The effect of manganese and silicon additions on the corrosion resistance of a polycrystalline nickel-based superalloy
Source abstract
Abstract
The service lives of nickel superalloys are often limited by environmental degradation. The present study compares oxidation, sulfidation and hot corrosion at 750 °C of three variants of a polycrystalline superalloy: a baseline alloy, a variant containing 1 wt% Mn and one containing 0.5 wt% Si. Mn reduced the oxidation rate without changing the scale morphology. The MnCr2O4 scale formed proved more protective against sulfidation and hot corrosion, but internal sulfides extended the damage depth. Si modified the oxide morphology to a continuous Cr2O3-Al2O3 dual layer. This provided improved protection, reducing the sulfidation depth by 2/3 and the hot corrosion depth by ½.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: High-Temperature Coating Behaviors · High Temperature Alloys and Creep · Metallurgical Processes and Thermodynamics
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (50)
Show source-provided references
1. Effects of environment on high-temperature fatigue crack growth in a superalloy10.1007/BF02811710 ↗
2. Effect of SO2 and water vapour on the low-cycle fatigue properties of nickel-base superalloys at elevated temperature10.1016/j.msea.2012.11.079 ↗
3. Influence of environmental factors on the corrosion-fatigue response of a nickel-based superalloy10.1080/02670836.2017.1300419 ↗
4. Corrosion-fatigue testing of Ni-based superalloy RR100010.1080/02670836.2016.1242827 ↗
5. Hot corrosion of materials: a fluxing mechanism?10.1016/S0010-938X(01)00057-9 ↗
6. Luthra · 1982 · 1843
7. Reed · 2006
8. Oxidation behaviour of a next generation polycrystalline Mn containing Ni-based superalloy10.1016/j.scriptamat.2015.10.001 ↗
9. Sulfidation of manganese in H2S-H2 atmospheres at temperatures between 1073 and 1273 K10.1007/BF00603836 ↗
10. Oxidation of manganese in CO[sub 2]-CO mixtures10.1149/1.2423353 ↗
11. High-temperature sulfidation of Fe-Mn alloys10.1007/BF00604104 ↗
12. Sulfidation behavior of a binary Fe-Mn alloy10.1007/BF00665013 ↗
13. Characterisation of oxide scale formation on a new single crystal superalloy for power generation applications10.3184/096034012X13335334078005 ↗
14. The effect of boron on oxide scale formation in a new polycrystalline superalloy10.1016/j.scriptamat.2016.09.013 ↗
15. M. C. Hardy, “European Patent Specification EP2562277 B1.”.
16. Effect of surface preparation on the 815°C oxidation of single-crystal nickel-based superalloys10.1007/s11837-015-1639-6 ↗
17. Kinetic and morphological development of oxide-sulfide scales on manganese at 1073 K10.1007/BF00665193 ↗
18. Oxidation behaviour of a next generation polycrystalline Mn containing Ni-based superalloy10.1016/j.scriptamat.2015.10.001 ↗
19. Effect of nickel base superalloy composition on oxidation resistance in SO2 containing, high pO2 environments10.1002/maco.201307299 ↗
20. Oxidation and the effects of high temperature exposures on notched fatigue life of an advanced powder metallurgy disk superalloy10.7449/2012/Superalloys_2012_863_872 ↗
21. Defect and transport properties of sulfides and sulfidation in metals10.1515/HTMP.1984.6.1-2.1 ↗
22. The standard free energy of formation of nonstoichiometric niobium sulfides,” Metall
23. Molybdenum and niobium sulphides10.1038/185376a0 ↗
24. The defect structure of 2s Nb1+xS2 and the high-temperature sulfidation of niobium10.1007/BF00665664 ↗
25. Precipitation around welds in the nickel-base superalloy, Inconel 71810.1016/0001-6160(85)90231-7 ↗
26. S. J. S. University, “Interactive Ellingham Diagram tool.” [Online]. Available: http://www.engr.sjsu.edu/ellingham/.
27. University of Cambridge, “Interactive Ellingham diagram tool.” [Online]. Available: https://www.doitpoms.ac.uk/tlplib/ellingham_diagrams/interactive.php.
28. Critical evaluation and thermodynamic modeling of the Mn-Cr-O system for the oxidation of SOFC interconnect10.1016/j.ssi.2006.01.012 ↗
29. Identifying heating rate dependent oxidation reactions on a nickel-based superalloy using synchrotron diffraction10.1016/j.actamat.2019.10.019 ↗
30. Oxidation fo Ni-Cr-Al Alloys between 1000C and 1200C10.1149/1.2407837 ↗
31. Oxidation behaviour of a next generation polycrystalline Mn containing Ni-based superalloy10.1016/j.scriptamat.2015.10.001 ↗
32. Modelling of high temperature oxidation of alumina-forming single-crystal nickel-base superalloys10.1016/j.actamat.2012.06.036 ↗
33. Oxidation of nickel-based single-crystal superalloys for industrial gas turbine applications10.1016/j.actamat.2010.09.027 ↗
34. Sulphide formation after pre-oxidation of chromia formers10.1016/S0010-938X(96)00069-8 ↗
35. High-temperature corrosion of pure chromium in SO2 (700-1000°C)10.1007/BF00603790 ↗
36. The thermochemistry of transition metal sulfides10.1007/BF00608014 ↗
37. Thermal stability of the MoS2 phase in injection moulded 17-4 PH stainless steel10.1016/S2238-7854(12)70024-8 ↗
38. High temperature oxidation and corrosion of metals
39. The chromium-sulphur system between 873 K and 1364 K10.1016/0022-5088(77)90194-1 ↗
40. Kofstad · 1988
41. Thermodynamics of molten sulfate mixtures10.1149/1.2124305 ↗
42. Synergistic dissolution of oxides in molten sodium sulfate10.1149/1.2086647 ↗
43. Reaction morphologies developed by nickel aluminides in type II hot corrosion conditions: the effect of chromium10.1016/j.corsci.2015.08.029 ↗
44. High-temperature sulfidation of Fe-30Mo alloys containing ternary additions of Al10.1007/BF00664708 ↗
45. High-temperature sulfidation behavior of Ni-Nb alloys
46. Kinetics and morphological development of the sulfide scale on a Nickel-20 w/o chromium alloy in hydrogen sulfide-hydrogen atmospheres at 700°C10.1149/1.2408156 ↗
47. The Ni-S system and related minerals10.1093/petrology/3.1.126 ↗
48. Pedrazzini · 2018 · 49
49. Effects of oxidation and hot corrosion in a nickel disc alloy
50. High-temperature corrosion of manganese in pure SO210.1007/BF00604101 ↗