Improved oxidation resistance of 15 wt.% Cr ferritic stainless steels containing 0.08–2.45 wt.% Al at 1000 °C in air
Source abstract
Abstract
Abstract Improved oxidation resistance of 15 wt.% Cr ferritic stainless steels at 1000 °C in air has been obtained. Weight gain per unit area is in parabolic relation to oxidation time and parabolic rate constant significantly decreases with increased Al content. Diffusion of Al is enhanced and the porous Cr 2 O 3 rich outer layer is replaced by a more compact Al 2 O 3 rich outer layer in steels with higher Al contents. The appearance of continuous and compact Al 2 O 3 oxide scale contributes to the significantly improved oxidation resistance property and the oxidation mechanism has been suggested based on microstructural observations.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: High-Temperature Coating Behaviors · Nuclear Materials and Properties · Catalytic Processes in Materials Science
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (31)
Show source-provided references
1. Thermally grown oxide films and corrosion performance of ferritic stainless steels under simulated exhaust gas condensate conditions10.1016/j.corsci.2014.06.041 ↗
2. Effect of grain boundary characteristics on the oxidation behavior of ferritic stainless steel10.1016/j.corsci.2011.08.020 ↗
3. The effect of annealing on the corrosion behaviour of 444 stainless steel for drinking water applications10.1016/j.corsci.2014.06.025 ↗
4. Effect of SO2 on oxidation of type 409 stainless steel and its implication on condensate corrosion in automotive mufflers10.1016/j.corsci.2013.11.018 ↗
5. Intergranular corrosion of Ti-stabilized 11wt.% Cr ferritic stainless steel for automotive exhaust systems10.1016/j.corsci.2009.07.008 ↗
6. Characterization of precipitates formed in a ferritic stainless steel stabilized with Zr and Ti additions10.1016/j.matchar.2005.05.006 ↗
7. Effect of chromium content on intergranular corrosion and precipitation of Ti-stabilized ferritic stainless steels10.1016/j.corsci.2010.01.037 ↗
8. Microstructure and texture of Nb+Ti stabilized ferritic stainless steel10.1016/j.matchar.2008.03.018 ↗
9. Effect of copper and aluminium addition on mechanical properties and corrosion behaviour of AISI 430 ferritic stainless steel gas tungsten arc welds10.1016/j.jmrt.2013.02.009 ↗
10. Effect of hot band annealing processes on microstructure, texture and r-value of ferritic stainless steel10.1016/S1006-706X(10)60157-4 ↗
11. Effect of aluminum on microstructure, mechanical properties and pitting corrosion resistance of ultra-pure 429 ferritic stainless steels10.1016/j.matdes.2014.09.074 ↗
12. High temperature oxidation behaviour of high Al content ferritic and austenitic stainless steels with and without rare-earth element addition10.1007/s11085-011-9274-2 ↗
13. The effects of Cr and Al concentrations on the oxidation behavior of oxide dispersion strengthened ferritic alloys10.1016/j.corsci.2013.07.004 ↗
14. Effects of Co, Al and Mo on the long term passivation of 9Cr-3W (wt.%) ferritic steels in air and wet air at 650°C10.1016/j.corsci.2014.01.030 ↗
15. Influence of aluminium on creep strength of 9–12% Cr steels10.1016/j.msea.2009.07.060 ↗
16. Effects of aluminum content on the mechanical properties of a 9Cr-0.5Mo-1.8W steel10.1007/s11661-997-0284-2 ↗
17. Corrosion behavior of an alumina forming austenitic steel exposed to supercritical carbon dioxide10.1016/j.corsci.2013.12.023 ↗
18. The development of alumina-forming austenitic stainless steels for high-temperature structural use10.1007/s11837-008-0083-2 ↗
19. Oxidation behaviour of FeAl intermetallic. The effects of Y and/or Zr on isothermal oxidation kinetics10.1016/S0966-9795(00)00007-8 ↗
20. The single-crystal Raman spectra of nearly opaque materials. Iron (III) oxide and chromium (III) oxide10.1039/j19700000980 ↗
21. Temperature-dependent light-scattering studies of the Verwey transition and electronic disorder in magnetite10.1103/PhysRevB.9.5236 ↗
22. Raman microspectroscopy of some iron oxides and oxyhydroxides10.1002/(SICI)1097-4555(199711)28:11<873::AID-JRS177>3.0.CO;2-B ↗
23. Characterization of nonmelted particles and molten splats in plasma-sprayed Al2O3 coatings by a combination of scanning electron microscopy, X-ray diffraction analysis, and confocal Raman analysis10.1007/s11666-012-9863-x ↗
24. Thin film of aluminum oxide through pulsed laser deposition: a micro-Raman study10.1016/S0921-5107(00)00554-7 ↗
25. Chapter 3.3—Ellingham diagram
26. Ion diffusion study in the oxide layers due to oxidation of AISI 439 ferritic stainless steel10.1007/s11085-013-9451-6 ↗
27. Corrosion behaviour of 16%Cr-4%Al and 16%Cr ODS ferritic steels under different metallurgical conditions in a supercritical water environment10.1016/j.corsci.2010.05.043 ↗
28. The effects of the minor alloying elements Al, Si and Mn on the cyclic oxidation of Ni-Cr-W-Mo alloys10.1016/j.corsci.2014.02.015 ↗
29. Oxidation of 316 stainless steel in supercritical water10.1016/j.corsci.2009.03.008 ↗
30. Crystal structure and isothermal compression of Fe2O3, Cr2O3, and V2O3 to 50 kbars10.1063/1.327451 ↗
31. Effect of high pressure on the lattice parameters of Cr2O3 and α-Fe2O310.1063/1.1727313 ↗