Abstract

Abstract Coating technologies are cost-effective solutions to the Cl-induced hot corrosion problems in biomass boilers. In this study, an arc sprayed Fe-Cr-Mo amorphous coating was fabricated and exposed to a stimulated biomass firing condition at 500 °C and 600 °C. Fe and Cr in the coating were vulnerable to chlorination and continuously evaporated, leaving Cr depletion zones. The distribution of Mo was inhomogeneous, and Mo-rich zones were resistant to gaseous corrosive species but susceptible to electrochemical attack as temperature increased. The crevices in the coating were detrimental to its corrosion resistance by acting as corrodent diffusing channels.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: High-Temperature Coating Behaviors · Metallic Glasses and Amorphous Alloys · Advanced materials and composites

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (69)

Show source-provided references
1. IEA · Renewables 2019 · 2019
2. IEA · Bioenergy Power Gener. · 2020
3. Advantages and disadvantages of composition and properties of biomass in comparison with coal: An overview10.1016/j.fuel.2015.05.050 ↗
4. Ash-related issues during biomass combustion: Alkali-induced slagging, silicate melt-induced slagging (ash fusion), agglomeration, corrosion, ash utilization, and related countermeasures10.1016/j.pecs.2015.09.003 ↗
5. An overview of the chemical composition of biomass10.1016/j.fuel.2009.10.022 ↗
6. Characterisation of the most representative agricultural and forestry biomasses in France for gasification10.1007/s12649-015-9374-3 ↗
7. Utilizing biomass and waste for power production-a decade of contributing to the understanding, interpretation and analysis of deposits and corrosion products10.1016/j.fuel.2004.08.026 ↗
8. Transformation and release to the gas phase of Cl, K, and S during combustion of annual biomass10.1021/ef049944q ↗
9. Predicting gaseous emissions from small-scale combustion of agricultural biomass fuels10.1016/j.biortech.2014.11.100 ↗
10. Karlsson · 2015
11. Field test corrosion experiments in Denmark with biomass fuels
12. The implications of chlorine-associated corrosion on the operation of biomass-fired boilers10.1016/S0360-1285(00)00003-4 ↗
13. Larsson · 2017
14. The effects of chlorides, hydrogen chloride, and sulfur dioxide in the oxidation of steels below deposits10.1016/0010-938X(95)00011-8 ↗
15. Impact of deposits and their morphology on the active corrosion of iron in chlorine- and sulfur-containing atmospheres in the temperature range of 350–500 °C10.1007/s11085-018-9845-6 ↗
16. The influence of KCl on the corrosion of an austenitic stainless steel (304L) in oxidizing humid conditions at 600°C: A microstructural study10.1007/s11085-009-9156-z ↗
17. Lab-scale investigation of deposit-induced chlorine corrosion of superheater materials under simulated biomass-firing conditions
18. Effect of flue gas composition on deposit induced high temperature corrosion under laboratory conditions mimicking biomass firing. Part II: Exposures in SO2 containing atmospheres10.1002/maco.201609174 ↗
19. The role of alloying elements in commercial alloys for corrosion resistance in oxidizing-chloridizing atmospheres. Part II: Experimental investigations10.1002/maco.200303673 ↗
20. The role of alloying elements in commercial alloys for corrosion resistance in oxidizing-chloridizing atmospheres. Part I: Literature evaluation and thermodynamic calculations on phase stabilities10.1002/maco.200390129 ↗
21. Corrosion mechanisms of ferritic-martensitic P91 steel and Inconel 600 nickel-based alloy in molten chlorides. Part II: NaCl-KCl-MgCl2 ternary system10.1016/j.solmat.2020.110675 ↗
22. Hot corrosion: a modification of reactants causing degradation10.1080/09603409.2017.1404692 ↗
23. The effects of KCl, K2SO4 and K2CO3 on the high temperature corrosion of a 304-type austenitic stainless steel10.1007/s11085-011-9240-z ↗
24. The influence of potassium-rich biomass ashes on steel corrosion above 550 °C10.1016/j.enconman.2019.02.074 ↗
25. Janz · 1976
26. An ESEM in situ investigation of initial stages of the KCl induced high temperature corrosion of a Fe-2.25Cr-1Mo steel at 400°C10.1016/j.corsci.2011.03.007 ↗
27. The influence of small amounts of KCl(s) on the high temperature corrosion of a Fe-2.25Cr-1Mo steel at 400 and 500°C10.1002/maco.201005942 ↗
28. Comparison of potassium chloride and potassium carbonate with respect to their tendency to cause high temperature corrosion of stainless 304L steel10.1016/j.fuproc.2011.12.016 ↗
29. KCl-induced high temperature corrosion of selected commercial alloys10.1002/maco.201408213 ↗
