journal article·2022-07

Investigations on the SCC initiation behavior of cold worked 316 L in high temperature oxygenated water at constant loads

Jiamei Wang, Tianyu Zhu, Kai Chen, Yichen Bao, Wujiang Ma, Miaomiao Zhang, Xianglong Guo, Peter L. Andresen, Lefu Zhang

Corrosion Science· Volume 203
Publisher page

Abstract

The effect of pH on the stress corrosion cracking (SCC) initiation behavior of 20% cold worked 316 L stainless steel (SS) at constant load was investigated. No cracks initiated after 4050 h testing in 360 °C high temperature water with a pH325 °C of 7.3, while extensive intergranular (IG) cracks initiated when the pH325 °C was increased to 10.1. A minimum crack initiation time of 886 h was detected at 0.9 YS. Localized attack of grain boundaries (GBs) and deformation bands is considered to be the precursor of crack initiation. The mechanistic understanding of the crack initiation and propagation is discussed.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Metal and Thin Film Mechanics · High Temperature Alloys and Creep

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (59)

Show source-provided references
1. IGSCC of non-sensitized stainless steels in high temperature water10.1016/j.jnucmat.2008.08.005 ↗
2. P.L. Andresen, Perspective and direction of stress corrosion cracking in hot water, Proceedings of the 10th International Symposium on Environmental Degradation of Materials in Nuclear Power Systems-Water Radiolysis, Lake Tahoe, Nevada, 2001.
3. Emerging issues and fundamental processes in environmental cracking in hot water10.5006/1.3278483 ↗
4. R.W. Staehle, Quantitative Micro-Nano (QMN) Approach to SCC Mechanism and Prediction-Starting a Third Meeting, Proc. 15th International Conference on Environmental Degradation of Materials in Nuclear Power Systems-Water Reactors. John Wiley & Sons, Inc., 2012.10.1002/9781118456835.ch161 ↗
5. Stress corrosion cracking on cold-worked austenitic stainless steels in PWR environment
6. Dependence of stress corrosion cracking for cold-worked stainless steel on temperature and potential, and role of diffusion of vacancies at crack tips10.5006/1.3278507 ↗
7. Scc in pwrs: learning from a bottom-up approach
8. A mechanistic study of the temperature dependence of the stress corrosion crack growth rate in sus316 stainless steels exposed to PWR primary water10.1016/j.actamat.2016.05.010 ↗
9. The influence of ppb levels of chloride impurities on the stress corrosion crack growth behaviour of low-alloy steels under simulated boiling water reactor conditions10.1016/j.corsci.2016.03.001 ↗
10. P. Berge, J.R. Donati, B. Prieux, D. Villard, Caustic stress corrosion of Fe-Cr-Ni austenitic alloys, 6th international congress on metallic corrosion, Sydney, Australia, 1975.
11. P.L. Andresen, P.W. Emigh, M.M. Morra, R.M. Horn, Effects of yield strength, corrosion potential, stress intensity factor, silicon and grain boundary character on the SCC of stainless steels, Proceedings of the 11th International Conference on Environmental Degradation of Materials in Nuclear Power Systems - Water Reactors. TMS, Stevenson, Washington, USA, 2003, pp. 816–833.
12. T. Shoji, G.F. Li, J. Kwon, S. Matsushima, Z.P. Lu, Quantification of yield strength effects on IGSCC of austenitic stainless steels in high temperature water. Proceedings of the 11th International Conference on Environmental Degradation of Materials in Nuclear Power Systems-Water Reactors, Stevenson, Washington, USA, 2003, pp. 834–844.
13. Stress corrosion cracking in the heat affected zone of a stainless steel 308L-316L weld joint in primary water10.1016/j.corsci.2016.02.030 ↗
14. D. Du, J. Wang, K. Chen, L. Zhang, P.L. Andresen, Environmentally assisted cracking of forged 316LN stainless steel and its weld in high temperature water, Corros. Sci. 147 (209) 69–80.10.1016/j.corsci.2018.10.032 ↗
15. Effect of temperature and loading mode on environmentally assisted crack growth of a forged 316L SS in oxygenated high-temperature water10.1016/j.corsci.2014.06.035 ↗
16. Effects of chloride and oxygen on stress corrosion cracking of cold worked 316/316L austenitic stainless steel in high temperature water10.1016/j.corsci.2016.04.035 ↗
17. Synergistic effects of local strain-hardening and dissolved oxygen on stress corrosion cracking of 316NG weld heat-affected zones in simulated BWR environments10.1016/j.jnucmat.2011.12.030 ↗
18. Effects of water chemistry on stress corrosion cracking of 316NG weld metals in high temperature water10.1179/1743278214Y.0000000186 ↗
19. Cracking Testing Guidelines: With Emphasis on High Temperature Water. EPRI, Palo Alto
20. Féron · 2016 · 3
21. International round-robin on stress corrosion crack initiation of alloy 600 material in PWR primary water10.5006/3532 ↗
22. K. Chen, J. Wang, L. Zhang, Investigation on the stress corrosion crack initiation and propagation behavior of alloy 600 in high-temperature water, Corrosion 74 (12018) 1395–1405.10.5006/2913 ↗
23. Study of grain boundary character along intergranular stress corrosion crack paths in austenitic alloys10.1016/S1359-6454(01)00064-7 ↗
