Abstract

Highlights - Corrosion of Inconel 601 in molten carbonate salt was studied for energy storage. - Analysis revealed partial recovery with stress relieving due to annealing. - Annealing resulted in lower corrosion rate and susceptibility. - Cold-work caused the development of driving forces for localised attack. The interaction between Inconel 601 and the eutectic mixture of Li2CO3 + K2CO3 + Na2CO3 at 450° C was investigated for thermal energy storage. Electron backscatter diffraction, optical microscopy, Volta potential, polarization and impedance measurements were used to compare the alloy behaviour in cold-worked and annealed conditions. Results showed that annealing leads to a lower corrosion rate accompanied by fewer areas of localised attack. Volta potential measurements confirmed the development of micro-anodic sites on the surface in cold-worked condition which provide driving force for localised attack. These sites were found responsible for relatively higher corrosion rate and formation of meta-stable pits.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Molten salt chemistry and electrochemical processes · Aluminum Alloy Microstructure Properties · Metallurgical Processes and Thermodynamics

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (58)

Show source-provided references
1. Numerical simulation of the simultaneous precipitation of δ and γ′ phases in the Ni-base superalloy ATI Allvac®718Plus™
2. The effect of structural evolution in INCONEL 601 on intergranular corrosion10.1016/S0254-0584(98)00149-7 ↗
3. 22 – Physical metallurgy of the nickel-based superalloys
4. 1 – introduction to concentrating solar power (CSP) technology
5. Gomez · 2011
6. High-temperature phase change materials for thermal energy storage10.1016/j.rser.2009.11.011 ↗
7. Thermal energy storage technologies and systems for concentrating solar power plants10.1016/j.pecs.2013.02.001 ↗
8. Lithium in thermal energy storage: a state-of-the-art review10.1016/j.rser.2014.10.096 ↗
9. 20 – high-temperature molten salts for solar power application
10. Stress assisted oxidative failure of Inconel 601 for thermal energy storage10.1016/j.solmat.2016.10.008 ↗
11. Role of grain boundary carbides in cracking behavior of Ni base alloys10.5516/NET.07.2012.013 ↗
12. Stress corrosion cracking behavior at inconel and low alloy steel weld interfaces10.1007/s11661-014-2560-2 ↗
13. Characterization of corrosion interfaces by the scanning kelvin probe force microscopy technique10.1149/1.1359199 ↗
14. Microstructure of polycrystalline Ti and its microelectrochemical properties by means of electron-backscattering diffraction (EBSD)10.1016/S0013-4686(01)00572-2 ↗
15. Effects of sample orientation on the corrosion of zinc in ammonium sulfate and sodium hydroxide solutions10.1016/0010-938X(91)90089-8 ↗
16. The effect of crystallographic orientation on the active corrosion of pure magnesium10.1016/j.scriptamat.2007.10.027 ↗
17. Crystal orientation and electrochemical corrosion of polycrystalline Mg10.1016/j.corsci.2012.05.019 ↗
18. Dissolution of magnesium oxide in aqueous acid: an atomic force microscopy study10.1021/jp982260x ↗
19. Chapter 10 – surfaces, grain boundaries and interfaces
20. 23 – recovery and recrystallization: phenomena, physics, models, simulation
21. Residual stress and its role in failure10.1088/0034-4885/70/12/R04 ↗
22. Infrared brazing Inconel 601 and 422 stainless steel using the 70Au-22Ni-8Pd braze alloy10.1007/s10853-005-0446-9 ↗
23. Pitting characteristics of alloy 600 and alloy 601 in a chloride-containing acidic environment10.5006/1.3290372 ↗
24. Low-temperature stress corrosion cracking of alloy 601 in thiosulfate and chloride solutions10.5006/1.3283963 ↗
25. Reference electrodes for ionic liquids and molten salts
26. Pseudo-reference electrodes
27. Direct electrochemical reduction of titanium dioxide to titanium in molten calcium chloride10.1038/35030069 ↗
28. Pinpoint and bulk electrochemical reduction of insulating silicon dioxide to silicon10.1038/nmat900 ↗
29. EEstablishing a correlation between interfacial microstructures and corrosion initiation sites in Al/Cu joints by SEM–EDS and AFM–SKPFM10.1016/j.corsci.2013.10.039 ↗
30. 1 – Mechanistic and fractographic aspects of stress-corrosion cracking (SCC)
31. Interface migration during recrystallization: the role of recovery and stored energy gradients10.1007/BF02698245 ↗
32. Competition between recovery and recrystallization10.1016/S0921-5093(01)01860-3 ↗
33. Diffusion-migration transport in a system with butler-volmer kinetics, an exact solution10.1016/0013-4686(94)00359-9 ↗
34. Electrochemistry of molten-salt corrosion10.1016/0921-5093(91)90265-O ↗
35. Solubility of NiO in molten Li2CO3, Na2CO3,K2CO3, and Rb2CO3 at 910°C10.1149/1.2096093 ↗
36. Electrochemical studies of the corrosion of Ni and Fe in molten carbonate10.2320/jinstmet1952.48.7_720 ↗
37. Corrosion behavior of nickel‐iron alloys in molten carbonate10.1149/1.1836387 ↗
38. Corrosion of composite tube air-ports in kraft recovery boiler: Cr2O3, Fe2O3, NiO solubility in molten hydroxide
39. Corrosion of nickel in molten carbonate10.1149/1.2059276 ↗
40. The solubility of NiO in binary mixtures of molten carbonates10.1149/1.2096301 ↗
41. Electrochemical impedance models for molten salt corrosion10.1016/S0010-938X(00)00108-6 ↗
42. Effect of processing parameters on the corrosion behaviour of friction stir processed AA 2219 aluminum alloy10.1016/j.solidstatesciences.2008.11.007 ↗
43. Pitting corrosion of friction stir welded aluminum alloy thick plate in alkaline chloride solution10.1016/j.electacta.2009.12.083 ↗
44. Microstructures and electrochemical behaviors of the friction stir welding dissimilar weld10.1016/S1001-0742(11)61072-3 ↗
45. Lasia · 2014
46. Lvovich · 2012
47. Diffusion impedance
48. The influence of sulphate-reducing bacteria biofilm on the corrosion of stainless steel AISI 31610.1016/j.corsci.2006.10.040 ↗
49. An investigation of the capacitance dispersion on the fractal carbon electrode with edge and basal orientations10.1016/S0013-4686(03)00464-X ↗
50. Corrosion behavior of stainless-steel and nickel-base alloys in molten-carbonate10.1149/1.2049983 ↗
51. Calibration of the scanning Kelvin probe force microscope under controlled environmental conditions10.1016/j.electacta.2012.01.054 ↗
52. Local potential measurements with the SKPFM on aluminium alloys10.1016/j.electacta.2004.01.045 ↗
53. Integrated AFM and SECM for in situ studies of localized corrosion of Al alloys10.1016/j.electacta.2006.12.073 ↗
54. Microstructure and corrosion characterization of the interfacial region in dissimilar friction stir welded AA5083 to AA702310.1016/j.corsci.2016.02.027 ↗
55. Chapter 4 – introduction to dislocations
56. Twinning in nanocrystalline fcc metals10.1002/adem.200400163 ↗
57. Lai · 1990
58. On the orientation dependence of static recovery in low-carbon steels10.1016/0956-716X(95)00276-2 ↗