30. Are NaCl and KCl equally corrosive on superheater materials of steam boilers?10.1016/j.fuel.2012.07.020 ↗
31. Role of alloying elements and carbides in the chlorine-induced corrosion of steels and alloys10.1590/S1516-14392004000100013 ↗
32. Effect of microstructure on KCl corrosion attack of modified AISI 310 steel10.1080/09603409.2017.1389381 ↗
33. Hot corrosion behaviors of TP347H and HR3C stainless steel with KCl deposit in oxy-biomass combustion10.1016/j.jenvman.2020.110411 ↗
34. High temperature interaction of Al/Si-modified Fe–Cr alloys with KCl10.1016/j.corsci.2006.10.019 ↗
35. Thermally sprayed coatings resistant to erosion and corrosion for power plant boilers - A review10.1016/j.surfcoat.2014.10.046 ↗
36. Chloride- and sulphate-induced hot corrosion mechanism of super austenitic stainless steel S31254 under dry gas environment10.1016/j.corsci.2019.108295 ↗
37. Fabrication and characterization of thermal-sprayed Fe-based amorphous/nanocrystalline composite coatings: An overview10.1007/s11666-014-0096-z ↗
38. High-temperature erosion resistance of FeBSiNb amorphous coatings deposited by arc spraying for boiler applications10.1007/s11666-012-9876-5 ↗
39. Iron-based bulk metallic glasses10.1179/1743280412Y.0000000007 ↗
40. Pitting initiation in Fe-based amorphous coatings10.1016/j.actamat.2012.04.005 ↗
41. Bulk glassy Fe-Cr-Mo-C-B alloys with high corrosion resistance10.1016/S0010-938X(02)00002-1 ↗
42. Subsequent sealing of thermally sprayed coatings to increase corrosion resistance10.1179/sur.1994.10.1.46 ↗
43. Corrosion resistance of Fe-Cr-based amorphous alloys: An overview10.1016/j.jnoncrysol.2016.04.009 ↗
44. Formation and corrosion behavior of Fe-based amorphous metallic coatings by HVOF thermal spraying10.1016/j.surfcoat.2009.08.025 ↗
45. Iron-based amorphous metals: High-performance corrosion-resistant material development10.1007/s11661-008-9779-8 ↗
46. Microstructure and properties of Fe-based amorphous metallic coating produced by high velocity axial plasma spraying10.1016/j.jallcom.2009.04.086 ↗
47. Chlorine-induced high-temperature corrosion and erosion-corrosion of HVAF and HVOF-sprayed amorphous Fe-based coatings10.1016/j.surfcoat.2019.01.080 ↗
48. The corrosion behaviours of plasma-sprayed Fe-based amorphous coatings10.1080/02670844.2017.1319647 ↗
49. Influence of sealing treatment on the corrosion resistance of Fe-based amorphous coatings in HCl solution10.1016/j.jallcom.2017.04.179 ↗
50. Preparation and characterization of highly amorphous HVOF stainless steel coatings10.1016/j.jallcom.2010.02.062 ↗
51. Correlation between microstructural characteristics and the abrasion wear resistance of sealed thermal-sprayed coatings10.1016/j.surfcoat.2005.07.092 ↗
52. Element-resolved corrosion analysis of stainless-type glass-forming steels10.1126/science.1230081 ↗
53. Synthesis and characterization of mica iron oxide
54. Spatial and temporal confinement of salt fluxes for the shape-controlled synthesis of Fe2O3 nanocrystals10.1021/cm3038087 ↗
55. Lide · 2004
56. Molten salt synthesis of calcium hydroxyapatite whiskers10.1111/j.1151-2916.2001.tb00653.x ↗
57. Chloride salt systems for high temperature thermal energy storage: Properties and applications
58. Investigation on the thermal properties of Fe2O(SO4)2 Part II10.1023/A:1011599719230 ↗
59. Thermal decomposition of Fe2(SO4)3: Demonstration of Fe2O3 polymorphism10.1023/A:1022543323651 ↗
60. Maier · 2015
61. The effect of temperature on mechanical properties of oxide scales formed on a carbon steel in a simulated municipal solid waste incineration environment10.1016/j.surfcoat.2013.10.035 ↗
62. High-temperature chemistry of HCl and Cl210.1016/j.combustflame.2015.04.002 ↗
63. KCl induced corrosion of a 304-type austenitic stainless steel at 600°C: The role of potassium10.1007/s11085-005-5704-3 ↗
64. Comparison of the high-temperature chloride-induced corrosion between duplex steel and Ni based alloy in presence of H2S10.1016/j.corsci.2018.04.042 ↗
65. High-temperature corrosion in waste-to-energy boilers10.1007/s11666-006-9005-4 ↗
66. Chlorine-induced high temperature corrosion of HVAF-sprayed Ni-based alumina and chromia forming coatings10.1016/j.corsci.2017.12.033 ↗
67. A microstructural and kinetic investigation of the KCl-induced corrosion of an FeCrAl alloy at 600°C10.1007/s11085-015-9546-3 ↗
68. Evidence of corrosion on metallic surfaces at 500°C and 560°C by metal-potassium trisulphate formation in oxy-co-combustion10.1016/j.fuel.2016.06.064 ↗
69. Fireside corrosion degradation of HVOF thermal sprayed FeCrAl coating at 700–800 °C10.1016/j.surfcoat.2015.01.074 ↗