The comparison of the corrosion of ultrapure iron and low-carbon steel under NaCl-electrolyte droplets
Source abstract
Abstract
Abstract The corrosion of ultrapure iron under deliquesced NaCl particles was compared with that of low-carbon steel. The critical droplet size for corrosion to occur was larger for ultrapure iron (150–200 μm) than that for low-carbon steel (40–100 μm) indicating a lower corrosion propensity for ultrapure iron. Polarization experiments performed under NaCl micro-droplets showed that ultrapure iron had passivation-like behavior and a pitting-like potential of ∼1.69 VSCE compared to ∼0.4 VSCE for low-carbon steel. The disparity was attributed to a more homogenous and protective iron oxide film on ultrapure iron as compared to that on low-carbon steel.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Corrosion Behavior and Inhibition · Hydrogen embrittlement and corrosion behaviors in metals · Metallurgical Processes and Thermodynamics
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (37)
Show source-provided references
1. The initiation mechanism of corrosion of zinc by sodium chloride particle deposition10.1016/S0010-938X(01)00056-7 ↗
2. Effect of sodium chloride particles on the atmospheric corrosion of pure copper10.5006/1.3299244 ↗
3. Electrochemical investigations of micro-droplets formed on metals during the deliquescence of salt particles in atmosphere10.1016/j.elecom.2005.02.018 ↗
4. Micro-droplets formation during the deliquescence of salt particles in atmosphere10.5006/1.3278152 ↗
5. In situ studies of the effect of CO2 on the initial NaCl-induced atmospheric corrosion of copper10.1149/1.1984448 ↗
6. Effect of carbon dioxide on sodium chloride-induced atmospheric corrosion of copper10.1149/1.2098327 ↗
7. In situ studies of the effect of SO2 on the initial NaCl-induced atmospheric corrosion of copper10.1149/1.2104107 ↗
8. Advantage of super-hydrophobic surface as a barrier against atmospheric corrosion induced by salt deliquescence10.1016/j.corsci.2014.09.001 ↗
9. Study of the atmospheric corrosion of galvanised steel in a micrometric electrolytic droplet10.1016/j.elecom.2006.03.024 ↗
10. Pitting corrosion mechanism of Type 304 stainless steel under a droplet of chloride solutions10.1016/j.corsci.2006.08.016 ↗
11. Corrosion of galvanised steel under an electrolytic drop10.1016/j.corsci.2006.05.027 ↗
12. Use of inkjet printing to deposit magnesium chloride salt patterns for investigation of atmospheric corrosion of 304 stainless steel10.1016/j.corsci.2011.05.055 ↗
13. Corrosion of an Al–Mg–Si alloy under MgCl2 solution droplets10.1016/j.corsci.2011.02.035 ↗
14. Li · 2010 · 205
15. Atmospheric corrosion initiation on steel from predeposited NaCl salt particles in high humidity atmospheres10.1179/147842209X12476568584296 ↗
16. In situ Raman spectroscopic study of NaCl particle-induced marine atmospheric corrosion of carbon steel10.1149/2.013204jes ↗
17. In situ Raman spectroscopic identification of rust formation in Evans' droplet experiments10.1016/j.elecom.2012.02.014 ↗
18. Atmospheric-corrosion electrochemistry of NaCl droplets on carbon steel10.1149/2.035211jes ↗
19. Effect of relative humidity on corrosion of steel under sea salt aerosol proxies II. MgCl2, artificial seawater10.1149/2.0231410jes ↗
20. Effect of relative humidity on corrosion of steel under sea salt aerosol proxies I. NaCl10.1149/2.0221410jes ↗
21. Marine aerosol drop size effects on the corrosion behavior of low carbon steel and high purity iron10.1149/2.1171412jes ↗
22. Aerosol salt particle deposition on metals exposed to marine environments: a study related to marine atmospheric corrosion10.1149/2.071405jes ↗
23. Limitations in microelectrochemical capillary cell testing and transformation of electrochemical transients for acquisition of microcell impedance data10.1016/j.electacta.2005.01.010 ↗
24. The effect of specimen size on the measured pitting potential of stainless steel10.1016/S0010-938X(97)83146-0 ↗
25. The use of microcapillary techniques to study the corrosion resistance of AZ91 magnesium alloy at the microscale10.1016/j.corsci.2011.05.054 ↗
26. Electrochemical properties of intermetallic phases and common impurity elements in magnesium alloys10.1149/1.3523229 ↗
27. In situ studies of sulfate nest formation on iron10.1149/1.1775911 ↗
28. Characterisation of initial atmospheric corrosion carbon steels by field exposure and laboratory simulation10.1016/j.corsci.2007.01.009 ↗
29. Initial NaCl-particle induced atmospheric corrosion of zinc-Effect of CO2 and SO210.1016/j.corsci.2007.06.005 ↗
30. Corrosion of Zn under acidified marine droplets10.1016/j.corsci.2011.01.044 ↗
31. The role of electrochemical polarization in micro-droplets formation10.1016/j.elecom.2008.09.010 ↗
32. Oxygen distribution as a factor in the corrosion of metals10.1021/ie50184a012 ↗
33. Evans · 1960
34. Electrochemical study of resistance to localized corrosion of stainless steels for biomaterial applications10.1149/1.1393307 ↗
35. Electrochemical behavior of two austenitic stainless steel biomaterials
36. Effect of composition on the electrochemical behavior of austenitic stainless steel in Ringer's solution10.5006/0010-9312-33.6.204 ↗
37. Effect of secondary phase precipitation on the corrosion behavior of duplex stainless steels10.3390/ma7075268 ↗