journal article·2016-09

Influence of substrate composition on the oxidation performance of nickel aluminide coating prepared by pack cementation

Yuhua Zhou, Li Wang, Guan Wang, Dongliang Jin, Wei Hao, Xiaofeng Zhao, Jian Zhang, Ping Xiao

Corrosion Science· Volume 110
Publisher page

Abstract

Effects of substrate compositions on the microstructure and oxidation behavior of NiAl coating by pack cementation were investigated. It is found that substrate compositions have a profound influence on the coating microstructure and oxidation performance. The DZ125 and DD6 coating systems exhibit better spallation resistance due to the presence of Hf. The interface rumpling, as well as the TiO2 and Ti-rich oxide are responsible for the oxide spallation of the DZ411 coating system. The voids at the oxide/coating interface, leading to a lower interfacial adhesion, result in the worst oxide spallation of the Ni and Hastelloy X coating systems.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: High-Temperature Coating Behaviors · Intermetallics and Advanced Alloy Properties · Flame retardant materials and properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (39)

Show source-provided references
1. Reed · 2006
2. Isothermal oxidation behavior of single crystal superalloy DD610.1016/S1003-6326(11)61210-7 ↗
3. A study on the microstructure and cyclic oxidation behavior of the pack aluminized Hastelloy X at 1100°C10.1016/j.surfcoat.2006.07.257 ↗
4. Advances in coating design for high performance gas turbines10.1557/mrs2003.194 ↗
5. Kinetics and mechanism of isothermal oxidation of compositionally graded yttria stabilized zirconia (YSZ) based thermal barrier coating10.1016/j.corsci.2014.06.050 ↗
6. Wrinkling of α-alumina films grown by oxidation-II. Oxide separation and failure10.1016/S1359-6454(98)00134-7 ↗
7. Oxidation of NiAl and FeAl10.1016/S0966-9795(99)00037-0 ↗
8. The influence of oxides on the performance of advanced gas turbines10.1016/j.jeurceramsoc.2007.12.023 ↗
9. Substrate and bond coat compositions: factors affecting alumina scale adhesion10.1016/S0921-5093(97)00851-4 ↗
10. Influence of substrate material on oxidation behavior and cyclic lifetime of EB-PVD TBC systems10.1016/S0257-8972(01)01481-5 ↗
11. Substrate effect on the high-temperature oxidation behavior of a Pt-modified aluminide coating. Part I: influence of the initial chemical composition of the coating surface10.1007/s11085-006-9024-z ↗
12. Effect of Hf, Y and C in the underlying superalloy on the rumpling of diffusion aluminide coatings10.1016/j.actamat.2007.10.006 ↗
13. Effect of superalloy substrate and bond coating on TBC lifetime10.1016/j.surfcoat.2010.08.154 ↗
14. Microstructures and cyclic oxidation behaviour of Pt-free and low-Pt NiAl coatings on the Ni-base superalloy Rene-8010.1016/j.corsci.2011.10.037 ↗
15. Microstructure and oxidation behavior of Al and Hf co-deposition coatings on nickel-based superalloys10.1016/j.surfcoat.2013.02.049 ↗
16. Effect of Y2O3 content in the pack on microstructure and hot corrosion resistance of Y-Co-modified aluminide coating10.1016/j.corsci.2014.05.018 ↗
17. Effect of Al content on the lifetime of thermally grown oxide formed on Ni-Al alloys after isothermal oxidation10.1016/j.corsci.2014.07.023 ↗
18. Substrate effect on the high temperature oxidation behavior of a Pt-modified aluminide coating. Part II: long-term cyclic-oxidation tests at 1050°C10.1007/s11085-007-9072-z ↗
19. Effect of heat treatment on coating microstructure applied by high activity diffusion process on IN738LC10.1179/1743294412Y.0000000064 ↗
20. Surface rumpling of a (Ni, Pt)Al bond coat induced by cyclic oxidation10.1016/S1359-6454(00)00156-7 ↗
21. Characterization and understanding of residual stresses in a NiCoCrAlY bond coat for thermal barrier coating application10.1016/j.actamat.2015.04.053 ↗
22. High-temperature oxidation behavior of minor Hf doped NiAl alloy in dry and humid atmospheres10.1016/j.corsci.2013.06.017 ↗
23. Oxidation behavior of Hf-modified aluminide coatings on Inconel-718 at 1050°C10.6000/2369-3355.2014.01.01.4 ↗
24. Mechanisms controlling durability of thermal barrier coatings10.1016/S0079-6425(00)00020-7 ↗
25. Bose · 2007 · 29
26. Optimization of reactive-element additions to improve oxidation performance of alumina-forming alloys10.1111/j.1151-2916.2003.tb03358.x ↗
27. Nondestructive evaluation of the oxidation stresses through thermal barrier coatings using Cr3+ piezospectroscopy10.1063/1.117182 ↗
28. The adhesion of alumina films to metallic alloys and coatings10.1002/(SICI)1521-4176(200005)51:5<358::AID-MACO358>3.0.CO;2-C ↗
29. The role of chemical composition on the oxidation performance of aluminide coatings10.1016/j.surfcoat.2004.08.007 ↗
30. Development of improved bond coat for enhanced turbine durability
31. Cyclic oxidation of β-NiAl with various reactive element dopants at 1200°C10.1016/j.corsci.2012.09.010 ↗
32. Effect of quaternary additions on the oxidation behavior of Hf-doped NiAl10.1023/A:1023087926788 ↗
33. Effects of minor elements on the cyclic-oxidation behavior of commercial Fe-base 800-series alloys10.1023/B:OXID.0000038785.16792.3d ↗
34. Oxidation behaviour of NiAl. II. Cavity formation beneath the oxide scale on NiAl of different stoichiometries10.1016/0010-938X(93)90271-H ↗
35. The role of oxidation induced cavities on the failure of the thermally grown oxide on binary β-NiAl alloys10.3139/146.030157 ↗
36. Influence of Pt on the metal-oxide interface during high temperature oxidation of NiAl bulk materials10.1016/j.corsci.2008.12.016 ↗
37. Interfacial segregation pore formation, and scale adhesion on NiAl alloys10.1007/s11085-005-1954-3 ↗
38. Observations of reactive element gettering of sulfur in thermally grown oxide pegs10.1016/j.scriptamat.2006.06.017 ↗
39. Effect of Sm, Gd Yb, Sc and Nd as reactive elements on oxidation behaviour of β-NiAl at 1200°C10.1016/j.corsci.2013.10.021 ↗