Contribution of acoustic emission to the understanding of sulfide stress cracking of low alloy steels

Véronique Smanio, Marion Fregonese, Jean Kittel, Thierry Cassagne, François Ropital, Bernard Normand

Corrosion Science· Volume 53· Issue 12

Abstract

Abstract The acoustic emission technique was applied to standard tests devoted to evaluate sulfide stress cracking susceptibility of steels for oil and gas industry. The mapping of the density of AE signals vs. their location on the specimen gauge length as a function of time allowed early detection of cracking, and gave meaningful information on incubation times and propagation rates. Sulfide stress cracking initiation was correlated with the presence of critical surface defects. A mechanism involving plastic strain and/or metal dissolution was proposed to account for crack propagation.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Material Properties and Failure Mechanisms · Non-Destructive Testing Techniques

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (50)

Show source-provided references
1. NACE MR0175/ISO 15156-1, Petroleum and natural gas industries – materials for use in H2S containing environments in oil and gas production – Part 1: general principles for selection of cracking-resistant materials, International Organization for Standardization, Geneva, Switzerland, 2001.
2. Troiano · Trans. ASM · 1960 · 52 · 54
3. R. Oriani, A decohesion theory for hydrogen-induced crack propagation, in: R. Staehle, J. Hochmann, R. McCright (Eds.), Stress Corrosion Cracking and Hydrogen Embrittlement of Iron Base Alloy, NACE, Houston, 1977, pp 351–360
4. Beachem · Metall. Trans. · 1972 · 3 · 43710.1007/BF02642048 ↗
5. Eastman · Metall. Soc. AIME · 1981 · 397
6. Lynch · Acta Metall. · 1988 · 36 · 263910.1016/0001-6160(88)90113-7 ↗
7. Crolet · La Revue de Métallurgie · 2004 · 101 · 105310.1051/metal:2004111 ↗
8. S.N. Smith, B. Brown, W. Sun, Corrosion at higher H2S concentrations and moderate temperatures, NACE Corrosion/2011 Paper No. 11081, Houston, Texas, USA, 13–17 March, 2011.
9. Morris · J. Electrochem. Soc. · 1980 · 127 · 122810.1149/1.2129861 ↗
10. Smith · Br. Corros. J. · 1975 · 10 · 13610.1179/000705975798320701 ↗
11. Hernandez-Espejel · Corros. Sci. · 2010 · 52 · 225810.1016/j.corsci.2010.04.003 ↗
12. The use of acoustic emission for the study and monitoring of localized corrosion phenomena
13. Yuyama · J. Acoust. Emission · 1983 · 2 · 71
14. Pollock · Br. Corros. J. · 1982 · 17 · 10310.1179/000705982798274381 ↗
15. Gerberich · Mater. Sci. Eng. · 1988 · 103 · 18510.1016/0025-5416(88)90565-4 ↗
16. Ferrer · Wear · 1999 · 231 · 10810.1016/S0043-1648(99)00120-9 ↗
17. Rettig · Corrosion · 1976 · 32 · 12110.5006/0010-9312-32.4.121 ↗
18. Mansfeld · Corrosion · 1979 · 35 · 54110.5006/0010-9312-35.12.541 ↗
19. Arora · Corrosion · 1984 · 40 · 45910.5006/1.3577916 ↗
20. Magaino · J. Electrochem. Soc. · 1987 · 134 · 299310.1149/1.2100328 ↗
21. Jones · Corrosion · 1992 · 48 · 75110.5006/1.3315996 ↗
22. Mazille · Corrosion Science · 1995 · 37 · 136510.1016/0010-938X(95)00036-J ↗
23. Fregonese · J. Mater. Sci. · 2001 · 36 · 55710.1023/A:1004891514836 ↗
24. Fregonese · Corrosion Science · 2001 · 43 · 62710.1016/S0010-938X(00)00099-8 ↗
25. Kim · NDT&E Int. · 2003 · 36 · 55310.1016/S0963-8695(03)00065-3 ↗
26. Kim · Corros. Sci. · 2006 · 48 · 394510.1016/j.corsci.2006.03.006 ↗
