Hydrogen-enhanced compatibility constraint for intergranular failure in FCC FeNiCoCrMn high-entropy alloy
Source abstract
Abstract
Abstract The fundamental mechanism of hydrogen embrittlement was investigated in the high-entropy alloy FeNiCoCrMn using slow strain rate tensile tests with and without internal hydrogen. Hydrogen induced intergranular failure and reduced the average grain elongation parallel to the tensile axis, but also increased the local plasticity within grains. The influence of hydrogen on plasticity establishes a compatibility constraint across grain boundaries, which results in failure along the hydrogen-weakened grain boundaries. This study is the first to directly confirm the presence of the hydrogen-enhanced compatibility constraint in a high-entropy alloy and highlights the importance of developing a physical understanding of grain-scale interactions.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: High Entropy Alloys Studies · Hydrogen embrittlement and corrosion behaviors in metals · High-Temperature Coating Behaviors
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (64)
Show source-provided references
1. Microstructural development in equiatomic multicomponent alloys10.1016/j.msea.2003.10.257 ↗
2. Tensile properties of high-and medium-entropy alloys10.1016/j.intermet.2013.03.018 ↗
3. Processing, microstructure and mechanical properties of the CrMnFeCoNi high-entropy alloy10.1007/s11837-015-1589-z ↗
4. The influences of temperature and microstructure on the tensile properties of a CoCrFeMnNi high-entropy alloy10.1016/j.actamat.2013.06.018 ↗
5. Effect of cryo-deformation on structure and properties of CoCrFeNiMn high-entropy alloy10.1016/j.intermet.2014.12.004 ↗
6. Temperature dependence of the mechanical properties of equiatomic solid solution alloys with face-centered cubic crystal structures10.1016/j.actamat.2014.08.026 ↗
7. A fracture-resistant high-entropy alloy for cryogenic applications10.1126/science.1254581 ↗
8. Mechanisms of radiation-induced segregation in CrFeCoNi-based single-phase concentrated solid solution alloys10.1016/j.actamat.2016.12.046 ↗
9. Enhancing radiation tolerance by controlling defect mobility and migration pathways in multicomponent single-phase alloys10.1038/ncomms13564 ↗
10. Sluggish diffusion in Co–Cr–Fe–Mn–Ni high-entropy alloys10.1016/j.actamat.2013.04.058 ↗
11. The effect of hydrogen on the mechanical properties of high purity iron II. Effect of quenched-in hydrogen below room temperature10.1016/0025-5416(79)90192-7 ↗
12. Solute segregation and hydrogen-induced intergranular fracture in an alloy steel10.1007/BF02644295 ↗
13. Hydrogen-induced intergranular fracture of steels10.1016/S0013-7944(00)00124-7 ↗
14. Grain-boundary engineering markedly reduces susceptibility to intergranular hydrogen embrittlement in metallic materials10.1016/j.actamat.2009.05.012 ↗
15. Hydrogen-induced intergranular failure in nickel revisited10.1016/j.actamat.2012.01.040 ↗
16. Role of grain boundary chemistry and the environment on intergranular fracture
17. Hydrogen induced intergranular cracking of nickel and nickel-base alloys
18. Fracture mode transition of iron in hydrogen as a function of grain boundary sulfur10.1016/0036-9748(80)90142-8 ↗
19. Intergranular embrittlement of nickel by hydrogen: the effect of grain boundary segregation10.1007/BF02644118 ↗
20. Intergranular brittleness in iron10.1016/0001-6160(66)90004-6 ↗
21. Hydrogen embrittlement of the equi-molar FeNiCoCr alloy10.1016/j.actamat.2018.07.032 ↗
22. Hydrogen embrittlement in compositionally complex FeNiCoCrMn FCC solid solution alloy10.1016/j.cossms.2017.11.002 ↗
23. Hydrogen-induced compatibility constraints across grain boundaries drive intergranular failure of Ni10.1016/j.msea.2019.05.036 ↗
24. Brittle fracture of grain boundaries10.1023/B:INTS.0000028644.07075.4e ↗
25. Effect of hydrogen environment on the separation of Fe grain boundaries10.1016/j.actamat.2016.01.067 ↗
26. Elucidating the contribution of mobile hydrogen-deformation interactions to hydrogen-induced intergranular cracking in polycrystalline nickel10.1016/j.actamat.2018.07.043 ↗
27. Hydrogen - the versatile embrittler: whitney award lecture10.5006/1.3583875 ↗
28. Hydrogen embrittlement understood10.1007/s11663-015-0325-y ↗