24. The effect of grain boundary character distribution on the high temperature deformation behavior of Ni–16Cr–9Fe alloys10.1016/S1359-6454(03)00207-6 ↗
25. Effect of δ-ferrite on the stress corrosion cracking behavior of 321 stainless steel10.1016/j.corsci.2019.07.005 ↗
26. Effect of dissolved oxygen and hydrogen on the stress corrosion cracking behavior of alloy 600 in high temperature water10.1016/j.jnucmat.2020.152603 ↗
27. Environment assisted cracking of 308l weld metal in high temperature water
28. Stress corrosion crack initiation of alloy 600 in pwr primary water10.1016/j.corsci.2017.04.013 ↗
29. P.L. Andresen and P. Chou, SCC initiation and growth in PWR water containing KOH vs. LiOH, Proceedings of the 19th International Conference on Environmental Degradation of Materials in Nuclear Power Systems - Water Reactors. Boston, MA, August 18–22, 2019.
30. Effect of pH on corrosion behavior of 316l stainless steel in hydrogenated high temperature water10.1002/maco.201709761 ↗
31. Characterization of oxide scales grown on alloy 310s stainless steel after long term exposure to supercritical water at 500 °C10.1016/j.matchar.2016.09.013 ↗
32. An insight into PWR primary water SCC mechanisms by comparing surface and crack oxidation10.1016/j.corsci.2018.12.020 ↗
33. Microstructural characterization of SCC crack tip and oxide film for SUS 316 stainless steel in simulated PWR primary water at 320°C10.1080/18811248.2005.9726383 ↗
34. Characterization of the crack initiation and propagation in alloy 600 with a cold-worked surface10.1016/j.corsci.2019.03.014 ↗
35. Influence of surface condition on primary water stress corrosion cracking initiation of alloy 600
36. Miura · 2012
37. Effect of thermal ageing and dissolved gas on corrosion of 308l stainless steel weld metal in simulated PWR primary water
38. A mechanistic study of SCC in Alloy 600 through high-resolution characterization10.1016/j.corsci.2018.01.004 ↗
39. Effects of zinc injection on stress corrosion cracking of cold worked austenitic stainless steel in high-temperature water environments10.1016/j.scriptamat.2017.05.032 ↗
40. Stress corrosion cracking of the fusion boundary for 304l/82 dissimilar metal weld joint in simulated primary water10.5006/3343 ↗
41. Microstructural and microchemical mechanisms controlling intergranular stress corrosion cracking in light-water-reactor systems10.1016/0022-3115(94)90020-5 ↗
42. P.M. Scott, An Overview of Internal Oxidation as a Possible Explanation of Intergranular Stress Corrosion Cracking of Alloy 600 in PWRS, Ninth International Symposium on Environmental Degradation of Materials in Nuclear Power Systems-Water Reactors, The Minerals, Metals and Materials Society, 1999, pp. 3–12.10.1002/9781118787618.ch1 ↗
43. Degradation of grain boundary strength by oxidation in alloy 600
44. The role of cold work and applied stress on surface oxidation of 304 stainless steel10.1016/j.corsci.2011.11.021 ↗
45. Effect of surface preparation on intergranular stress corrosion cracking of alloy 600 in hydrogenated steam10.5006/1.3279916 ↗
46. Pourbaix diagrams for the ternary system of iron-chromium-nickel10.5006/1.3283945 ↗
47. Effects of hydrogen peroxide on intergranular stress corrosion cracking of stainless steel in high temperature water, (IV)10.1080/18811248.2001.9715020 ↗
48. N. Sumitani, T. Kusakabe, K. Onimura, S. Tokunaga, Proceedings: 1989 EPRI Alloy 690 Workshop, Report. NP-6750, EPRI, Palo Alto, CA, 1990.
49. Understanding the effect of surface finish on stress corrosion crack initiation in warm-forged stainless steel 304L in high-temperature water10.1016/j.scriptamat.2019.01.032 ↗
50. Stress corrosion crack initiation in machined type 316L austenitic stainless steel in simulated pressurized water reactor primary water10.1016/j.corsci.2018.04.003 ↗
51. Stress corrosion cracking of sensitized type 304 stainless steel in high-temperature water with anionic impurities contamination10.5006/0690 ↗
52. N. Huin, O. Calonne, M. Herbst, R. Kilian, SCC of Austenitic Stainless Steels Under Off-Normal Water Chemistry and Surface Conditions. In Proceedings of the 18th International Conference on Environmental Degradation of Materials in Nuclear Power Systems-Water Reactors. The Minerals, Metals & Materials Series. Springer, Cham, 2019.
53. S. Lozano-Perez. How oxidized grain boundaries fail10.1016/j.actamat.2013.05.012 ↗
54. Effect of rising and falling K profiles on SCC growth rates in high-temperature water10.1115/1.2748830 ↗
55. dK/da effects on the SCC growth rates of nickel base alloys in high-temperature water10.1016/j.jnucmat.2018.02.032 ↗
56. Modelling the electrochemical crack size effect on stress corrosion crack growth rate10.1016/j.corsci.2017.06.016 ↗
57. Retardation of crack initiation and growth in austenitic stainless steels by laser peening without protective coating10.1016/j.msea.2005.11.017 ↗
58. Electrochemical aspects of the stress corrosion cracking of iron-chromium-nickel alloys in caustic solutions10.1016/0010-938X(80)90135-3 ↗
59. Life prediction by mechanistic modeling and system monitoring of environmental cracking of iron and nickel alloys in aqueous systems10.1016/0025-5416(88)90564-2 ↗