013.10.017 ↗
5. Effects of H2SO4 content on electrochemical activation of etched tunnels on aluminum foil10.5006/2269 ↗
6. Effects of HNO3 concentration on the pit morphologies of aluminum foil etched in HNO3–HCl and HNO3–H2SO4–HCl solutions10.1007/s12613-016-1212-5 ↗
7. Mechanical attrition assisted DC etching aluminum foils with enhanced capacitance10.1007/s10854-016-5356-x ↗
8. Relationship between trace Mn and the pitting behavior of aluminum foil used for high voltage electrolytic capacitors10.1016/S1875-5372(14)60095-3 ↗
9. Effect of tunnel structure on the specific capacitance of etched aluminum foil10.1007/s12613-014-0998-2 ↗
10. Effect of chemical plating Zn on DC-etching behavior of Al foil in HCl–H2SO410.1016/S1003-6326(13)62913-1 ↗
11. Effect of electrodepositing Ag on DC etching aluminum foils for electrolytic capacitor10.1007/s10854-017-6385-9 ↗
12. Effects of polymer corrosion inhibitor on widening etch tunnels of aluminum foil for capacitor10.1016/j.corsci.2013.07.011 ↗
13. Effect of citric acid on microstructure and electrochemical characteristics of high voltage anodized alumina film formed on etched Al Foils10.1016/S1003-6326(11)60689-4 ↗
14. Preparation of Nb2O5-Al2O3 composite anodic oxide film for an aluminum electrolytic capacitor by electrodeposition-annealing and anodization10.1007/s11664-019-07774-7 ↗
15. Formation and properties of Al2O3–ZrO2 composite anodic oxide film on etched aluminum foil by electrodeposition and anodization10.1007/s10854-015-3922-2 ↗
16. Effect of Thiourea on the corrosion behavior of aluminum anode foil of aluminum electrolytic capacitor10.1007/s11665-018-3530-4 ↗
17. Effects of 2-methyl-1, 3-propanediol in boric acid solution on the anodizing behavior and electrical properties of ZrO2 coated Al foil10.1016/j.surfcoat.2016.12.081 ↗
18. Effect of trace tartaric acid on anodizing of etched aluminum foil for high voltage electrolytic capacitor10.1007/s10854-013-1268-1 ↗
19. Improved distribution of etched tunnels on aluminum foil with silane treatment10.1016/j.porgcoat.2018.11.017 ↗
20. Self-assembled layers for the temporary corrosion protection of magnesium-AZ31 alloy10.1016/j.corsci.2020.108619 ↗
21. Density functional theory (DFT) as a powerful tool for designing new organic corrosion inhibitors. Part 1: an overview10.1016/j.corsci.2015.01.037 ↗
22. Electrochemical, surface-analytical, and computational DFT study of alkaline etched aluminum modified by carboxylic acids for corrosion protection and hydrophobicity10.1149/2.0181911jes ↗
23. Evaluation of Thymus vulgaris plant extract as an eco-friendly corrosion inhibitor for stainless steel 304 in acidic solution by means of electrochemical impedance spectroscopy, electrochemical noise analysis and density functional theory10.1016/j.jcis.2016.11.048 ↗
24. The use of quantum chemical methods in corrosion inhibitor studies10.1016/j.corsci.2008.08.043 ↗
25. A conundrum for density functional theory10.1126/science.aal3442 ↗
26. Experimental and theoretical studies on the corrosion inhibition of copper by two indazole derivatives in 3.0% NaCl solution10.1016/j.jcis.2016.03.023 ↗
27. A benchmark for materials simulation10.1126/science.aaf3412 ↗
28. Scanning tunneling microscopy and density functional theory investigations on molecular self-assembly of graphene on Ru(0 0 0 1)10.1016/j.apsusc.2016.01.214 ↗
29. DFT studies of 2-mercaptobenzothiazole and 2-mercaptobenzimidazole as corrosion inhibitors for copper10.1016/j.corsci.2020.108840 ↗
30. Adsorption and thermal stability of 2-mercaptobenzothiazole corrosion inhibitor on metallic and pre-oxidized Cu(1 1 1) model surfaces10.1016/j.apsusc.2019.145132 ↗
31. Relationship between structure and inhibition behaviour of quinolinium salts for mild steel corrosion: experimental and theoretical approach10.1016/j.corsci.2015.02.034 ↗
32. Quantum chemical studies on the some inorganic corrosion inhibitors10.1016/j.corsci.2013.07.023 ↗
33. Highly functionalized epoxy macromolecule as an anti-corrosive material for carbon steel: computational (DFT, MDS), surface (SEM-EDS) and electrochemical (OCP, PDP, EIS) studies10.1016/j.molliq.2020.112535 ↗
34. A new insight into corrosion inhibition mechanism of copper in aerated 3.5 wt.% NaCl solution by eco-friendly Imidazopyrimidine Dye: experimental and theoretical approach10.1016/j.cej.2018.08.079 ↗
35. Synthesis and investigation of pyran derivatives as acidizing corrosion inhibitors for N80 steel in hydrochloric acid: theoretical and experimental approaches10.1016/j.jallcom.2018.05.236 ↗
36. The effect of surface electronic structure on the bioactivity of neutral dopant Si, Ge, and Sn on TiO2 (110): a DFT Study10.1002/pssb.201700185 ↗
37. The roles of mercapto, benzene, and methyl groups in the corrosion inhibition of imidazoles on copper: II. Inhibitor–copper bonding10.1016/j.corsci.2015.05.041 ↗
38. Universal solvation model based on solute Electron density and on a continuum model of the solvent defined by the bulk dielectric constant and atomic surface tensions10.1021/jp810292n ↗
39. Multiwfn: a multifunctional wavefunction analyzer10.1002/jcc.22885 ↗
40. Koopmans · 1934 · 1 · 104
41. Enhanced corrosion resistance of mild steel in normal sulfuric acid medium by 2,5-bis(n-thienyl)-1,3,4-thiadiazoles: electrochemical, X-ray photoelectron spectroscopy and theoretical studies10.1016/j.apsusc.2007.05.062 ↗
42. On the consistent use of electrophilicity index and HSAB-based electron transfer and its associated change of energy parameters10.1016/j.cplett.2011.03.045 ↗
43. Inhibitory mechanism of mimosa tannin using molecular modeling and substitutional adsorption isotherms10.1016/S0254-0584(01)00569-7 ↗
44. Benzotriazole as an inhibitor of brass corrosion in chloride solution10.1016/j.apsusc.2007.04.083 ↗
45. The enhancement of benzotriazole on epoxy functionalized silica sol–gel coating for copper protection10.1016/j.apsusc.2013.03.083 ↗
46. Analysis of molecular electronic structure of imidazole- and benzimidazole-based inhibitors: a simple recipe for qualitative estimation of chemical hardness10.1016/j.corsci.2010.11.016 ↗
47. The Royal Society of Chemistry · 2007
48. Formation and effect of the branched layer during the tunnel etching of aluminum foil10.1007/s10853-019-03979-7 ↗