Corrosion of magnesia-chromite refractory by PbO-rich copper slags
Source abstract
Abstract
The work presents corrosion of direct-bonded MgO-Cr refractory by three types of PbO-rich copper slags. Pellet test, contact corrosion test and hot stage microscopy test enabled to study corrosion phenomena at 1300 °C and 1450 °C, respectively. The structure and microstructure of the after-corrosion samples were deeply analyzed, with the former one aided by development of image detection algorithms. Slags infiltrated the refractory through open pores and cracks. Slag components diffused into refractory and changed its original composition. Forsterite solid solution, Mg2SiO4 s.s., which formed as the only corrosion product caused swelling of microstructure and disintegration of magnesia-chromite direct bonds, critical for the performance of refractory.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Metallurgical Processes and Thermodynamics · Advanced materials and composites · High-Temperature Coating Behaviors
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (59)
Show source-provided references
1. Degradation mechanisms and use of refractory linings in copper production processes: a critical review10.1016/j.jeurceramsoc.2013.10.005 ↗
2. Chromite in refractories
3. Post mortem analysis of burned magnesia-chromite brick used in short rotary furnace of secondary lead smelting10.1590/S0366-69132009000100008 ↗
4. Refractories for copper production10.1080/08827509608914131 ↗
5. Chromite — a cost-effective refractory raw material for refractories in various metallurgical applications
6. Assessment of coclinkered shaped magnesite-chromite refractories processed from Egyptian materials
7. Bezchromowe, niewypalane materiały ogniotrwałe
8. Galos · 1999
9. Innovative magnesia-chrome fused grain material for non-ferrous metals refractory applications
10. Wpływ warunków wypalania na kształtowanie mikrostruktury tworzyw magnezjowo-chromitowych
11. Beneficiation of low grade chromite ore and its characterization for the formation of magnesia-chromite refractory by economcally viable process
12. A comparison of the effect of nanostructured MgCr2O4 and FeCr2O4 additions on the microstructure and mechanical properties of direct-bonded magnesia-chrome refractories10.1016/j.ceramint.2019.09.028 ↗
13. High-performance chromite by structure stabilization treatment10.1007/s42243-019-00354-3 ↗
14. The effect of a temperature gradient on the phase formation inside a magnesia-chromite refractory in contact with a non-ferrous PbO-SiO2-MgO slag10.1016/j.jeurceramsoc.2015.03.028 ↗
15. Copper anode furnace: chemical, mineralogical and thermo-chemical considerations of refractory wear mechanisms10.1007/s11837-018-3089-4 ↗
16. Optimisation of an anode furnace refractory lining using distinct magnesia-chromite refractory types
17. Identification of magnesia-chromite refractory degradation mechanisms of secondary copper smelter linings10.1016/j.jeurceramsoc.2016.02.036 ↗
18. The effect of phase formation during use on the chemical corrosion of magnesia-chromite refractories in contact with a non-ferrous PbO-SiO2 based slag10.1016/j.jeurceramsoc.2013.12.026 ↗
19. Premchand, Characteristics and utilisation of copper slag – a review10.1016/S0921-3449(02)00171-4 ↗
20. Chemical degradation of magnesia-chromite refractory used in the conversion step of the pyrometallurgical copper-making process: a thermochemical approach10.1016/j.ceramint.2018.07.052 ↗
21. Post-mortem study of magnesia-chromite refractory used in Peirce-Smith Converter for copper-making process, supported by thermochemical calculations10.1016/j.ceramint.2018.04.168 ↗
22. Improving corrosion behaviour of magnesia-chrome refractories by addition of nanoparticles
23. New refractory materials for the copper industry