29. Enumeration of the hydrogen-enhanced localized plasticity mechanism for hydrogen embrittlement in structural materials10.1016/j.actamat.2018.12.014 ↗
30. Assessment of the impact of hydrogen on the stress developed ahead of a fatigue crack10.1016/j.actamat.2019.05.028 ↗
31. Hydrogen resistance of a 1 GPa strong equiatomic CoCrNi medium entropy alloy10.1016/j.corsci.2020.108510 ↗
32. A strong and ductile medium-entropy alloy resists hydrogen embrittlement and corrosion10.1038/s41467-020-16791-8 ↗
33. Resistance of CoCrFeMnNi high-entropy alloy to gaseous hydrogen embrittlement10.1016/j.scriptamat.2017.03.029 ↗
34. Hydrogen enhances strength and ductility of an equiatomic high-entropy alloy10.1038/s41598-017-10774-4 ↗
35. Influence of pre-strain on the gaseous hydrogen embrittlement resistance of a high-entropy alloy10.1016/j.msea.2018.01.107 ↗
36. Strong resistance to hydrogen embrittlement of high-entropy alloy10.1016/j.msea.2018.08.101 ↗
37. Ultrahigh-strength CoCrFeMnNi high-entropy alloy wire rod with excellent resistance to hydrogen embrittlement10.1016/j.msea.2018.06.086 ↗
38. Comparative study of hydrogen embrittlement in stable and metastable high-entropy alloys10.1016/j.scriptamat.2018.03.003 ↗
39. Hydrogen embrittlement of an interstitial equimolar high-entropy alloy10.1016/j.corsci.2018.03.040 ↗
40. Grain refinement effect on hydrogen embrittlement resistance of an equiatomic CoCrFeMnNi high-entropy alloy10.1016/j.ijhydene.2019.04.280 ↗
41. Modeling hydrogen induced damage mechanisms in metals
42. Atomistic study of hydrogen embrittlement of grain boundaries in nickel: I. Fracture10.1016/j.jmps.2017.01.020 ↗
43. The effect of diffusive hydrogen segregation on fracture of polycrystalline nickel10.1016/0001-6160(86)90010-6 ↗
44. The influence of hydrogen on the plastic deformation, ductility, and fracture of nickel in tension10.1016/0001-6160(63)90209-8 ↗
45. First principles assessment of ideal fracture energies of materials with mobile impurities: implications for hydrogen embrittlement of metals10.1016/j.actamat.2004.06.037 ↗
46. Influence of hydrogen on the grain boundary crack propagation in bcc iron: a molecular dynamics simulation10.1016/j.commatsci.2018.03.053 ↗
47. SIMS study of hydrogen at the surface and grain boundaries of nickel bicrystals10.1016/0001-6160(87)90150-7 ↗
48. First-principles investigation of hydrogen trapping and diffusion at grain boundaries in nickel10.1016/j.actamat.2015.07.031 ↗
49. Meso-scale anisotropic hydrogen segregation near grain-boundaries in polycrystalline nickel characterized by EBSD/SIMS10.1016/j.matlet.2015.12.016 ↗
50. The dual role of coherent twin boundaries in hydrogen embrittlement10.1038/ncomms7164 ↗
51. Influence of hydrogen on dislocation self-organization in Ni, Acta Mater
52. An HVEM study of hydrogen effects on the deformation and fracture of nickel10.1016/0001-6160(86)90071-4 ↗
53. Atomistic studies of hydrogen effects on grain boundary structure and deformation response in FCC Ni10.1016/j.commatsci.2016.05.014 ↗
54. Revisiting hydrogen embrittlement models and hydrogen-induced homogeneous nucleation of dislocations10.1016/j.scriptamat.2009.09.037 ↗
55. Frankel · 1984
56. Dislocation cell formation in metals10.1063/1.1659399 ↗
57. Hydrogen effects on the interaction between dislocations10.1016/S1359-6454(97)00349-2 ↗
58. Hydrogen effects on the character of dislocations in high-purity aluminum10.1016/S1359-6454(99)00156-1 ↗
59. A mechanism behind hydrogen-assisted fatigue crack growth in ferrite-pearlite steel focusing on its behavior in gaseous environment at elevated temperature10.1016/j.corsci.2020.108558 ↗
60. Effect of dislocation cell walls on hydrogen adsorption, hydrogen trapping and hydrogen embrittlement resistance10.1016/j.corsci.2020.108428 ↗
61. The influence of hydrogen on cyclic plasticity of <001> oriented nickel single crystal. Part I: dislocation organisations and internal stresses10.1016/j.ijplas.2019.09.017 ↗
62. Effect of grain size on the resistance to hydrogen embrittlement of API 2W Grade 60 steels using in situ slow-strain-rate testing10.1016/j.corsci.2017.08.032 ↗
63. The advantage of grain refinement in the hydrogen embrittlement of Fe–18Mn–0.6C twinning-induced plasticity steel10.1016/j.corsci.2015.01.012 ↗
64. The effect of grain size and aging on hydrogen embrittlement of a maraging steel10.1016/j.corsci.2008.06.044 ↗