Metal dusting behaviour of Cr–Ni steels and Ni-base alloys in a simulated syngas mixture
Source abstract
Abstract
Abstract Long-term laboratory exposure tests for various Cr and Ni content steels and Ni-base alloys were conducted at 650 °C in a 60vol.%CO–26%H2–11.5%CO2–2.5%H2O gas mixture simulating syngas environments. Upon isothermal heating, alloys with 15% and 20% Cr had many pits on the surface after a brief exposure, while no pit was found on alloys containing of 60% Ni and more than 23% Cr exposed for up to 5000 h. The thermal cycling accelerated pit initiation drastically, resulting that all test specimens except 30%Cr–60%Ni alloy suffered from metal dusting. From a measurement of pit depths, Ni proved to be an effective alloying element to retard the pit growth: growth rate for 75% Ni alloy has achieved double-digit decrease compared to that for 20% Ni. Microscopic observations has revealed that platelet graphite aligned perpendicular at the boundary of gas/metal of pits. The length of the platelet graphite for high Ni alloys was appreciably longer than that for low Ni steels. This can be interpreted from the difference of super saturation of carbon.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Graphite, nuclear technology, radiation studies · Metallurgical Processes and Thermodynamics
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (26)
Show source-provided references
1. Prange · Corrosion · 1959 · 15 · 619t10.5006/0010-9312-15.12.13 ↗
2. Eberle · Corrosion · 1959 · 15 · 622t10.5006/0010-9312-15.12.16 ↗
3. Hoyt · Corrosion · 1959 · 15 · 627t10.5006/0010-9312-15.12.21 ↗
4. H.J. de Bruyn, M.L. Holland, Materials experience in a methane reforming plant, CORROSION/98, paper no. 429, Houston, TX: NACE, 1999.
5. The fundamentals of metal dusting
6. R.F. Hochman, Basic studies of metal dusting deterioration (“metal dusting”) in carbonaceous environments at elevated temperatures, in: Proc. of the 4th International Congress on Metallic Corrosion, NACE, 1972, p. 258.
7. Grabke · Werkst. Korros. · 1993 · 44 · 8910.1002/maco.19930440306 ↗
8. Nava Paz · Oxid. Met. · 1993 · 39 · 43710.1007/BF00664665 ↗
9. Grabke · Corros. Sci. · 1993 · 35 · 114110.1016/0010-938X(93)90334-D ↗
10. Grabke · Mater. Corros. · 1994 · 45 · 21510.1002/maco.19940450402 ↗
11. Grabke · Mater. Corros. · 1996 · 47 · 49510.1002/maco.19960470904 ↗
12. J. Klöwer, H.J. Grabke, E.M. Müller-Lorenz, D.C. Agarwal, Metal dusting and carburization resistance of nickel-base alloys, CORROSION/97, paper no.139, Houston, TX: NACE, 1997.
13. Schneider · Steel Res. · 1997 · 68 · 32610.1002/srin.199701796 ↗
14. Pippel · Mater. Corros. · 1998 · 49 · 30910.1002/(SICI)1521-4176(199805)49:5<309::AID-MACO309>3.0.CO;2-1 ↗
15. Chun · Mater. Corros. · 1999 · 50 · 63410.1002/(SICI)1521-4176(199911)50:11<634::AID-MACO634>3.0.CO;2-F ↗
16. Chun · J. Electrochem. Soc. · 2000 · 147 · 368010.1149/1.1393958 ↗
17. Y. Nishiyama, N. Otsuka, T. Kudo, Mater. Trans., submitted for publication.
18. Szakalos · Corros. Sci. · 2002 · 44 · 225310.1016/S0010-938X(02)00053-7 ↗
19. H.J. de Bruyn, E.H. Edwin, S. Brendryen, Apparent influence of steam on metal dusting, CORROSION/2001, paper no. 1383, Houston, TX: NACE, 2001.
20. Bose · Z. Metallkd. · 1978 · 69 · 8
21. Nishiyama · Corrosion · 2003 · 59 · 68810.5006/1.3277598 ↗
22. Schueler · Hydrocarbon Process. · 1972 · 73
23. Parks · Stainless Steel World · 1997 · 9 · 44
24. B.A. Baker, G.D. Smith, V.W. Hartmann, L.E. Shoemaker, Nickel-base material solutions to metal dusting, CORROSION/2002, paper no. 2394, Houston, TX: NACE, 2002.
25. Toh · Materials at High Temperature · 2003 · 20 · 12910.3184/096034003782748982 ↗
26. Wagner · Z. Electrochem. · 1950 · 63 · 772