27. Jomdecha · NDT&E Int. · 2007 · 40 · 58410.1016/j.ndteint.2007.05.003 ↗
28. Bellanger · NDT&E Int. · 2002 · 35 · 38510.1016/S0963-8695(02)00011-7 ↗
29. Seah · Corros. Sci. · 1993 · 34 · 170710.1016/0010-938X(93)90042-F ↗
30. Jaubert · Insight · 2005 · 47 · 46510.1784/insi.2005.47.8.465 ↗
31. Weng · J. Chin. Inst. Eng. · 1993 · 16 · 19510.1080/02533839.1993.9677491 ↗
32. M.S. Cayard, R.D. Kane, Evaluation of various methods of reducing the duration of SSC qualification testing, NACE Corrosion/97 Paper No. 97057, New-Orleans, Louisiana, USA, 9–14 March, 1997.
33. A.D.B. Gingell, X. Garat, Observations of damage modes as a function of microstructure during NACE TM0177-96 tensile testing of API 5L grade X60 linepipe steels, NACE Corrosion/99 Paper No. 99600, San Antonio, Texas, USA, 25–30 April, 1999.
34. Weng · J. Chin. Inst. Eng. · 1993 · 16 · 48910.1080/02533839.1993.9677521 ↗
35. Tsaiet · J. Electrochem. Soc. · 1998 · 145 · 196810.1149/1.1838584 ↗
36. S. Amami, P. Marchand, S. Duval, X. Longaygue, M. Fregonese, H. Mazille, J.P. Millet, Detection by acoustic emission technique of the corrosion stress cracking within steel structures in H2S containing mediums, EFC Eurocorr/2003, Budapest, Hungary, 28 September–2 October, 2003.
37. NACE TM0284-2003, Evaluation of pipeline and pressure vessel steels for resistance to hydrogen-induced cracking, NACE International, Houston, TX, USA, 2003.
38. NACE TM0177-96, Laboratory testing of metals for resistance to specific forms of environmental cracking in H2S environments, NACE International, Houston, Texas, USA, 1996.
39. Smanio · J. Mater. Sci. · 2010 · 45 · 553410.1007/s10853-010-4613-2 ↗
40. Smanio · Corros. · 2011 · 67 · 65002-110.5006/1.3595097 ↗
41. J. Galland, J. Sojka, M. Jerome, Introduction d’hydrogène dans les aciers. 1ère partie: Rôle de paramètres physicochimique et métallurgiques sur la fragilisation par l’hydrogène, in: B. Normand, N. Pébère, C. Richard, M. Wery (Eds.), Prévention et lutte contre la corrosion : une approche scientifique et technique. Presses Polytechniques et Universitaires Romandes, Lausanne, 2004, pp. 311–319.
42. EFC Publication No. 16, Guidelines on materials requirements for carbon and low alloy steels for H2S-containing environments in Oil and Gas production, The Institute of Materials, London, UK, 1995.
43. Kittel · Corros. Sci. · 2010 · 52 · 138610.1016/j.corsci.2009.11.044 ↗
44. E.P. Cernoky, D.L. Sponseller, T.E. Sponseller, Unconventional applications of NACE method–a tests to investigate and characterize fundamental aspects of low alloy steel in H2S environments, NACE Corrosion/2006 Paper No. 129, San Diego, California, USA, 12–15 March, 2006.
45. D. Le Friant, Ph.D. thesis, Ecole Nationale Supérieure des Mines de Saint Etienne, France, 2000.
46. Dawoud · Corros. Sci. · 1992 · 33 · 29510.1016/0010-938X(92)90153-T ↗
47. Saenz de Santa Maria · Corros. Sci. · 1989 · 29 · 6910.1016/0010-938X(89)90081-4 ↗
48. MacIntyre · Br. J. Non-Destr. Test. · 1978 · 20 · 135
49. H.A. Ernst, J. Villasante, N. Pachao, D. Johnson, Specimen geometry effects on crack growth in sour environments, NACE Corrosion/2002 Paper No. 02060, Denver, Colorado, USA, 7–14 April, 2002.
50. K.E. Szklarz, Understanding the size effect in NACE TM0177 method D (DCB) testing and implications for users, NACE Corrosion/2001 Paper No. 01074, Houston, Texas, USA, 11–16 March, 2001.