24. Wetting behavior between fayalite-type slags and solid magnesia10.1111/j.1151-2916.1997.tb03112.x ↗
25. Influence of FeO/SiO2 and CaO/SiO2 ratios in iron-saturated ZnO-rich fayalite slags on the corrosion of MgO10.1111/jace.14379 ↗
26. Chemical wear of basic brick linings in the non-ferrous industry
27. Chemical degradation mechanisms of magnesia–chromite refractories in the copper smelting furnace10.1007/s11837-018-3083-x ↗
28. The influence of ZnO in fayalite slag on the degradation of magnesia-chromite refractories during secondary Cu smelting10.1016/j.jeurceramsoc.2015.03.013 ↗
29. Effect of ZnO level in secondary copper smelting slags on slag/magnesia-chromite refractory interactions10.1016/j.jeurceramsoc.2016.02.004 ↗
30. Gregurek · 2018
31. Corrosion mechanism of magnesia-chromite refractories by ZnO-containing fayalite slags: effect of funnel glass addition10.1007/s12613-019-1912-8 ↗
32. Chemical corrosion mechanisms of magnesia-chromite and chrome-free refractory bricks by copper metal and anode slag10.1016/j.jeurceramsoc.2006.08.020 ↗
33. Corrosive interaction between slags high in copper and nickel oxides and periclase, periclase-chromite, and chromite refractories10.1007/s11148-006-0003-3 ↗
34. The influence of slag compositional changes on the chemical degradation of magnesia-chromite refractories exposed to PbO-based non-ferrous slag saturated in spinel10.1016/j.jeurceramsoc.2014.08.017 ↗
35. Influence of the atmosphere on the mechanical properties and slag resistance of magnesia-chrome bricks10.1016/j.ceramint.2020.01.146 ↗
36. Characterization of copper slag
37. Effect of the chemical composition of slag on the corrosion of calcium zirconate material
38. Application of hot-stage microscopy to evaluating sample morphology changes on heating10.1007/s10973-016-5323-z ↗
39. Wojnar · 2002
40. Wojnar · 2020
41. Degradation mechanisms of magnesia-chromite refractories in vacuum-oxygen decarburization ladles during production of stainless steel10.1179/030192300677525 ↗
42. The ‘direct bond’ in magnesia chromite and magnesia spinel refractories10.1111/j.1151-2916.1995.tb08885.x ↗
43. Chemical wear mechanism of magnesia-chromite refractory for an oxygen bottom-blown copper-smelting furnace: a post-mortem analysis10.1016/j.ceramint.2020.09.124 ↗
44. Research and development of novel refractory of MgO doped with ZrO2 nanoparticles for copper slag resistance10.3390/ma14092277 ↗
45. Phase equilibria of the MgO-Cu2O-CuO system10.1016/S0025-5408(96)00184-5 ↗
46. 〈https://www.sciencedirect.com/topics/chemistry/copper-oxide〉, (Accessed 30 October 2021).
47. Explaining the dependence of M-site diffusion in forsterite on silica activity: a density functional theory approach
48. Effects of Mg/Si ratio on microwave dielectric characteristics of forsterite ceramics10.1111/j.1551-2916.2007.01656.x ↗
49. Post-mortem study of magnesia-chromiterefractory used in the gas area of a submerged arcfurnace for the copper-making process
50. Kucharski · 2003
51. Slag characterization: a necessary tool for modeling and simulating refractory corrosion on a pilot scale10.1007/s11837-014-1070-4 ↗
52. Thermodynamics of arsenic in FeOx-CaO-SiO2 slags10.1007/s11663-010-9430-0 ↗
53. Technological implications of neo-formed hematite crystals in ceramic lead glazes
54. Interaction of refractories with the melt in copper smelting
55. System CuO-MgO-Cu2O. Phase relations in air dependent on temperature
56. The wetting of refractory products by copper and cuprous oxides
57. Comparative analysis of refractory wear in the copper-making process by a novel (industrial) dynamic test10.1016/j.ceramint.2018.10.027 ↗
58. Postmortem study of a magnesia-chromite brick from a lead recycling furnace10.1007/s11837-015-1512-7 ↗
59. Phase formation processes and structural changes in chromite-periclase refractories used during nickel production10.1007/s11148-012-9433-2 ↗