Abstract

Abstract The effect of chemical pretreatments on the electrochemical etching behavior of aluminium was investigated with the topographic studies of surface and the analysis of initial potential transients. Two-step pretreatments with H 3 PO 4 and H 2 SiF 6 result in a high density of pre-etch pits on aluminium surface by the incorporation of phosphate ion inside the oxide film and the removal of surface layer by aggressive fluorosilicic acid solution. It generates a high density of etch pits during electrochemical etching and results in the capacitance increase of etched Al electrode by expanding the surface area, up to 61.3 μF/cm 2 with the pretreatment solution of 0.5 M H 3 PO 4 at 65 °C and 10 mM H 2 SiF 6 at 45 °C.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Anodic Oxide Films and Nanostructures · Corrosion Behavior and Inhibition · Concrete Corrosion and Durability

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (14)

Show source-provided references
1. The chemical nature of aluminium corrosion, III. The dissolution mechanism of aluminium oxide and aluminium powder in various electrolytes10.1149/1.2129520 ↗
2. The chemical nature of aluminium corrosion, V. Energy transfer in aluminium dissolution10.1149/1.2123881 ↗
3. Effects of electrolyte composition and applied potential on the repassivation kinetics of pure aluminium10.1016/0013-4686(95)94180-3 ↗
4. Sequence of steps in the pitting of aluminium by chloride ions10.1016/S0010-938X(02)00231-7 ↗
5. Metastable pitting behavior of aluminium single crystals10.1016/S0010-938X(00)00032-9 ↗
6. Pitting corrosion of aluminium10.1016/S0010-938X(99)00012-8 ↗
7. The role of indole and its derivatives in the pitting corrosion of Al in neutral chloride solution10.1016/S0010-938X(03)00067-2 ↗
8. Effects of pH and chloride concentration on pitting corrosion of AA6061 aluminium alloy10.1016/j.corsci.2008.03.006 ↗
9. Growth rates of aluminium etch tunnels10.1149/1.2095356 ↗
10. Electrochemical tunnel etching of aluminium10.1149/1.2115495 ↗
11. Adsorption of sulfate and chloride ions on aluminium10.1016/S0013-4686(97)10188-8 ↗
12. Initial events during the passivation of rapidly dissolving aluminium surfaces10.1149/1.2054945 ↗
13. Growth of etch pits formed during sonoelectrochemical etching of aluminium10.1016/j.electacta.2005.04.070 ↗
14. Effect of trace elements on etching of aluminium electrolytic capacitor foil10.1149/1.2114188 ↗